Abstract
Abstract The changes produced in the dielectric permittivity, the transverse piezoelectric coefficient, the k31 coupling factor, the s11E elastic compliance and the mechanical quality factor of PZT-4D hard piezoceramics by heating have been investigated. The ceramics were then repoled, and the reversible and irreversible components of the changes quantified. The results showed that depolarisation began at 150°C. A high level of poling was retained even after heating at 300°C (d31=−83×10−12 C N−1 and k31=0.225), only 20°C below the transition temperature. However, a significant irreversible degradation of the mechanical quality factor, Qm, occurred at a temperature as low as 100°C. Experiments on thinned specimens showed that the degradation of Qm took place in the Ag doped layer produced by the electrodes. Indentation surface cracks were also introduced into the ceramics to investigate the behaviour of cracks during the thermal treatments.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Temperature characteristics for multilayer piezoelectric ceramic actuator10.7567/JJAPS.24S3.209 ↗
2. A high speed impact actuator using multilayer piezoelectric ceramics10.1016/0924-4247(90)80064-C ↗
3. Measuring methods for high-power characteristics of piezoelectric materials10.1557/PROC-360-15 ↗
4. Heat generation in multilayer piezoelectric actuators10.1111/j.1151-2916.1996.tb08095.x ↗
5. Fracture behaviour of cyclically loaded PZT10.1111/j.1151-2916.1994.tb04649.x ↗
6. Uchino · 1997
7. Vibration-level characteristics for iron-doped lead zirconate titanate ceramic10.1143/JJAP.32.2422 ↗
8. Ageing of (Pb,La)(Zr,Ti)O3 ferroelectric ceramics and the space charge arising on hot poling10.1007/BF00550809 ↗
9. Materials issues in design and performance of piezoelectric actuators: an overview10.1016/S1359-6454(98)00102-5 ↗
10. Morgan Matroc Limited-Unilator Division, Piezoelectric Ceramic Products Catalogue.
11. Electrical after effects in Pb(Ti,Zr)O3 ceramics10.1080/00150197808236770 ↗
12. Algueró, M., Cheng, B. L., Gibson, I. R., Guiu, F. and Reece, M. J., Crack growth during poling and polarisation reversal in commercial piezoceramics. Boletı́n de la Sociedad Española de Cerámica y Vidrio, 1999. 38(16), 593–598.10.3989/cyv.1999.v38.i6.899 ↗
13. Jaffe · 1971
14. IEEE Standard on Piezoelectricity. ANSI/IEEE Std 176, 1987.
15. Accurate measurement of coefficients in a ferroelectric ceramic10.1109/T-SU.1969.29524 ↗
16. Domain wall clamping by orientation of defects10.1063/1.352948 ↗
17. Temperature and bias characteristics of Pb(Zr-Ti)O3 families ceramics10.1143/JJAP.4.867 ↗
18. Diffusional penetration of silver from electrodes into PZT ceramics10.1007/BF00570062 ↗
19. Effect of silver doping on the physical and electrical properties of PLZT ceramics10.1111/j.1151-2916.1983.tb10071.x ↗
20. Effects of silver and palladium doping on the dielectric properties of 0.9Pb(Mg1/3Nb2/3))3-0.1PbTiO3 ceramic10.1111/j.1151-2916.1996.tb07907.x ↗
21. Direct evaluation of domain wall and intrinsic contributions to the dielectric and piezoelectric response and their temperature dependence on lead zirconate-titanate ceramics10.1063/1.355874 ↗
22. Anisotropy of fracture toughness of piezoelectric ceramics10.1111/j.1151-2916.1985.tb15319.x ↗
23. Growth of indentation cracks in poled and unpoled PZT10.1016/S0955-2219(96)00089-1 ↗
24. Elastic/plastic indentation damage in ceramics: the median/radial crack system10.1111/j.1151-2916.1980.tb10768.x ↗