Thermal diffusivity measurement of SiC fibre reinforced BMAS glass ceramic composites exposed mechanical damage
Source abstract
Abstract
Abstract Gas turbine blades in aerospace engines are one of the possible application areas for glass ceramic composites which may be subjected to various mechanical loads and can be damaged during operation. Therefore, various types of ceramic matrix composite are being evaluated for high temperature applications. Barium osumilite is a glass ceramic matrix formulation and believed to be suitable using for those applications. In this study, SiC fibre reinforced barium magnesium aluminium silicate (BMAS) glass ceramic matrix composites exposed to mechanical damage by the tensile fatigue test at the temperature of 700, 900, 1000 °C and then the effect of mechanical damage on the thermal diffusivity of the composites were investigated. The thermal diffusivity measurements were performed from 100 to 1000 °C. The obtained results indicated that the thermal diffusivity values of the composites that exposed to mechanical damage by thermal fatigue at various temperatures resulted in 32% lowering in the thermal diffusivity values of the composites fatigued at 700 °C compared with the values of as received.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Thermal properties of materials · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. High temperature materials—a general review10.1007/BF00576759 ↗
2. Recent developments in fiber reinforced high temperature ceramic composites
3. Fiber reinforced glasses and glass ceramics for high performance applications
4. Silicon carbide fibre reinforced glass ceramic matrix composites exhibiting high strength and toughness10.1007/BF00543747 ↗
5. Brennan, J. J., Chyung, K. and Taylor, M. P., High strength thermally stable magnesium aluminosilicate glass ceramic matrix SiC fibre composite, USA patent No.: 4589900, 1986.
6. Microstructure property relationships of the fibre reinforced magnesium alumina silicates. I. Mechanical properties and failure characteristic10.1016/1359-6454(95)00387-8 ↗
7. Effect of preparation parameters on the properties of unidirectional SiC fibre reinforced MAS and BMAS glass-ceramics10.1016/S0266-3538(96)00176-5 ↗
8. Influence of the laminate lay-up on the fatigue behaviour of SiC-fibre/BMAS-matrix composites10.1016/S1359-835X(98)00177-8 ↗
9. The mechanical behaviour of glass and glass-ceramic matrix composites10.1016/S0921-5093(99)00572-9 ↗
10. In situ speckle observation of Tyrano/BMAS composites in shear strength measurements10.1016/S1359-8368(02)00132-4 ↗
11. Effect of heat treatment in air on the structure and properties of barium osumilite reinforced with Nicalon fibres10.1007/BF02403903 ↗
12. Environmental ageing effect in a silicon carbide reinforced glass ceramic matrix composite10.1111/j.1365-2818.1995.tb03556.x ↗
13. Effect of silicon fibre or whisker reinforcement on the thermal diffusivity, conductivity of an osumilite glass ceramics10.1111/j.1151-2916.1987.tb05671.x ↗
14. Thermal expansion behaviour of unidirectionally SiC fibre reinforced MAS and BMAS glass ceramics
15. Yılmaz, R. and Taylor, R., Effect of heat treatment in air on the thermal properties of SiC fibre reinforced composite, part 1 a barium osumilite (BMAS) matrix glass ceramic composite, J. Mater. Sci., 2006, in press.10.1007/s10853-006-1443-3 ↗
16. Fatigue behaviour of borosilicate glass-ceramic matrix, Nicalon (silicon carbide) fibre composites10.1007/BF00367834 ↗
17. Minford · 1986
18. Damage development and moduli reductions in Nicalon-calcium aluminosilicate composites under static fatigue and cyclic fatigue10.1111/j.1151-2916.1993.tb06640.x ↗
19. The effects of thermal fatigue on a SiC fibre/aluminosilicate glass composite10.1007/BF00588299 ↗
20. Thermal diffusivity of composites
21. Construction of apparatus for the heat pulse thermal diffusivity measurements from 300 to 3000 K10.1088/0022-3735/13/11/014 ↗
22. Structure and chemistry of fibre matrix interfaces in silicon carbide fibre reinforced glass ceramic composites: an electron microscopy study10.1007/BF01161176 ↗
23. Effect of micro-cracking on thermal conductivity: analysis and experiment
24. Role of thermal barrier in effective thermal diffusivity/conductivity of SiC fibre reinforced reaction bonded silicon nitride10.1111/j.1151-2916.1990.tb06511.x ↗
25. Role of interfacial debonding and matrix cracking in the effective thermal diffusivity of SiC fibre reinforced chemical vapour deposited SiC matrix composites10.1007/BF00721838 ↗
26. Role of interfacial debonding and matrix cracking in the effective thermal diffusivity of SiC fibre reinforced chemical vapour infiltrated silicon carbide matrix composites10.1111/j.1151-2916.1991.tb07150.x ↗