journal article·2010-03

Effect of the specimen size on strength of Si3N4+SiC composite

Lucia Hegedűsová, Monika Kašiarová, Erika Csehová, Ján Dusza

Publisher page

Abstract

Abstract Bending and contact strength of a recently developed carbon derived Si3N4 + SiC micro/nanocomposite have been investigated in four-point and opposite sphere modes using specimens with two different sizes of 3 mm × 4 mm × 45 mm and 1 mm × 2 mm × 20 mm. The fracture origins during bending test were clusters of pores and large SiC grains with different size, shape and location, which resulted in relatively low strength (675 MPa and 832 MPa) and Weibull moduli (6.4 and 8.6). The fracture origins in specimens tested in contact mode were cone cracks, originated and arised during the loading, and their similar size and shape, together with the preexisting stress field resulted in high strength (1167 MPa and 1997 MPa) and relative high Weibull moduli (17 and 15). In agreement with the theory, bending test specimens with smaller effective volume exhibited higher strength. In contact test, interaction of cone cracks occured in the small specimens at lower load as in larger one, which resulted in the lower strength of small specimens.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Perspective on the development of high-toughness ceramics10.1111/j.1151-2916.1990.tb06493.x ↗
2. Microstructural design of silicon nitride with improved fracture toughness. I. Effects of grain shape and size10.1111/j.1151-2916.1998.tb02702.x ↗
3. Unique opportunities for microstructural engineering with duplex and laminar ceramic composites10.1111/j.1151-2916.1992.tb07188.x ↗
4. New design concept of structural ceramics: ceramic nanocomposites: composites10.2109/jcersj.99.974 ↗
5. Structural ceramic nanocomposites10.1016/S0955-2219(96)00222-1 ↗
6. Silicon nitride/silicon carbide nanocomposite materials. I. Fabrication and mechanical properties at room temperature10.1111/j.1151-2916.1998.tb02456.x ↗
7. High-temperature strength and microstructural analysis in Si3N4/20vol%–SiC nanocomposites10.1111/j.1151-2916.1999.tb01863.x ↗
8. SiC/Si3N4 nano/micro-composite—processing, RT and HT mechanical properties10.1016/S0955-2219(99)00176-4 ↗
9. Munz · 1996
10. Design data for engineering ceramics: a review of the flexure test10.1111/j.1151-2916.1991.tb08259.x ↗
11. Weibull · 1939
12. Hertz, H.H., On the contact of elastic solids. J. Reine. Angew. Math., 1881, 92, 156–171. Translated and reprinted in English, In Hertz's Miscellaneous Papers, ed. P. Lenard. Chs. 5 and 6. Authorized English translation by D. E. Jones and G. A. Schott. Macmillan, London, U.K., 1896.
13. Indentation of ceramics with spheres: a century after Hertz10.1111/j.1151-2916.1998.tb02580.x ↗
14. Lawn · 1993
15. Measurement of the fracture properties of brittle solids by Hertzian indentation10.1016/0001-6160(78)90087-1 ↗
16. The Hertzian stress field and formation of cone cracks. I. Theoretical approach10.1016/0956-7151(92)90328-C ↗
17. The Hertzian stress field and formation of cone cracks. II. Determination of fracture toughness10.1016/0956-7151(92)90329-D ↗
18. Statical determination of surface flaw distributions in brittle materials10.1016/0955-2219(95)00005-F ↗
19. Surface mechanical analyses by Hertzian indentation10.1590/S0366-69132004000200005 ↗
20. Angle of Hertzian cone cracks10.1111/j.1151-2916.1998.tb02542.x ↗
21. Test devices for strength measurements of bars under contact loading
22. Fett · 2000
23. Contact strength measurements of bars under opposite sphere loading10.1023/A:1021668932660 ↗
24. Fatigue of alumina under contact loading10.1016/S0013-7944(02)00094-2 ↗
25. Sphere contact fatigue of coarse grained Al2O3 ceramic10.1111/j.1460-2695.2006.01047.x ↗
26. Influence of stress gradients on failure in contact strength tests with cylinder loading10.1016/S0013-7944(01)00147-3 ↗
27. Weibull analysis of ceramics under high stress gradients10.1016/S0955-2219(03)00024-4 ↗
28. Fractography and fracture mechanics property assessment of advanced structural ceramics10.1179/095066099101528270 ↗
29. Mechanical failure of advanced ceramics: the value of fractography10.4028/www.scientific.net/KEM.223.1 ↗
30. Dusza · 1998 · 187
31. Fractographic montage for a Si3N4–SiC nanocomposite10.1111/j.1551-2916.2006.00956.x ↗
32. Quinn · 1991 · vol. 4
33. Hegedűsová, L., Contact strength and fatigue of ceramic materials. Ph.D. Thesis, Institute of Materials Research, Slovak Academy of Sciences, Košice, 2008.