Development of a hoop-strength test for model sphero-cylindrical dental ceramic crowns: FEA and fractography
Source abstract
Abstract
Abstract Here we describe the development of a mechanical test that simulates a circumferential “hoop-stress” at the margins of model dental ceramic crowns. A simplified sphero-cylindrical geometry was modelled in two thicknesses and machined out of two glass-ceramic materials. The specimens were loaded by a conical metallic piston to induce circumferential hoop-stresses at the margins until fracture. Broken specimens were fractographically analyzed to determine the location of the fracture origin and to measure the dimensions of the critical defect, allowing the calculation of the stress at failure from fracture mechanics relations. For thick specimens, machining defects at the outer margins barely played a role in fracture initiation. For thin specimens, outer defects started to dominate the failure mode. CAD/CAM machining showed to predispose thinner margins to early fracture. Crowns should be designed with increased thickness in order to minimize the effect of marginal damage in the circumferential stress field inducing fracture.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Dental Implant Techniques and Outcomes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Fracture rates and lifetime estimations of CAD/CAM all-ceramic restorations10.1177/0022034515608187 ↗
2. Report on fractures of trilayered all-ceramic fixed dental prostheses10.1016/j.csefa.2016.10.001 ↗
3. Fractographic analyses of all-ceramic crowns: a study of 27 clinically failed crowns10.1016/j.dental.2013.03.018 ↗
4. Fracture origins in twenty-two dental alumina crowns10.1016/j.jmbbm.2015.08.006 ↗
5. Chipping fracture resistance of dental CAD/CAM restorative materials: part 2. Phenomenological model and the effect of indenter type10.1016/j.dental.2014.02.014 ↗
6. Grinding damage assessment for CAD-CAM restorative materials10.1016/j.dental.2016.12.004 ↗
7. Hard machining, glaze firing and hydrofluoric acid etching: Do these procedures affect the flexural strength of a leucite glass-ceramic?10.1016/j.dental.2015.04.005 ↗
8. Strength-limiting damage in lithium silicate glass-ceramics associated with CAD-CAM10.1016/j.dental.2018.11.004 ↗
9. Fracture surface characterization of clinically failed all-ceramic crowns10.1111/eos.12128 ↗
10. Machining cracks in finished ceramics, Fractography of Advanced Ceramics
11. Fractographic analyses of all-ceramic restorations
12. Clinically relevant fracture testing of all-ceramic crowns10.1016/j.dental.2013.04.026 ↗
13. Spatial distribution of residual stresses in glass-ZrO2 sphero-cylindrical bilayers10.1016/j.jmbbm.2016.03.013 ↗
14. Chairside CAD/CAM materials. Part 1: measurement of elastic constants and microstructural characterization10.1016/j.dental.2016.10.009 ↗
15. International · 2015
16. Fracture toughness testing of biomedical ceramic-based materials using beams, plates and discs10.1016/j.jeurceramsoc.2018.08.012 ↗
17. Surface crack in tension or in bending - A reassessment of the Newman and Raju formula in respect to fracture toughness measurements in brittle materials10.1016/j.jeurceramsoc.2012.01.011 ↗
18. Corrigendum to "Surface crack in tension or in bending - A reassessment of the Newman and Raju formula in respect to fracture toughness measurements in brittle materials (vol 32, pg 1491, 2012)"10.1016/j.jeurceramsoc.2017.05.008 ↗
19. Belli · 2019
20. Chairside CAD/CAM materials. Part 2: flexural strength testing10.1016/j.dental.2016.10.008 ↗
21. Monte Carlo simulations of strength distributions of brittle materials - Type of distribution, specimen and sample size
22. Fracture of ceramics10.1002/adem.200700347 ↗
23. Carson · 2014