journal article·2002-07

Internal protection of C/C composites by boron-based compounds

S Labruquère, R Pailler, A Guette, R Naslain

Publisher page

Abstract

Abstract Boron-based protections were used on carbon fibre preforms in order to protect interfacial zones in C/C composites from oxidation. Wet treatments (H 3 BO 3 in aqueous solution) and B–P CVD-coatings are not stable under low pressures at 1000 °C (the matrix deposition conditions in conventional CVI). Hence, they could not be used as C/C composite internal protections. Boron-ion implantation in carbon fibres improves their tensile strength by healing superficial carbon fibre defects but is not efficient as an internal protection in C/C composites, the boron-ions being implanted too far from the carbon fibre surface. B–C CVD-deposits are also not very efficient as internal protections. They oxidize faster than the carbon and lead to an important volume decrease. Holes are then formed at the interfacial zones at the beginning of the oxidation of the C/B–C/C composite passing from the surface to the core of the material.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Metal and Thin Film Mechanics · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (8)

Show source-provided references
1. Influence of boron on carbon fiber microstructure, physical properties and oxidation behavior10.1016/0008-6223(91)90076-U ↗
2. Jacques, S., Elaboration et Caractérisation des Matériaux C(B). Applications en tant qu'Interphases dans les Composites SiC–SiC. PhD thesis, No. 1398, University of Bordeaux, December, 1995.
3. Effect of boron implantation on the oxidation behavior of three-dimensional carbon–carbon composites10.1016/0008-6223(93)90040-H ↗
4. Labruquère, S., Bourrat, X., Pailler, R. and Naslain, R., Structure and oxidation of C/C composites: role of the interface. Carbon, in press.10.1016/S0008-6223(00)00142-1 ↗
5. Enhancement of the oxidation resistance of interfacial area in C/C composites10.1016/S0955-2219(01)00410-1 ↗
6. Carbon–carbon materials and composites using CVD and CVI processing (an overview)
7. Shear moduli of carbon, Si–C–O, Si–C–TiO and alumina single ceramic fibers as assessed by tension pendalum tests10.1016/0266-3538(93)90059-P ↗
8. McKee · Carbon · 1986 · 24 · 733