Spinel saturation of a PbO based slag as a method to mitigate the chemical degradation of magnesia-chromite bricks
Source abstract
Abstract
Abstract For nonferrous smelters, the chemical wear of the magnesia-chromite bricks caused by the direct contact with the slag leads to regular replacement of the lining before complete failure. This is a costly and time intensive procedure. Increasing the lining’s lifetime, by reducing the chemical wear, would result in a reduction of both the installation cost and the production losses. In this paper, the potential of changing the slag composition to limit the chemical dissolution rate by saturating the slag in spinel components is investigated by isothermal static finger tests. When saturating the slag in spinel by adding Fe 2 O 3 , a spinel layer forms at the interface between the refractory sample and the liquid slag. As the dissolution of MgO from the refractory in the slag is now controlled by solid state diffusion through the new spinel layer, the chemical wear rate is substantially decreased, thereby increasing the lifetime of the lining.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Iron and Steelmaking Processes · Metal Extraction and Bioleaching
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Refractory materials for the copper and lead industry
2. Refractories for the copper and lead industry
3. Degradation mechanisms and use of refractory linings in copper production processes: a critical review10.1016/j.jeurceramsoc.2013.10.005 ↗
4. Refractories in copper production
5. Melt corrosion of oxide and oxide–carbon refractories10.1179/095066099101528234 ↗
6. Chemical corrosion mechanisms of magnesia-chromite and chrome-free refractory bricks by copper metal and anode slag10.1016/j.jeurceramsoc.2006.08.020 ↗
7. Penetration and corrosion of magnesia grain by silicate slags10.1179/096797800681036 ↗
8. Comparison of ferrous calcium silicate slag and calcium ferrite slag interactions with magnesia-chrome refractories10.1007/s11663-011-9499-0 ↗
9. Phase formation processes and structural changes in chromite-periclase refractories used during nickel production10.1007/s11148-012-9433-2 ↗
10. General aspects of periclase-chromite refractory wear during nickel production10.1007/s11148-011-9398-6 ↗
11. Corrosive interaction between slags high in copper and nickel oxides and periclase: periclase-chromite, and chromite refractories10.1007/s11148-006-0003-3 ↗
12. Analysis and interpretation of refractory micro structures in studies of corrosion mechanisms by liquid oxides10.1016/j.jeurceramsoc.2007.10.012 ↗
13. Reactions of dense MgO with calcium ferrite-based slags at 1573K10.1007/s11663-005-0055-7 ↗
14. Reactions of dense MgO with calcium ferrite-based slags at 1573K10.1007/s11663-005-0055-7 ↗
15. Direct and indirect slag corrosion of oxide and oxide-C refractories
16. In situ observation of the direct and indirect dissolution of MgO particles in CaO-Al2O3-SiO2-based slags10.1016/j.jeurceramsoc.2006.05.107 ↗
17. Degradation of MgO refractory in CaO-SiO2-MgO-FeOx and CaO-SiO2-Al2O3-MgO-FeOx slags under forced convection10.1007/s11663-005-0036-x ↗
18. Experimental study of phase equilibria in the PbO-ZnO-"Fe2O3"-CaO-SiO2 system in air for high lead smelting slags (CaO/SiO2=0.35 and PbO/(CaO+SiO2)=5.0 by weight)10.1007/s11663-002-0065-7 ↗
19. he influence of slag compositional changes on the chemical degradation of magnesia-chromite refractories exposed to PbO-based non-ferrous slag saturated in spinel10.1016/j.jeurceramsoc.2014.08.017 ↗
20. Coupled experimental and thermodynamic modelling study of the system PbO-ZnO-FeO-Fe2O3-CaO-SiO2-Al2O3 for lead and zinc smelting
21. The effect of the CaO/SiO2 ratio on the phase equilibria in the ZnO-"Fe2O3"-(PbO+CaO+SiO2) system in air: CaO/SiO2=0.1, PbO/(CaO+SiO2)=6.2, and CaO/SiO2=0.6, PbO/(CaO+SiO2)=4.310.1007/s11663-003-0064-3 ↗
22. Experimental liquidus in the PbO-ZnO-Fe2 system in air, with CaO/SiO2 = 0.35 and PbO/(CaO + SiO2)=3.210.1007/s11663-002-0068-4 ↗
23. Thermodynamic optimization of the systems PbO-SiO2: PbO-ZnO, ZnO-SiO2 and PbO-ZnO-SiO210.1007/s11663-997-0055-x ↗
24. FactSage thermochemical software and databases10.1016/S0364-5916(02)00035-4 ↗
25. FactSage thermochemical software and databases – recent developments10.1016/j.calphad.2008.09.009 ↗
26. The effect of phase formation during use on the chemical corrosion of magnesia–chromite refractories in contact with a non-ferrous PbO–SiO2 based slag10.1016/j.jeurceramsoc.2013.12.026 ↗
27. The influence of ZnO in fayalite slag on the degradation of magnesia-chromite refractories during secondary Cu smelting10.1016/j.jeurceramsoc.2015.03.013 ↗
28. The effect of ZnO level in secondary copper smelting slags on slagmagnesia-chromite refractory interactions10.1016/j.jeurceramsoc.2016.02.004 ↗