Cyclic contact fatigue behavior of baria-silicate glass-ceramics as a function of crystal aspect ratio
Source abstract
Abstract
Ceramic materials are potentially useful for dental applications because of their esthetic potential and biocompatibility. However, evidence of contact fatigue damage in ceramics raises considerable concern regarding its effect on the survival probability predicted for dental prostheses. To simulate intraoral conditions, Hertzian indentation loading with steel indenters was applied in this study to characterize the fatigue failure mechanisms of ceramic materials. Baria silicate glasses and glass-ceramics with different aspect ratios of crystals were selected because the glass and crystal phases have similar density, elastic modulus, and thermal expansion coefficients. Therefore, this system is a model ceramic for studying the effect of crystal geometry on contact cyclic fatigue failure. The subsequent flexural strength results show that the failure of materials with a low fracture toughness such as baria-silicate glass (0.7 MPa m1/2) and glass-ceramic with an aspect ratio of 3.6/1 (1.3 MPa m1/2) initiated from cone cracks developed during cyclic loading for 103 to 105 cycles. The mean strengths of baria-silicate glass and glass-ceramics with an aspect ratio of 3.6/1 decreased significantly as a result of the presence of a cone crack. Failures of baria-silicate glass-ceramics with an aspect ratio of 8.1/1 (Kc = 2.1 MPa m1/2) were initiated from surface flaws caused by either grinding or cyclic loading. The gradual decrease of fracture stress was observed in specimens with an aspect ratio of 8.1/1 after loading in air for 103 to 105 cycles. A reduction of approximately 50 % in fracture stress levels was found for specimens with an aspect ratio of 8.1/1 after loading for 105 cycles in deionized water. Thus, even though this glass-ceramic with an 8.1/1 crystal aspect ratio material is tougher than that with a 3.6/1 crystal aspect ratio, the fatigue damage induced by a large number of cycles is comparable. The mechanisms for cyclic fatigue crack propagation in baria-silicate glass-ceramics are similar to those observed under quasi-static loading conditions. An intergranular fracture path was observed in glass-ceramics with an aspect ratio of 3.6/1. For an aspect ratio of 8.1/1, a transgranular fracture mode was dominant.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Dental Research and COVID-19
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Glass–ceramics in dentistry: a review10.3390/ma13051049 ↗
2. A survey of crown and fixed partial denture failures: length of service and reasons for replacement10.1016/0022-3913(86)90379-3 ↗
3. Failed conventional bridge work from general dental practice: clinical aspects and treatment needs 142 cases10.1038/sj.bdj.4807133 ↗
4. Clinical evaluation of a castable ceramic material (abstract)
5. Role of microstructure on contact damage and strength degradation of micaceous glass-ceramics10.1016/S0109-5641(98)00013-X ↗
6. Mechanical characterization of dental ceramics by Hertzian contacts10.1177/00220345980770041201 ↗
7. Fatigue strength of several dental ceramics indicated for CAD-CAM monolithic restorations10.1590/1807-3107bor-2018.vol32.0053 ↗
8. Influence of cyclic loading on the fracture toughness and load bearing capacities of all-ceramic crowns
9. Mechanical fatigue of a feldspathic dental porcelain10.1016/0109-5641(93)90071-W ↗
10. Cyclic mechanical fatigue of a feldspathic dental porcelain
11. Relationship between static chemical and cyclic mechanical fatigue in a feldspathic porcelain10.1016/S0109-5641(97)80019-X ↗
12. Investigation of the dry and wet fatigue properties of three all-ceramic crown systems
13. Fatigue of dental ceramics in a simulated oral environment10.1177/00220345860650071901 ↗
14. Factors influencing the survival of implant-supported ceramic-Ceramic prostheses: a randomized, controlled clinical trial
15. The evolution of’ cone’ cracks under axi-symmetric loading conditions10.1007/BF00018436 ↗
16. Fracture mechanics analysis of crack shapes due to cyclic loading in baria-silicate glass10.1557/JMR.2007.0430 ↗
17. Deformation and fracture of mica-containing glass-ceramics in Hertzian contacts10.1557/JMR.1994.0762 ↗
18. Cyclic fatigue of a mica-containing glass-ceramics at Hertzian contacts10.1557/JMR.1994.2654 ↗
19. Use of contact testing in the characterization and design of all-ceramic crownlike layer structures: a review10.1067/mpr.2001.119581 ↗
20. Fracture surface analysis of dental ceramics: clinically failed restorations
21. Fracture surface characterization of clinically failed all-ceramic crowns10.1177/00220345940730120601 ↗
22. Nucleation and crystallization of barium silicate glasses
23. Mechanical properties of 3BaO-5SiO2 glass10.1111/j.1151-2916.1974.tb11352.x ↗
24. Electron microscopic technique for determining the percent crystallinity of glass-ceramic materials10.1111/j.1151-2916.1964.tb13831.x ↗
25. Crack-extension force for a part-through crack in a plate10.1115/1.3640649 ↗
26. Effect of grinding on flaw geometry and fracture of glass10.1111/j.1151-2916.1977.tb15484.x ↗
27. Fractal analysis of toughening behavior in 3BaO•5SiO2 glass ceramics10.1111/j.1151-2916.2000.tb01232.x ↗
28. Strength degradation of brittle surfaces: blunt indenters10.1111/j.1151-2916.1975.tb19015.x ↗
29. Strength degradation by projectile impacts10.1111/j.1151-2916.1973.tb12710.x ↗
30. Damage processes in Si3N4 bearing material under contact loading10.1016/0043-1648(96)06970-0 ↗
31. Lifetime-limiting strength degradation from contact fatigue in dental ceramics10.1177/00220345000790020501 ↗
32. Anusavice · 1996
33. Indentation of ceramics with spheres: a century after Hertz10.1111/j.1151-2916.1998.tb02580.x ↗
34. Failure of all-ceramic fixed partial dentures in vitro and in vivo: analysis and modeling10.1177/00220345950740060301 ↗
35. Clinically relevant approach to failure testing of all-ceramic restorations10.1016/S0022-3913(99)70103-4 ↗
36. Holand · 2002
37. Multiple range and multiple F tests10.2307/3001478 ↗
38. Critical values for Duncan’s multiple range test10.2307/2527770 ↗
39. Effect of flaw shape on strength of ceramics10.1111/j.1151-2916.1976.tb09406.x ↗
40. Mecholsky · 1983
41. Irwin · 1971
42. Fracture surface analysis of ceramics10.1007/BF00545152 ↗