journal article·2022-07Open access

Micromechanical properties of vapour-exposed SiCf/BN/SiC ceramic-matrix composites

Robin M.G. De Meyere, Louise Gale, Stephen Harris, Ian Edmonds, Adam L. Chamberlain, Thomas J. Marrow, David E.J. Armstrong

Abstract

SiCf/BN/SiC Ceramic-Matrix Composites are candidate materials for aero-engines, but their interphase stability after potential low-temperature water-vapour exposures during flight cycles is not well known. The examination of these composites exposed for 50, 250 and 500 h at low temperature (65 °C) and 95% relative humidity was therefore performed, in order to understand if resulting oxidation products affected the mechanical properties at the micro-scale. The composites were subject to fibre push-out tests to compare pristine from degraded composites. It was found that whilst the sample exposed for 50 h had no significant change from pristine, the samples exposed for 250 and 500 h had a clear decrease in interfacial shear strengths measured. Parallel studies also revealed that whilst damage was strongly localised, the diffusion of water within the composite was not fully complete at exposure times between 50 and 250 h. The permeability of the CMC was shown to be affected at longer exposure times where differences in mechanical performances even between tows and within tows were noted.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Bansal, N.P. & Lamon, J. Ceramic matrix composites: materials, modeling and technology.
2. Degradation mechanisms of SiC/BN/SiC after low temperature humidity exposure10.1016/j.jeurceramsoc.2020.05.007 ↗
3. Consequence of intermittent exposure to moisture and salt fog on the high‐temperature fatigue durability of several ceramic‐matrix composites10.1111/j.1151-2916.2003.tb03464.x ↗
4. Hi-NicalonTM-SSiC fiber oxidation and scale crystallization kinetics10.1111/j.1551-2916.2011.04647.x ↗
5. Borosilicate glass-induced fiber degradation of SiC/BN/SiC composites exposed in combustion environments10.1111/ijac.12499 ↗
6. Degradation of a SiC‐SiC composite in water vapor environments
7. Silicon carbide oxidation in steam up to 2 MPa10.1111/jace.13094 ↗
8. General relationship for the thermal oxidation of silicon10.1063/1.1713945 ↗
9. Modeling environmental degradation of SiC-based fibers10.1111/jace.14086 ↗
10. Effects of Microstructural Instability on the Creep Behavior of Si-C-O (Nicalon) Fibers in Argon10.1111/j.1151-2916.1993.tb06608.x ↗
11. Fibre-reinforced multifunctional SiC matrix composite materials10.1080/09506608.2016.1213939 ↗
12. A review of SiC fiber oxidation with a new study of Hi-Nicalon SiC fiber oxidation10.1002/adem.201600166 ↗
13. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
14. High-temperature stability of SiC-based composites in high-water-vapor-pressure environments10.1111/j.1151-2916.2003.tb03463.x ↗
15. Hay, R.S. & Petry, D. Fiber strength with coatings from sols and solutions. in Proceedings of the 20th Annual Conference on Composites, Advanced Ceramics, Materials, and Structures-B: Ceramic Engineering and Science Proceedings, Volume 17, Issue 4 43–52 (John Wiley & Sons, Inc., 2009).10.1002/9780470314876.ch3 ↗
16. Models of high-temperature, environmentally assisted embrittlement in ceramic-matrix composites10.1111/j.1151-2916.1996.tb08982.x ↗
17. Intermediate temperature oxidative strength degradation of a SiC/SiNC composite with a polymer-derived matrix10.1111/jace.14741 ↗
18. Cabet. Review: Oxidation of SiC/SiC Composites in Low Oxidising and High Temperature Environment. Mater. Issues Gener. IV Syst. (2008). doi:10.1007/978–1-4020–8422-5.10.1007/978-1-4020-8422-5_18 ↗
19. Boria fluxing of SiC in ceramic matrix composite aeropropulsion applications10.1149/MA2015-01/13/1122 ↗
20. Oxidation of BN-coated SiC fibers in ceramic matrix composites10.1111/j.1151-2916.1996.tb08163.x ↗
21. Interface characterization by TEM, AES and SIMS in tough SiC (ex-PCS) fibre-SiC (CVI) matrix composites with a BN interphase10.1007/BF01159815 ↗
22. Wing · 2016
23. High-temperature oxidation of boron nitride: II, boron nitride layers in composites10.1111/j.1151-2916.1999.tb01944.x ↗
24. Model of oxidation-induced fiber fracture in SiC/SiC composites10.1111/jace.13180 ↗
25. High-Temperature Oxidation of Boron Nitride: I, Monolithic Boron Nitride10.1111/j.1551-2916.1999.tb20075.x ↗
26. Degradation mechanisms of a SiC fiber reinforced self-sealing matrix composite in simulated combustor environments10.1016/j.jeurceramsoc.2006.02.042 ↗
27. Singh, D., Zhu, D., Zhu, Y. & Singh, M. (Mrityunjay). Design, development, and applications of engineering ceramics and composites. in 8th Pacific Rim Conference on Ceramic and Glass Technology, May 31-June 5, 2009, Vancouver, British Columbia 336 (Wiley, 2010).
28. Oxidative and hydrolytic stability of boron nitride — a new approach to improving the oxidation resistance of carbonaceous structures10.1016/0008-6223(94)00163-T ↗
29. Preparation, properties and applications of boron nitride thin films10.1016/0040-6090(88)90008-9 ↗
30. Stability to moisture for chemically vapour-deposited boron nitride10.1007/BF01174496 ↗
31. Degradation of boron nitride interfacial coatings fabricated by chemical vapor infiltration on SiC fibers under ambient air/room temperature conditions10.1016/j.ceramint.2018.12.191 ↗
32. Microstructural Stability of Nicalon at 1000deg; C in Air after Exposure to Salt (NaCl) Water10.1111/j.1151-2916.1995.tb08927.x ↗
33. Kim · 2009 · 103
34. Measurement of interfacial fracture energy by single fibre push-out testing and its application to the titanium–silicon carbide system10.1016/S1359-6454(98)00009-3 ↗
35. Properties of Multilayered Interphases in SiC/SiC Chemical-Vapor-Infiltrated Composites with “Weak” and “Strong” Interfaces10.1111/j.1151-2916.1998.tb02627.x ↗
36. Optimizing the fibre push-out method to evaluate interfacial failure in SiC/BN/SiC ceramic matrix composites
37. A novel trench fibre push-out method to evaluate interfacial failure in long fibre composites10.1557/s43578-021-00153-1 ↗