Abnormal grain growth in iron-containing SiC fibers
Source abstract
Abstract
Abstract Understanding the role of sintering aids during microstructure evolution is critical to the manufacture of densified SiC fibers. A variety of TEM characterization techniques are combined to investigate grain growth behavior in iron-doped SiC fibers. Ultra-large SiC grains in micron size, as the self-assembly of nano sub-grains into a similar orientation, were consistently discovered at the surface and indicative of abnormal grain growth. The growth front consisted of polycrystalline nanograins wetted by iron-rich particles, where several sub-grains were found to unify their (111) planes with a misorientation angle less than 10°, indicating grain rotation at the growth front. It is proposed that iron-rich particles form a quasi-liquid interfacial phase during sintering, which facilitates coherent attachment of grains and results in fast grain growth using neighboring irregular-shaped nanograins as building blocks. The imperfect ordered coalescence of nanograins introduces structural heterogeneities, including low angle grain boundaries and porosities.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Silicon Carbide Semiconductor Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Processing and properties of macroporous silicon carbide ceramics: a review10.1016/j.jascer.2013.07.003 ↗
2. Mechanical properties and structure of a new commercial SiC-type fibre (Tyranno)10.1007/BF01153999 ↗
3. A review of the development of three generations of small diameter silicon carbide fibres10.1007/s10853-006-6566-z ↗
4. Effects of density on the mechanical properties of spark plasma sintered β-SiC10.1016/j.ceramint.2020.02.101 ↗
5. Densification of ultrafine SiC powders10.1007/BF00352770 ↗
6. Mechanical properties of nanostructured silicon carbide consolidated by spark plasma sintering10.1016/j.jeurceramsoc.2012.07.030 ↗
7. Defect control of SiC polycrystalline fiber synthesized from poly-aluminocarbosilane10.1016/j.jeurceramsoc.2016.02.022 ↗
8. Study of the ion-irradiation behavior of advanced SiC fibers by raman spectroscopy and transmission electron microscopy10.1111/jace.13342 ↗
9. Microstructural characterization and fracture properties of SiC-based fibers annealed at elevated temperatures10.1007/s10853-006-0579-5 ↗
10. Oxidation behavior of Tyranno ZMI-SiC fiber/SiC-SiBC matrix composite from 800 to 1200 °C
11. Microstructural evolution of the latest generation of small‐diameter SiC-based fibres tested at high temperatures10.1046/j.1365-2818.1997.d01-620.x ↗
12. Excellent heat resistance of Si-Zr-C-O fibre10.1023/A:1004506300754 ↗
13. Microstructures of a SiC-ZrC ceramic fiber derived from a polymeric precursor10.3390/ma13092142 ↗
14. High-strength alkali-resistant sintered SiC fiber stable to 2200 ℃10.1038/35820 ↗
15. Thermal properties of silicon carbide composites fabricated with chopped Tyranno® Si-Al-C fibres10.1016/j.jeurceramsoc.2005.07.008 ↗
16. Structure and properties of sylramicTM silicon carbide fiber-a polycrystalline stoichiometric β-SiC composition10.1002/9780470294437.ch16 ↗
17. Effect of composition and heat treatment conditions on the tensile strength and creep resistance of SiC-based fibers10.1016/S0955-2219(99)00114-4 ↗
18. Iron nanoparticle-containing silicon carbide fibers prepared by pyrolysis of Fe(CO)5-doped polycarbosilane fibers10.1111/j.1551-2916.2009.03369.x ↗
19. Temperature-dependent microstructure and phase evolution of iron-containing SiC fibers10.1016/j.ceramint.2014.06.011 ↗
20. A development mechanism of graded microstructures in iron-containing SiC fibers revealed by electron microscopy10.1016/j.matchar.2020.110177 ↗
21. Grain growth and interfacial structures in SiC fibers10.1016/j.ceramint.2020.01.021 ↗
22. Anomalous thermal expansion of γ-iron nanocrystals inside multiwalled carbon nanotubes10.1103/PhysRevB.88.081402 ↗
23. Densification of liquid-phase-sintered silicon carbide10.1023/A:1006753213286 ↗
24. Mechanism of grain growth in liquid-phase-sintered β–SiC10.1557/JMR.1999.0581 ↗
25. Development of high tensile strength silicon carbide fibre using an organosilicon polymer precursor10.1038/273525a0 ↗
26. Grain growth by multiple ordered coalescence of nanocrystals during spark plasma sintering of SrTiO3 nanopowders10.1016/j.actamat.2012.08.027 ↗
27. Ordered coalescence of nanocrystallites contributing to the rapid anisotropic grain growth in silicon nitride ceramics10.1016/j.scriptamat.2013.04.017 ↗
28. Direction-specific van der waals attraction between rutile TiO2 nanocrystals10.1126/science.aah6902 ↗
29. In-situ liquid cell transmission electron microscopy investigation on oriented attachment of gold nanoparticles10.1038/s41467-018-02925-6 ↗
30. Formation mechanism of large SiC grains on SiC fiber surfaces during heat treatment10.1039/C6CE00427J ↗
31. Surface finish effects and the strength-grain size relation in SiC10.1111/j.1151-2916.1977.tb14112.x ↗