Ceramic micro parts. Part 1: How thermal debinding can be utilized to enhance surface finish and mechanical properties
Source abstract
Abstract
Abstract Thermal debinding represents the most critical processing step of powder injection moulding (PIM) of ceramics. Defects such as cracks and pores might be caused, when the process cannot be controlled properly. Considering low-pressure injection moulding (LPIM), however, thermal debinding opens up the possibility to enhance the mechanical properties of ceramic micro parts. In this study, the unique effect of surface defect healing is presented, which takes place during debinding. It enables improved surface finish and results in increased mechanical strength and reliability. As a model, 3Y-TZP micro bending bars with dimensions of 200 μm × 200 μm × 1200 μm were selected. It could be revealed that thermal debinding can be utilized to increase the characteristic 3-point-bending strength up to 3235 MPa with Weibull modulus of 21.4. This result corresponds to macroscopic bending strength of 1727 MPa, which can be achieved only by exhausting fabrication methods and surface post-processing.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Injection Molding Process and Properties · Advanced machining processes and optimization · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (70)
Show source-provided references
1. Ceramics in microtechnology: status, requirements and challenges
2. A review of micro-powder injection moulding as a microfabrication technique10.1088/0960-1317/21/4/043001 ↗
3. Microceramic injection molding
4. Ceramic injection moulding: a review of developments in production technology, materials and applications
5. Powder injection moulding of metallic and ceramic micro parts10.1007/s00542-011-1274-2 ↗
6. Development of a rapid prototyping process chain for the production of ceramic microcomponents10.1023/A:1016150126206 ↗
7. Development of a roadmap for advanced ceramics: 2010–202510.1016/j.jeurceramsoc.2008.10.015 ↗
8. Recent developments in micro ceramic injection molding10.3139/146.101737 ↗
9. Medical and dental applications for microminiature powder injection moulding – a roadmap for growth
10. Mikrospritzgießen bringt Keramik in Hochform
11. Low-pressure injection moulding
12. Hot moulding – an interesting forming process
13. Injection molding of components for microsystems10.1007/s005420100094 ↗
14. Manufacturing of ceramic microcomponents by a rapid prototyping process chain10.1002/1527-2648(200101)3:1/2<49::AID-ADEM49>3.0.CO;2-H ↗
15. Rapid manufacturing of ceramic microcomponents
16. Design and prototyping of a ceramic micro turbine: a case study10.1007/s00542-009-0974-3 ↗
17. Partial wick-debinding of low-pressure powder injection-moulded ceramic parts10.1016/j.jeurceramsoc.2010.07.011 ↗
18. Defect levelling during debinding for improved mechanical properties of ceramic micro Parts
19. Factors affecting strength and shape retention of zirconia micro bending bars during thermal debinding10.1016/j.ceramint.2011.04.076 ↗
20. Microstructure, surface topography and mechanical properties of molded ZrO2 microspecimens
21. Auhorn · 2006
22. Factors influencing the mechanical properties of moulded zirconia micro parts
23. Influence of surface defects and edge geometry on the bending strength of slip-cast ZrO2 micro-specimens10.1515/ijmr-2004-0106 ↗
24. Correlations between production process, states and mechanical properties of microspecimens made of zirconia10.1007/s00542-006-0242-8 ↗
25. Kasanická · 2008
26. Relationships between process, microstructure and properties of molded zirconia micro specimens10.1007/s00542-008-0631-2 ↗
27. Rögner · 2010
28. Influence of dispersant, storage time and temperature on the rheological properties of zirconia–paraffin feedstocks for LPIM10.1016/j.jeurceramsoc.2009.12.003 ↗
