Highly porous Sr-doped TiO2 ceramics maintain compressive strength after grain boundary corrosion
Source abstract
Abstract
Maintaining sufficient mechanical support during bone healing is an essential property for ceramic bone scaffolds. However, grain boundary (GB) dissolution may compromise the mechanical strength of polycrystalline ceramics in the physiological environment. Therefore, we investigated the GB formation and its impact on the compressive strength and corrosion behavior in TiO2 scaffolds doped with calcium and strontium. To alter the GB composition and densification process, sintering conditions were altered. Prolonged sintering times and increased sintering temperature led to improved densification and increased strength in Ca-doped scaffolds. However, dissolution of the resulting amorphous GBs caused a significant loss of compressive strength when exposed to an acidic environment. In contrast, a crystalline SrTiO3 GB phase present in Sr-doped scaffolds, for which increased sintering temperature combined with rapid cooling led to a significantly improved compressive strength. Formation of SrTiO3 crystals in the GBs maintained the strength for over 4 weeks in an acidic environment.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Bone Tissue Engineering Materials · Orthopaedic implants and arthroplasty · Orthopedic Infections and Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Development of TiO2 photocatalyst reaction for water purification10.1016/S1383-5866(02)00157-0 ↗
2. Generation of low-molecular-weight organic compounds in water by titania photocatalyst under UV-Vis light radiation10.1163/156856708784040623 ↗
3. Influence of process parameters on the photodegradation of synthesized azo pyridone dye in TiO2 water suspension under simulated sunlight10.1080/10934529.2011.526905 ↗
4. Apatite-coated titanium dioxide photocatalyst for air purification10.1016/j.cattod.2004.06.112 ↗
5. Processing of highly porous TiO2 bone scaffolds with improved compressive strength10.1016/j.jeurceramsoc.2012.08.016 ↗
6. TiO2 scaffolds in peri‐implant dehiscence defects: an experimental pilot study10.1111/clr.12725 ↗
7. A novel ultra-porous titanium dioxide ceramic with excellent biocompatibility10.1177/0885328209354925 ↗
8. TiO2 scaffolds sustain differentiation of MC3T3-E1 cells10.1166/jbt.2012.1055 ↗
9. Formation and adhesion of biomimetic hydroxyapatite deposited on titanium substrates10.1016/j.actbio.2007.03.006 ↗
10. Bone formation in TiO2 bone scaffolds in extraction sockets of minipigs10.1016/j.actbio.2012.02.020 ↗
11. Grain boundary corrosion of highly porous ceramic TiO2 foams is reduced by annealing and quenching10.1016/j.jeurceramsoc.2015.09.014 ↗
12. Grain boundary corrosion in TiO2 bone scaffolds doped with group II cations10.1016/j.jeurceramsoc.2018.12.055 ↗
13. Bone structure and metabolism10.1016/j.mpmed.2013.07.007 ↗
14. Microelectrode studies on the acid microenvironment beneath adherent macrophages and osteoclasts10.1016/0014-4827(88)90191-7 ↗
15. Corrosion of ceramics in aqueous hydrofluoric acid10.1111/j.1151-2916.2000.tb01348.x ↗
16. Theory of corrosion of glass and ceramics, Corrosion of glass
17. Atomic layer deposited TiO2 protects porous ceramic foams from grain boundary corrosion10.1016/j.corsci.2016.01.023 ↗
18. Protection of silicon nitride ceramics against corrosion in acidic aqueous solutions by enforced internal passivation10.1016/S0272-8842(03)00098-1 ↗
19. Silica and magnesia dopant distributions in alumina by high‐resolution scanning secondary ion mass spectrometry10.1111/j.1151-2916.1999.tb01866.x ↗
20. Silicon nitride for high‐temperature applications10.1111/j.1551-2916.2010.03839.x ↗
21. Coagulated concentrated anatase slurry leads to improved strength of ceramic TiO2 bone scaffolds10.1016/j.ceramint.2018.01.013 ↗
22. Epoxy interface method enables enhanced compressive testing of highly porous and brittle materials10.1016/j.ceramint.2015.09.045 ↗
23. Carter · 2007
24. Rahaman · 2017
25. Kwon · 2001
26. Strongly connected ex situ MgB2 polycrystalline bulks fabricated by solid-state self-sintering10.1088/0953-2048/25/11/115022 ↗
27. Phase diagram and structure of melts of the system CaO—TiO2—SiO2
28. Densification and mechanical properties of titanium diboride with silicon nitride as a sintering aid10.1111/j.1151-2916.1999.tb02199.x ↗
29. Densification, sintering reactions, and properties of titanium diboride with titanium disilicide as a sintering aid10.1111/j.1551-2916.2007.01911.x ↗
30. Structural effects on glass stability and crystallization10.1039/C7CE02135F ↗
31. Effects of donor concentration and oxygen partial pressure on interface morphology and grain growth behavior in SrTiO310.1016/S1359-6454(02)00139-8 ↗