journal article·2015-02

Oxidation behaviors and microstructural alterations of a Mo(Si,Al)2-based composite after heating at 1580°C either in a furnace (ex-situ) or via alternating current (in-situ)

Kristina Hellström, Petter Persson, Erik Ström

Publisher page

Abstract

The commercial heating element Kanthal Super ER (Mo(Si,Al)(2)-based composite) was oxidized at 1580 degrees C for 24 h up to 1 year using two methods: (1) a furnace set at the desired temperature, (2) passing an alternating current (AC) through the material. Initially, the oxidation behaviors appeared similar for the AC- and furnace-exposed materials. However, at longer exposure times, the level of Al depletion was more pronounced in the furnace-exposed material. A dense alumina scale formed with the same thickness during the two types of exposures, although a porous outer alumina scale was also formed on the composite that was heated in the furnace. The bulk microstructures were also different, in that dark regions in a circle were noted on the AC-exposed material, while the dark regions were evenly distributed on the furnace-exposed material. These dark regions consisted of agglomerated Mo-5(Si,Al)(3) and Al2O3. The AC-exposed material also has "bands" where Al2O3 have agglomerated.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Intermetallics and Advanced Alloy Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. The beneficial effect of water vapour on the oxidation at 600 and 700 degrees C of a MoSi2-based composite10.1016/j.jeurceramsoc.2004.01.005 ↗
2. High-temperature oxidation of MoSi210.1007/s10853-009-4012-8 ↗
3. On the mechanism of MoSi2 pesting in the temperature range 400–500C
4. Oxidation behaviour of a MoSi2-based composite in different atmospheres in the low temperature range (400–550 degrees C)10.1016/j.jeurceramsoc.2003.11.024 ↗
5. Low temperature oxidation of fully dense and porous MoSi210.1016/S0921-5093(98)01078-8 ↗
6. Effect of third element on the pesting suppression of Mo–Si–X intermetallics (X=Al, Ta, Ti, Zr and Y)10.1016/0966-9795(96)00019-2 ↗
7. Effect of Al addition on the microstructure and low-temperature reactivity to oxygen of pre-formed MoSi210.1007/s10853-012-6623-8 ↗
8. Oxidation kinetics and composite scale formation in the system Mo(Al,Si)(2)10.1111/j.1151-2916.2002.tb00109.x ↗
9. Influences of Al content and secondary phase of Mo-5(Si,Al)(3) on the oxidation resistance of Al-rich Mo(Si,Al)(2)-base composites10.1016/S0966-9795(03)00072-4 ↗
10. Microstructure and properties stability of Al-alloyed MoSi2 matrix composites10.1016/j.intermet.2003.10.001 ↗
11. The intermediate and high temperature oxidation behaviour of Mo(Si1−xAlx)(2) intermetallic alloys10.1016/S0966-9795(96)00068-4 ↗
12. High-temperature oxidation of intermetallic compounds of Mo(Si1−xAlx)210.1016/0010-938X(93)90312-5 ↗
13. High temperature oxidation and pesting of Mo(Si,Al)210.1016/S0921-5093(97)00673-4 ↗
14. Oxidation behavior of a Mo (Si,Al)(2)-based composite at 300–1000 degrees C10.1016/j.intermet.2009.10.019 ↗
15. Oxidation behavior of a Mo(Si,Al)(2) composite at 900–1600 degrees C in dry air10.1007/s10853-012-6906-0 ↗
16. Oxidation behaviour of a Mo(Si,Al)(2) based composite at 1500 degrees C10.1016/j.intermet.2011.05.002 ↗
17. The role of microstructure on pesting during oxidation of MoSi2 and Mo(Si,Al)2 at 773K10.1007/BF01668515 ↗
18. Isothermal and cyclic oxidation of Mo(Si1−x, Alx)(2) up to 2048K10.2320/matertrans1989.34.1200 ↗
19. Sundberg · Ceram Int · 2004 · 30 · 189910.1016/j.ceramint.2003.12.046 ↗
20. Microstructural investigation of the initial oxidation at 1450 degrees C and 1500 degrees C of a Mo(Si,Al)(2)-based composite10.3184/096034009X464195 ↗
21. Evaporation behavior of SiO2 in N2O–2H2O atmospheres10.2320/matertrans.45.334 ↗
22. Polymeric gaseous species in the sublimation of Molybdenum trioxide10.1063/1.1743417 ↗
23. Interactions of water vapor with oxides at elevated temperatures10.1016/j.jpcs.2004.06.044 ↗
24. Thermodynamic reassessment of the Mo–Si and Al–Mo–Si systems10.1016/S0966-9795(00)00068-6 ↗