High quality sapphire crystal by advanced chemical transport process
Source abstract
Abstract
Abstract Single crystal sapphire was synthesized by chemical transport of Al-O generated by the reaction of polycrystalline Al2O3 ceramic and carbon. Using C-axis oriented polycrystalline Al2O3 ceramics as a seed crystal in the deposition temperature range, a C-axis sapphire crystal (Φ5xL35 mm) was grown at a temperature range of 700–1000 °C, and the growth rate in the C-axis direction was about 3.5 mm/h. The transmittance in the visible to infrared region of the synthesized sapphire is a theoretical value (transmission loss is lower than 0.1 %/cm), and the absorption edge was less than 200 nm (the band gap is 6.2 eV), which is shorter than the absorption edge (240 nm) of the commercially available single crystal (band gap 5.2 eV) synthesized by the Czochralski method. The dislocation density in this material was extremely low, and it was confirmed by lattice image observation that it was a high-quality single crystal with very few defects.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Glass properties and applications · Solid State Laser Technologies · Photonic Crystals and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. US Patent. 1004505. Synthetic sapphire. 1911, September 26.
2. Nassau · 1980
3. Memoire sur la Reproduction du Rubis par Fusion
4. Simulated optical radiation in ruby10.1038/187493a0 ↗
5. Growth of sapphire disk from the melt by gradient furnace technique10.1111/j.1151-2916.1970.tb16009.x ↗
6. Large sapphire for optical application
7. Sapphire: properties, growth, and applications
8. Recent developments in growth of shaped sapphire crystals
9. Edge-defined, film-fed crystal growth10.1016/0022-0248(72)90067-X ↗
10. Growth behavior of high density Al2O3 layer prepared by using cyclic chemical vapor deposition technology10.1166/jnn.2015.10390 ↗
11. Wear and oxidation resistance of combustion CVD grown alumina films10.1016/j.surfcoat.2012.05.011 ↗
12. Low-temperature Al2O3 atomic layer deposition10.1021/cm0304546 ↗
13. Vapor-phase growth of alpha alumina single crystals10.1111/j.1151-2916.1965.tb14650.x ↗
14. Improvements to crystal quality of sapphire grown by kyropolos method
15. Epitaxial neodymium-doped sapphire films, a new active medium for waveguide lasers10.1364/OL.34.003358 ↗
16. Lasing of Nd3+ in Sapphire10.1002/lpor.201500319 ↗
17. Neodymium and ytterbium doped sapphire films grown by pulsed laser deposition