journal article·2015-06

Influence of temperature and humidity on the strength of low temperature co-fired ceramics

Clemens Krautgasser, Robert Danzer, Peter Supancic, Raul Bermejo

Publisher page

Abstract

Abstract Strength degradation in glass and ceramic materials is related to subcritical crack growth mechanisms acting at the crack tip during mechanical loading. In this work the effect of humidity and temperature on the strength of a commercial low temperature co-fired ceramic was investigated using a biaxial testing procedure. Experiments were performed in argon and in air at different stress rates between 25 and 125 °C. The effect of humidity on strength was assessed at room temperature varying only the relative humidity. The sole effect of temperature was evaluated in argon at high stress rates. The combined effect of humidity and temperature was determined in air, testing at different temperatures. Results showed the existence of an inert strength of the material at room temperature. Measurements in ambient air showed a counterbalance effect of temperature and humidity yielding an almost constant strength for this material between 25 and 125 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Recycling and utilization of industrial and municipal waste in materials production · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Ceramic-filled-glass composite sintering
2. 60-GHz-band LTCC module technology for wireless gigabit transceiver applications
3. Prospects of low temperature co-fired ceramic (LTCC) based microfluidic systems for point-of-care biosensing and environmental sensing
4. Delayed fracture in glass10.1088/0959-5309/59/2/302 ↗
5. Influence of water vapour on crack propagation in soda-lime glass10.1111/j.1151-2916.1967.tb15145.x ↗
6. Subcritical crack growth in ceramics
7. A molecular mechanism for stress corrosion in vitreous silica10.1111/j.1151-2916.1983.tb15715.x ↗
8. Thermally activated crack propagation in brittle materials10.1007/BF00012548 ↗
9. Sub-critical crack growth in ceramics
10. Environmentally enhanced fracture of glass: a historical perspective10.1111/j.1551-2916.2009.03097.x ↗
11. Lifetime prediction for mechanically stressed low temperature co-fired ceramics10.1016/j.jeurceramsoc.2003.07.010 ↗
12. Sub-critical crack growth behavior of a low-temperature co-fired ceramic10.1111/j.1551-2916.2007.01626.x ↗
13. Subcritical crack growth in low temperature co-fired ceramics under biaxial loading10.1016/j.engfracmech.2012.12.004 ↗
14. Fracture toughness and strength distribution at room temperature of zirconia tapes used for electrolyte supported solid oxide fuel cells10.1016/j.jpowsour.2014.10.083 ↗
15. High temperature mechanical properties of zirconia tapes used for electrolyte supported solid oxide fuel cells10.1016/j.jpowsour.2014.09.068 ↗
16. Slow crack growth in brittle materials under dynamic loading conditions10.1007/BF00113930 ↗
17. Munz · 1999
18. Subcritical crack propagation in 3Y-TZP ceramics: static and cyclic fatigue10.1111/j.1151-2916.1999.tb02213.x ↗
19. Influence of the temperature on the strength and the subcritical crack growth rate of alumina10.1016/j.msea.2004.02.090 ↗
20. The ball on three balls test for strength testing of brittle discs: stress distribution in the disc10.1016/S0955-2219(01)00458-7 ↗
21. The ball on three balls test for strength testing of brittle discs. Part II: Analysis of possible errors in the strength determination10.1016/j.jeurceramsoc.2003.10.035 ↗
22. Morrell · 1999
23. Influence of measurement uncertainties on the determination of the Weibull distribution10.1016/j.jeurceramsoc.2011.09.008 ↗
24. Experimental approach to assess the effect of metallization on the strength of functional ceramic components10.1016/j.scriptamat.2011.12.029 ↗
25. Biaxial tensile strength test for brittle rectangular plates10.2109/jcersj.114.1054 ↗
26. http://www.mathesongas.com/pdfs/products/Argon-Pure-Gas.pdf [accessed 12.11.14].
27. ISO 23146 · 2008
28. Critical notch-root radius effect in SENB-S fracture toughness testing10.1016/0955-2219(95)00197-2 ↗
29. Polished notch modification of SENB-S fracture toughness testing10.1016/S0955-2219(97)00024-1 ↗
30. http://www.isfk.at/de/960/ [accessed 20.10.2013].
31. ANSYS · 2011
32. Strength reliability of 3D low temperature co-fired multilayer ceramics under biaxial loading10.1016/j.jeurceramsoc.2010.11.031 ↗
33. EN 843-5 · 1997 · 40
34. Mechanical failure of advanced ceramics: the value of fractography10.4028/www.scientific.net/KEM.223.1 ↗
35. Influence of internal architectures on the fracture response of LTCC components10.4028/www.scientific.net/KEM.409.275 ↗
36. The phenomenon of rupture and flow in solids
37. Crack-extension force for a part-through crack in a plate10.1115/1.3640649 ↗
38. Lawn · 1993 · 378
39. On the relationship between ceramic strength and the requirements for mechanical design10.1016/j.jeurceramsoc.2014.04.026 ↗
40. Surface crack in tension or in bending – a reassessment of the Newman and Raju formula in respect to fracture toughness measurements in brittle materials10.1016/j.jeurceramsoc.2012.01.011 ↗