Hot corrosion behaviour of barium-strontium aluminosilicates in a molten Na 2 SO 4 environment
Source abstract
Abstract
Abstract The hot corrosion behaviour of barium-strontium aluminosilicates (B 1− x S x AS) attacked by Na 2 SO 4 was investigated in the temperature range from 900 to 1100 °C and the weight change was measured as a function of the corrosion time. The surfaces and cross-sections of the corroded samples were observed by scanning electron microscopy in backscattered electron mode and energy-dispersive X-ray spectroscopy. The phase composition was characterized by X-ray diffraction. The results indicate that the hot corrosion of B 1 − x S x AS by molten Na 2 SO 4 was controlled by a diffusion-reaction mechanism. The strontium and/or barium cations diffused out of their aluminosilicate network, and the vacant sites were filled by sodium cations diffusing into the structure to form a NaAlSiO 4 on the top. Due to their smaller radius, the strontium atoms showed a faster diffusion rate than the barium atoms. The corrosion depth significantly increased with the temperature and the strontium concentration in the B 1 −x S x AS.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Nuclear materials and radiation effects · Concrete and Cement Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Design, fabrication, and application of thermostructural composites (TSC) like C/C, C/SiC, and SiC/SiC composites10.1002/adem.200290001 ↗
2. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
3. Current status and recent research achievements in SiC/SiC composites10.1016/j.jnucmat.2014.06.003 ↗
4. Self-healing mechanisms of a SiC fiber reinforced multi-layered ceramic matrix composite in high pressure steam environments10.1016/j.jeurceramsoc.2006.06.007 ↗
5. Mechanical behaviour and lifetime modelling of self-healing ceramic-matrix composites subjected to thermomechanical loading in air10.1016/j.compositesa.2008.10.020 ↗
6. Corrosion of silicon-based ceramics in combustion environments10.1111/j.1151-2916.1993.tb03684.x ↗
7. Observations of accelerated silicon carbide recession by oxidation at high water-vapor pressures10.1111/j.1151-2916.2000.tb01172.x ↗
8. Degradation mechanisms of a SiC fiber reinforced self-sealing matrix composite in simulated combustor environments10.1016/j.jeurceramsoc.2006.02.042 ↗
9. Reactivity of a C/SiC composite in water vapour10.1016/S0955-2219(00)00207-7 ↗
10. Kinetics and mechanism of corrosion of SiC by molten salts10.1111/j.1151-2916.1986.tb04698.x ↗
11. Corrosion of SiC/SiC composite in Na2SO4 vapor environments from 1000 to 1500°C10.1016/j.compositesa.2005.07.010 ↗
12. Review –volcanic ash and its influence on aircraft engine components10.1016/j.proeng.2014.12.604 ↗
13. Corrosion failures in gas turbine hot components10.1007/s11668-012-9571-3 ↗
14. Hot corrosion of α-SiC ceramics by V2O5 melt10.1007/BF01045359 ↗
15. Current status of environmental barrier coatings for Si-based ceramics
16. Performance of thermally sprayed Si/mullite/BSAS environmental barrier coatings exposed to thermal cycling in water vapor environment10.1016/j.surfcoat.2012.11.043 ↗
17. Accelerated oxidation of SiC CMC's by water vapor and protection via environmental barrier coating approach10.1016/S0955-2219(02)00141-3 ↗
18. High temperature water vapour corrosion of rare earth disilicates (Y,Yb,Lu)2Si2O7 in the presence of Al(OH)3 impurities10.1016/j.jeurceramsoc.2006.09.013 ↗
19. Influence of temperature and hot corrosion on the micro-nanomechanical behavior of protective mullite EBCs10.1016/j.ijrmhm.2014.09.025 ↗
20. Stability of interfaces in hybrid EBC/TBC coatings for Si-based ceramics in corrosive environments10.1016/j.ijrmhm.2014.08.013 ↗
21. Hot corrosion of γ-Y2Si2O7 in strongly basic Na2CO3 molten salt environment10.1016/j.jeurceramsoc.2007.05.011 ↗
22. Upper temperature limit of environmental barrier coatings based on mullite and BSAS10.1111/j.1151-2916.2003.tb03466.x ↗
23. Evaluation of CFCC liners with EBC after field testing in a gas turbine10.1016/S0955-2219(02)00142-5 ↗
24. Exploration of YPO4 as a potential environmental barrier coating10.1016/j.ceramint.2009.10.014 ↗
25. Corrosion of barium aluminosilicates by water-vapour: an investigation from first principles10.1016/j.corsci.2009.05.040 ↗
26. Hot corrosion behavior of barium aluminosilicate-coated C/SiC composites at 900°C10.1111/j.1551-2916.2009.03339.x ↗