Role of zirconia phase transformation, interface processes, and Ta2O5 doping on the blistering phenomenon of molten glass in contact with zirconia-based refractories

J. Hell, P. Vespa, I. Cabodi, O. Citti, F. Fournet-Fayard, J. Fouletier, M.C. Steil

Abstract

Abstract Bubble formation and removal within the molten glass is an important issue in glass industry. Various sources of bubbles have been identified in glass manufacturing: decomposition of the glass components, air trapping, oxidation/reduction reactions, precipitation resulting from insufficient refining, etc. It has been demonstrated in a previous paper that the blistering phenomenon at the interface between a molten glass and a zirconia-based refractory can be ascribed to the oxygen semipermeability through the zirconia phase. The objective of this study is to clarify the role of temperature on the blistering process, and especially, below and above the phase transition temperature of zirconia (monoclinic/tetragonal transformation) and to evaluate the role of zirconia doping on the blistering level. The influence of the kinetics of the surface processes at the glass/refractory interface is emphasized. Quantitative measurement of the slight blistering ascribed to the so-called “redox shock” is also given.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Glass properties and applications · Nuclear materials and radiation effects · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (65)

Show source-provided references
1. Refractories for the glass industry10.1016/0022-3093(86)90382-0 ↗
2. Mesoscopic Monte Carlo simulations of microstructure and conductivity of ZrO2–glass composites10.1016/j.actamat.2013.04.044 ↗
3. Finite element simulations of the deformation of fused-cast refractories based on X-ray computed tomography10.1016/j.commatsci.2006.01.033 ↗
4. Gas release phenomena in soda-lime-silica glass10.1016/j.jnoncrysol.2018.07.058 ↗
5. Interaction between solid, liquid and gas during glass batch melting10.1016/0022-3093(86)90799-4 ↗
6. Shelby · 2005
7. Bubble transport in three-dimensional laminar gravity-driven flow – mathematical formulation10.1016/j.jnoncrysol.2004.01.010 ↗
8. An Electrochemical Theory for Oxygen Reboil10.1111/j.1151-2916.1966.tb13162.x ↗
9. Effect of Sodium Sulfate and Temperature on the Fining of Float Glass10.1016/0022-3093(86)90456-4 ↗
10. Analysis of Gases Evolved by AZS Refractories and by Refractory Glass Melt Reactions – Techniques and Results – Contribution to the Bubble-Forming Mechanism of AZS Material
11. van Dijk · 1994
12. Electrochemical mechanism of the oxygen bubble formation at the interface between oxidic melts and zirconium silicate refractories
13. Bach · 2001
14. Comparative evaluation of the quality of fuse-cast refractories10.1007/BF00698216 ↗
15. Formation of Gaseous Inclusions on the Interface Between Refractory and Glass10.1007/BF00677404 ↗
16. Blistering phenomenon of molten glass in contact with zirconia-based refractories10.1016/j.jeurceramsoc.2021.03.063 ↗
17. The zirconia-hafnia system: DTA measurements and thermodynamic calculations10.1111/j.1551-2916.2006.01286.x ↗
18. Zirconia – an overview
19. Martensitic transformation in Zirconia10.1002/pssa.2210210102 ↗
20. Intrinsic Point Defect Equilibria in Tetragonal ZrO2 – Density Functional Theory Analysis with Finite Temperature Effects10.1103/PhysRevB.86.144109 ↗
21. Oxygen self-diffusion mechanisms in monoclinic ZrO2 revealed and quantified by density functional theory, random walk analysis, and kinetic Monte Carlo calculations
22. Defect Structure of ZrO2 and HfO210.1149/1.2425707 ↗
23. Electrical properties and defect structure of zirconia: I, monoclinic phase10.1111/j.1151-2916.1964.tb13124.x ↗
24. Electrical properties and defect structure of zirconia: II, Tetragonal Phase and Inversion10.1111/j.1151-2916.1965.tb14802.x ↗
25. On the Defect Structure of ZrO2 and HfO210.1149/1.2425644 ↗
26. Effect of Impurities on the Defects in Oxides and Their Relationship to Oxidation of Metal10.5006/0010-9312-24.11.379 ↗
27. Effect of oxide defect structure on the electrical properties of ZrO210.1111/j.1151-2916.1972.tb11336.x ↗
