journal article·2021-10

Preparation of a novel Sr-Zr oxide refractory for induction melting of high-activity alloy

Yubin Xiao, Guangyao Chen, Feihai Yu, Xiao Hou, Yin Zhang, Xingli Zou, Xionggang Lu, Chonghe Li

Publisher page

Abstract

Abstract In this study, a new Sr-Zr oxide refractory was designed and prepared through a solid-state reaction method according to the mole ratio of n(SrO): n(ZrO2) = 2:1. The results reveal that the Sr-Zr oxide refractory consisted of three phases, i.e., Sr2ZrO4, Sr3Zr2O7 and SrO. The thermodynamically stable phase Sr2ZrO4 was hard to form completely due to the limitation of reaction kinetics between SrCO3 and ZrO2, and thus Sr3Zr2O7 and SrO coexisted in the Sr-Zr oxide refractory. The composite refractory exhibited a good corrosion resistance during the melting of TiNi alloy melts, and only a slight interaction occurred in the refractory crucible after melting, with the formation of a reaction layer (28 μm in thickness). In addition, the oxygen concentration of the prepared TiNi alloys was determined to be only 0.046 wt.%. These results indicate that the Sr-Zr oxide composites have potential to be used as a refractory candidate for the induction melting of high-activity alloys.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Shape Memory Alloy Transformations · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Current situation and development trend of zirconium and zirconium alloys
2. On the reaction between NiTi melts and crucible graphite during vacuum induction melting of NiTi shape memory alloys10.1016/j.actamat.2005.05.004 ↗
3. Effect of interaction of refractories with Ni-based superalloy on inclusions during vacuum induction melting10.1007/s12613-020-2098-9 ↗
4. Viswanathan · 2008 · 1
5. Predicting thermodynamic stability of crucible oxides in molten titanium and titanium alloys10.1016/j.commatsci.2006.03.006 ↗
6. Recent developments in the research of shape memory alloys10.1016/S0966-9795(98)00070-3 ↗
7. Deformation and degradation of superelastic NiTi under multiaxial loading10.1016/j.actamat.2019.01.047 ↗
8. A comparison of chemistry and inclusion distribution and morphology versus melting method of NiTi alloys10.1007/s11665-009-9438-2 ↗
9. Interaction between refractory crucible materials and the melted NiTi shape-memory alloy10.1007/s11663-005-0068-2 ↗
10. Interfacial reactions between zirconia and titanium10.1016/S1359-6462(98)00328-5 ↗
11. The segregation of chemical composition in NiTi shape memory alloy melted by VIM in lime crucible10.4028/www.scientific.net/MSF.610-613.1315 ↗
12. Induction melting of NiTi shape memory alloys - the influence of the commercial crucible graphite on alloy quality, Materialwiss10.1002/mawe.200400725 ↗
13. Interactions between Ni-44Ti-5Al-2Nb-Mo alloy and oxide ceramics during directional solidification process10.1007/s10853-012-6577-x ↗
14. On the modification of hydration resistance of CaO with ZrO2 additive10.1111/ijac.12606 ↗
15. Interaction between the ceramic CaZrO3 and the melt of titanium alloys10.4028/www.scientific.net/AST.70.136 ↗
16. Preparation of SrZrO3 refractory and study on its compatibility with molten titanium alloys
17. Dissolution of BaZrO3 refractory in titanium melt10.1111/ijac.13009 ↗
18. On the evaluation of stability of rare earth oxides as face coats for investment casting of titanium10.1007/BF02667869 ↗
19. Investigating the corrosion resistance of calcium zirconate in contact with titanium alloy melts10.1016/j.jeurceramsoc.2014.08.031 ↗
20. System SrO‐ZrO2
21. Particularities of the technology of high-density technical ceramics. Sintering of oxide ceramic10.1007/s10717-009-9103-0 ↗
22. X-ray characterization of Sr3Zr2O7 hydrate10.1007/BF00552923 ↗
23. 2005
24. Hydration structures of MgO, CaO, and SrO (001) surfaces10.1021/acs.jpcc.6b07434 ↗
25. Corrosion mechanism of BaZrO3 refractory in titanium enrichment melt