29. DIN 4768 · 1990
30. Effect of surface-active substances on the rheological properties of silicon carbide suspensions in paraffin10.1111/j.1151-2916.2000.tb01184.x ↗
31. Heldele · 2009
32. Wadewitz · 1999
33. Effects of surfactant on properties of MIM feedstock10.1016/S1003-6326(07)60039-9 ↗
34. Surface modification of powders with carboxylic acids10.1007/BF01730436 ↗
35. Mechanical properties and low-temperature aging of tetragonal zirconia polycrystals processed by hot isostatic pressing10.1557/JMR.2003.0337 ↗
36. microstructure and mechanical properties of commercial Y-TZPs10.1007/BF01152158 ↗
37. Injection-molded ceramics: critical aspects of the binder removal process and component fabrication10.1016/0955-2219(93)90055-V ↗
38. Kinetics of capillary extraction of organic vehicle from ceramic bodies. Part II. Partitioning between porous media10.1016/0955-2219(91)90115-G ↗
39. Removal of organic binders in ceramic powder compacts
40. Liquid-phase transport during removal of organic binders in injection-molded ceramics10.1111/j.1151-2916.1990.tb06456.x ↗
41. Binder removal from injection moulded zirconia ceramics10.1016/S0272-8842(97)00090-4 ↗
42. Degradation of polyolefin blends used for ceramic injection molding10.1111/j.1151-2916.1989.tb05985.x ↗
43. Munz · 1999
44. Phenomenological study and modelling of wick debinding10.1016/j.ces.2008.04.040 ↗
45. Theory of thermal debinding
46. Flocculation after injection molding in ceramic suspensions10.1557/JMR.1994.2386 ↗
47. Capillary surface interfaces
48. Survey of sticking effects for micro parts handling
49. From “macro” to “micro” manipulation: models and experiments10.1109/TMECH.2004.828657 ↗
50. Two-dimensional micro-self-assembly using the surface tension of water10.1016/S0924-4247(97)80102-1 ↗
51. Surface tension-powered self-assembly of microstructures10.1109/JMEMS.2003.811724 ↗
52. Rheological properties of re-melted paraffin-wax suspensions used for LPIM10.1016/j.jeurceramsoc.2008.11.012 ↗
53. Schlechtriemen · 2010
54. Rheology of zirconia suspensions in a nonpolar organic medium10.1111/j.1151-2916.1995.tb07958.x ↗
55. Influence of dispersant structure on the rheological properties of highly-concentrated zirconia dispersions10.1016/j.jeurceramsoc.2004.05.002 ↗
56. Stability of aqueous alpha-Al2O3 suspensions with polymethacrylic acid polyelectrolyte10.1111/j.1151-2916.1988.tb05855.x ↗
57. Reversible-growth model: cluster–cluster aggregation with finite binding energies10.1103/PhysRevA.36.5015 ↗
58. Influence of powder agglomerates on the structure and rheological behavior of injection-molded zirconia–wax suspensions10.1111/j.1151-2916.1999.tb02136.x ↗
59. Effect of dispersants on the rheological behavior of zirconia–wax suspensions10.1111/j.1151-2916.1999.tb01890.x ↗
60. Ultrafine ceramic powder injection moulding: the role of dispersants10.1122/1.550737 ↗
61. Ceramic powder dispersion in nonaqueous systems
62. Influence of dispersant on rheology of zirconia–paraffin feedstocks and mechanical properties of micro parts fabricated via LPIM10.1002/9780470944066.ch4 ↗
63. DIN EN 843-1:2008-08 · 2008
64. Fracture of ceramics10.1002/adem.200700347 ↗
65. Transformation strengthening of as-fired zirconia ceramics10.1016/S0272-8842(97)00093-X ↗
66. Tosoh Corp. Data sheet TZ-3YS-E. Tokyo; 2011.
67. Effect of sintering temperature on microscopic and mechanical properties of 3Y-TZP dental ceramic
68. Tetragonal zirconia polycrystal (TZP) – a review10.1016/0267-3762(87)90060-9 ↗
69. Strength limitations of transformation-toughened zirconia alloys10.1111/j.1151-2916.1986.tb04785.x ↗
70. Some notes on the correlation between fracture and defect statistics: are Weibull statistics valid for very small specimens?10.1016/j.jeurceramsoc.2005.08.021 ↗