28. Martensitic transformation in zirconia: Part I. Nanometer scale prediction and measurement of transformation induced relief
29. Investigation of the electrical conductivity of sintered monoclinic zirconia (ZrO2)10.1016/j.ceramint.2017.03.152 ↗
30. Ionic and Electronic Conductivity in Y2O3-Doped Monoclinic ZrO210.1149/1.2401793 ↗
31. Interpretation of the Electrical Conductivity of ZrO2 and HfO2 at High Temperature (1300°C-1600°C) (in Fr.)10.1016/0022-4596(75)90275-3 ↗
32. Determination of thermodynamics and transport properties of non-stoichiometric oxides
33. Mixed conduction in Zr0.85Ca0.15O1.85 and Th0.85Y0.15Ol.925 solid electrolytes10.1149/1.2426723 ↗
34. Conduction Domains for Solid Electrolytes10.1149/1.2408241 ↗
35. Point Defects in Oxides: Tailoring Materials Through Defect Engineering10.1146/annurev-matsci-062910-100442 ↗
36. Oxidation of Oxygen-Deficient Zirconia and its Relationship to the Oxidation of Zirconium10.1149/1.2424088 ↗
37. Oxygen diffusion in monoclinic zirconia10.1016/0025-5408(68)90008-1 ↗
38. Diffusionless Phase Transformations in Zirconia and Hafnia10.1111/j.1151-2916.1963.tb11768.x ↗
39. Impedance spectroscopy of Mg-partially stabilized zirconia and cubic phase decomposition10.1016/0955-2219(95)00125-5 ↗
40. Structure and ionic mobility of Zirconia at High-Temperature10.1111/j.1151-2916.1985.tb15247.x ↗
41. Characterization of the electronic charge carriers in TZP10.1016/0167-2738(92)90265-Q ↗
42. Electrical conductivity of tetragonal zirconia below the transformation temperature10.1149/1.2127536 ↗
43. The Tetragonal-Monoclinic Transformation in Zirconia: Lessons Learned and Future Trends10.1111/j.1551-2916.2009.03278.x ↗
44. Oxygen self-diffusion mechanisms in monoclinic ZrO2 revealed and quantified by density functional theory, random walk analysis, and kinetic Monte Carlo calculations
45. Electrochemical semipermeability and the electrode microsystem in solid oxide electrolyte cells10.1149/1.2132787 ↗
46. Oxygen surface exchange in mixed ionic electronic conductor membranes10.1016/S0167-2738(98)00389-0 ↗
47. Influence of Oxygen Surface Exchanges on Oxygen Semi-Permeation through La(1-x)SrxFe(1-y)GayO(3-δ) Dense Membrane10.1149/1.3597086 ↗
48. Surface exchange polarization vs. gas concentration polarization in permeation through mixed ionic-electronic membrane10.1016/j.memsci.2017.07.028 ↗
49. Sarrazin · 2008
50. Oxygen permeation through dense Bi2V0.9Cu0.1O5.35 ceramic membranes10.1149/1.1516227 ↗
51. Densification of yttria-stabilized zirconia - Impedance spectroscopy analysis10.1149/1.1837416 ↗
52. Microstructure blocking effects versus effective medium theories in YSZ10.1016/S0955-2219(97)89966-9 ↗
53. On the role of the pore morphology on the electrical conductivity of porous yttria-stabilized zirconia10.1016/j.jeurceramsoc.2019.02.027 ↗
54. Foams in Glass Manufacturing
55. Solubility of gases in glass melts10.1002/bbpc.19961000932 ↗
56. Semiconduction and mixed ionic-electronic conduction in nonstoichiometric oxides: impact and control10.1016/S0167-2738(96)00585-1 ↗
57. Electrochemistry of Mixed Oxygen Ion and Electron Conducting Electrodes in Solid Electrolyte Cells10.1146/annurev-chembioeng-073009-101000 ↗
58. Mixed Ionic-Electronic Conducting Membranes (MIEC) for Their Application in Membrane Reactors: A Review10.3390/pr7030128 ↗
59. Electrocatalytic Properties and Nonstoichiometry of the High Temperature Air Electrode La1-xSrxMnO310.1149/1.2085761 ↗
60. Conventional oxygen electrode reaction: facts and models
61. Optimized SOFC electrode microstructure10.1016/S0167-2738(96)00464-X ↗
62. Mixed Ionic – Electronic Conducting (MIEC) ceramic-based membranes for oxygen separation10.1016/j.memsci.2008.03.074 ↗
63. Development of lanthanum strontium cobalt ferrite perovskite electrodes of solid oxide fuel cells – A review10.1016/j.ijhydene.2019.01.212 ↗
64. Reaction-Zone Expansions and Mechanism of the O2/Ag/Yttria-Stabilized Zirconia Electrode Reaction10.1149/1.1837451 ↗
65. I. Cabodi, M. Gaubil, Doped refractory with a high zirconia content, US Patent, US8273673B2, 25 Sept. 2012.