Abstract 3Y-TZP ceramics are commonly used in restorative dentistry for fixed partial dentures, implants, abutments and root posts. The stress-induced transformation-toughening mechanism leads to improved mechanical properties advocating 3Y-TZP to be ground or sandblasted for better clinical performance. Such invasive mechanical treatments facilitate the additional surface strengthening as a result of the residual compressive stresses, but the exact origin is not completely understood. This study evaluated the effect of continuous impacting between 3Y-TZP root posts during 500 -h-long shaking on the extent of (sub)surface microstructural changes affecting the fracture strength. With an increase of the shaking time the surface roughness decreased, where the grains were flattened and partially spalled. The observed 6-micrometre-thick altered subsurface region containing compressive residual stresses contributed to a systematic increase in the forces of fracture within the sample population; however, only for those containing the surface type of critical flaws that were in the form of mould imprints.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Dental Research and COVID-19

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
2. Ceramic steel?10.1038/258703a0 ↗
3. Phase change and mechanical properties of ZrO2-Y2O3 solid electrolyte after ageing10.1016/0167-2738(81)90138-7 ↗
4. Environmental degradation of zirconia ceramics10.1016/0955-2219(95)00035-S ↗
5. The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
6. Direct evidence for continuous linear kinetics in the low-temperature degradation of Y-TZP10.1016/j.actbio.2012.08.032 ↗
7. Ageing kinetics and strength of airborne-particle abraded 3Y-TZP ceramics10.1016/j.dental.2017.04.014 ↗
8. Long-time aging in 3 mol.% yttria-stabilized tetragonal zirconia polycrystals at human body temperature10.1016/j.actbio.2013.09.033 ↗
9. Effect of heat-treatment on grain size, phase assemblage, and mechanical properties of 3 mol% Y-TZP10.1111/j.1151-2916.1996.tb08980.x ↗
10. Ageing of dental zirconia ceramics10.1016/j.jeurceramsoc.2012.02.024 ↗
11. The influence of yttrium-segregation-dependent phase partitioning and residual stresses on the aging and fracture behaviour of 3Y-TZP ceramics10.1016/j.actbio.2017.08.014 ↗
12. Effect of cation dopant radius on the hydrothermal stability of tetragonal zirconia: Grain boundary segregation and oxygen vacancy annihilation10.1016/j.actamat.2015.12.051 ↗
13. The combined effect of alumina and silica co-doping on the ageing resistance of 3Y-TZP bioceramics10.1016/j.actbio.2014.09.009 ↗
14. The effect of nano-structured alumina coating on the bond strength of resin-modified glass ionomer cements to zirconia ceramics10.1016/j.jeurceramsoc.2012.03.037 ↗
15. Bonding to oxide ceramics - Laboratory testing versus clinical outcome10.1016/j.dental.2014.06.007 ↗
16. Complexity of the relationships between the sintering-temperature-dependent grain size, airborne-particle abrasion, ageing and strength of 3Y-TZP ceramics10.1016/j.dental.2015.12.004 ↗
17. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
18. Erosive damage depth in ceramics: a study on metastable, tetragonal zirconia10.1111/j.1151-2916.1979.tb18807.x ↗
19. The effects of dental grinding and sandblasting on ageing and fatigue behavior of dental zirconia (Y-TZP) ceramics10.1016/j.jeurceramsoc.2007.09.013 ↗
20. Subsurface evaluation of hydrothermal degradation of zirconia10.1016/j.actamat.2010.09.047 ↗
21. Impact of sandblasting on the mechanical properties and aging resistance of alumina and zirconia based ceramics10.1016/j.jeurceramsoc.2017.10.050 ↗
22. Fracture resistance of endodontically treated maxillary incisors restored with zirconia posts: effect of the internal plateau preparation10.1080/17436753.2018.1508625 ↗
23. Gwyddion: An open-source software for SPM data analysis
24. Structure and thermomechanical properties of partially stabilized zirconia in the CaO-ZrO2 system10.1111/j.1151-2916.1972.tb11241.x ↗
25. The effect of nano-structured alumina coating on resin-bond strength to zirconia ceramics10.1016/j.dental.2010.03.013 ↗
26. Unstable cracking (chipping) of veneering porcelain on all-ceramic dental crowns and fixed partial dentures10.1016/j.actbio.2008.12.016 ↗
27. CAD/CAM-machining effects on Y-TZP zirconia10.1016/j.dental.2003.08.007 ↗
28. X‐ray determination of transformation depths in ceramics containing tetragonal ZrO210.1111/j.1151-2916.1981.tb10285.x ↗
29. Microstructural changes in ground 3Y-TZP and their effect on mechanical properties10.1016/j.actamat.2011.07.024 ↗
30. Surface grain size and texture after annealing ground zirconia10.1016/j.jeurceramsoc.2015.12.022 ↗
31. Phase transformation and subsurface damage in 3Y-TZP after sandblasting10.1016/j.dental.2013.03.005 ↗
32. Effect of sandblasting and residual stress on strength of zirconia for restorative dentistry applications10.1016/j.jmbbm.2013.09.004 ↗
33. Rhombohedral phase produced in abraded surfaces of partially stabilized zirconia (PSZ)10.1007/BF00722220 ↗
34. Rhombohedral phase in Y2O3-partially-stabilized ZrO210.1111/j.1151-2916.1988.tb05776.x ↗
35. Cubic-to-rhombohedral phase transformation in zirconia by ion implantation10.1007/BF00720424 ↗
36. Origin of the hump on the left shoulder of the X-ray diffraction peaks observed in Y2O3-fully and partially stabilized ZrO210.1016/j.jallcom.2003.11.129 ↗
37. Ferroelastic domain switching as a toughening mechanism in tetragonal zirconia10.1111/j.1151-2916.1986.tb07341.x ↗
38. Microstructural changes in 3Y-TZP induced by scratching and indentation10.1016/j.jeurceramsoc.2012.02.026 ↗
39. On a ferroelastic mechanism governing the toughness of metastable tetragonal-prime (t′) yttria-stabilized zirconia
40. Ferroelastic and plastic deformation of t′-zirconia single crystals10.1111/j.1151-2916.2001.tb00911.x ↗
41. Effect of stress and temperature on ferroelastic domain switching of partially stabilized zirconia pseudo-single crystals10.2109/jcersj.104.529 ↗