journal article·2021-12

Novel design of YIG/MTC heterogeneous joint bonded by glass ceramic after amorphous glass cladding

Qianqian Chen, Tiesong Lin, Panpan Lin, Dian Ma, Hiroyuki Inoue, Peng He

Publisher page

Abstract

Abstract A new method of pre-cladding amorphous glass and glass-ceramic brazing was invented to obtain a high-reliability bonding of yttrium iron garnet ferrite (YIG) and magnesium titanate ceramic (MTC) at a relatively low temperature of 725oC. The amorphous glass cladding could alleviate the stress generated by thermal expansion difference between the glass ceramic and base materials. The microstructure shows that micron-scale and nanoscale CoFe2O4 phases were dispersed in the glass seam. The joint shear strength reached 117 ± 6.6 MPa due to the enhancement of CoFe2O4 phases, which was twice as that of the joint directly brazed by amorphous bismuth glass. Correspondingly, the joint weak area was transferred from the glass matrix to the vicinity of the interface and the base material, providing a direct evidence that the glass seam was strengthened by the glass ceramic. It is significant for improving high reliability of the microwave devices for long-term service.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microwave Dielectric Ceramics Synthesis · Magneto-Optical Properties and Applications · Ferroelectric and Piezoelectric Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Magnetic behavior of Ga doped yttrium iron garnet ferrite thin films deposited by sol-gel technique10.1016/j.ceramint.2020.07.217 ↗
2. Yttrium iron garnet: properties and applications review. Solid State Phenomena
3. Thermomagnetization characteristics and ferromagnetic resonance linewidth broadening mechanism for Ca-Sn Co-substituted YIG ferrites10.1016/j.ceramint.2018.03.249 ↗
4. Polycrystalline Bi substituted YIG ferrite processed via low temperature sintering10.1016/j.jallcom.2016.10.201 ↗
5. Magnetic performance and structural evaluation of La, Ce, Bi-substituted yttrium iron garnets10.1016/j.ceramint.2020.05.258 ↗
6. Effect of consolidation parameters on structural, microstructural and electrical properties of magnesium titanate ceramics10.1016/j.ceramint.2016.03.088 ↗
7. High-Q microwave dielectric materials based on the spinel Mg2TiO410.1111/j.1551-2916.2006.01271.x ↗
8. Concentrated solar energy used for sintering magnesium titanates for electronic applications10.1016/j.apsusc.2017.09.224 ↗
9. Formation enthalpy and magnetic properties of Bi-YIG powders10.1016/j.ceramint.2008.08.005 ↗
10. Magneto-dielectric composite based on Y3Fe5O12–CaTiO3 for radio frequency and microwave applications10.1016/j.jallcom.2018.12.366 ↗
11. Joining ZTA ceramic by using Dy2O3-Al2O3-SiO2 glass ceramic filler10.1016/j.jeurceramsoc.2020.06.011 ↗
12. Structure and properties of Fe2O3-doped 50Li2O-10B2O3-40P2O5 glass and glass-ceramic electrolytes10.1016/j.ssi.2019.115177 ↗
13. Synthesis and evaluation of a glass-ceramic system containing zinc ferrite nanocrystals10.1016/j.jnoncrysol.2021.120704 ↗
14. Joining alumina ceramic by using glass ceramic filler with high crystallinity for high temperature application10.1016/j.ceramint.2019.06.285 ↗
15. Joining of AlON ceramics by using β-SiAlON/Y-Si-Al-O-N glass-ceramic as interlayer10.1016/j.jnoncrysol.2018.10.027 ↗
16. The application of Lu-Al-Si-O-N oxynitride glass in transparent AlON ceramics joining10.1016/j.ceramint.2018.10.193 ↗
17. Joining of SiC ceramics using CaO-Al2O3-SiO2 (CAS) glass ceramics10.1016/j.jeurceramsoc.2019.09.030 ↗
18. Application of Nd2O3-Al2O3-SiO2 glass solder for joining of silicon carbide components10.1016/j.jeurceramsoc.2016.01.020 ↗
19. Zero stress-optic bismuth oxide-based glass10.1016/j.jnoncrysol.2017.10.023 ↗
20. A new design of the YIG/MTC joint brazed by bismuth-based glass10.1016/j.jeurceramsoc.2018.12.014 ↗