Abstract

This work investigates the scale effect observed on slow crack growth parameters for SiC-based fibers (Nicalon® and Tyranno® ZMI) and how it can be affected by the variability from a batch of tow to another one. A 10% difference on the stress exponents (nt) was numerically estimated using a dedicated Monte Carlo simulation. This effect is however marginal when compared to the lifetime scatter itself. This partly originates from the fiber slack in used tow specimen, assessed by tensile test completing the experimental work. The number of tensile tests to be performed is discussed. Specimen gauge length is an additional and significant source of discrepancies affecting the fiber alignment and subsequently the tow stress exponent.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Silicon Carbide Semiconductor Technologies · Mechanical Behavior of Composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
2. Silicon carbide and its composites for nuclear applications – historical overview10.1016/j.jnucmat.2019.151849 ↗
3. Ceramic-Matrix Composites enable revolutionary gains in turbine engine efficiency
4. G. Gardiner, Aeroengine composites, Part 1: The CMC invasion, Composites World (2015).
5. Ceramic matrix composites: nuclear applications
6. Strength–Probability–Time (SPT) relationships in ceramics10.1007/BF02403519 ↗
7. Stress-Rupture of Nicalon/SiC continuous fiber ceramic composites in air at 950°C10.1111/j.1151-2916.1997.tb03266.x ↗
8. Delayed failure at intermediate temperature (600 °-700 °C) in air in silicon carbide multifilament tows10.1111/j.1551-2916.2004.00888.x ↗
9. New insight into subcritical rupture of SiC-based filaments at intermediate temperatures (400–900 °C) under air10.1016/j.jeurceramsoc.2021.08.034 ↗
10. Delayed Failure of Hi-Nicalon and Hi-Nicalon S multifilament tows and single filaments at intermediate temperatures (500°-800°C)10.1111/j.1551-2916.2009.02924.x ↗
11. Reinforcement of ceramic matrix composites: properties of SiC-based filaments and tows
12. Subcritical crack growth models for static fatigue of Hi‐NicalonTM‐S SiC fiber in air and steam10.1111/jace.17728 ↗
13. Statistical data for the tensile properties and static fatigue of SiC-based bundles10.1016/j.dib.2020.106166 ↗
14. Static fatigue of SiC-based multifilament tows at intermediate temperature: the time to failure variability10.1016/j.ijfatigue.2020.106072 ↗
15. Delayed failure under static fatigue of Hi-Nicalon bundles: the role of stress dispersion on scale effect10.1016/j.matlet.2021.129806 ↗
16. Resistance to fatigue at intermediate temperature in air for SiC Hi-Nicalon Fibers: statistical distributions of lifetimes and strength degradation10.1111/j.1551-2916.2012.05414.x ↗
17. Static fatigue of Hi-NicalonTM-S fiber at elevated temperature in air, steam, and sillicic acid-saturated steam10.1111/jace.16799 ↗
18. Delayed failure prediction of SiC-based bundles: the impact of sampling size10.1016/j.ijfatigue.2020.105694 ↗
19. Simulating the variability and scale effect for slow crack growth in Hi-Nicalon SiC-based tows: a parametric study10.1016/j.jeurceramsoc.2021.07.032 ↗
20. Study of Nicalon-based ceramic fibres and powders by EXAFS spectrometry, X-ray diffractometry and some additional methods10.1007/BF02397093 ↗
21. Contribution to the understanding of the microstructure of first generation Si-C-O fibers
22. Composition and reactivity of various silicon carbide fibers, HTCMC810.1002/9781118932995.ch13 ↗
23. Dataset on fractographic analysis of various SiC-based fibers
24. Improvement of silicon carbide fibers mechanical properties by Cl2 etching10.1016/j.jeurceramsoc.2018.06.026 ↗
25. Carbide derived carbon (CDC) coatings for Tyranno ZMI SiC fibers10.1002/9780470294802.ch8 ↗
26. In-situ processing of carbon coating on the surface of SiC-based fibers10.1016/j.surfcoat.2010.07.060 ↗
27. Carbon derived from silicon carbide fibers, a comparative study10.1016/j.mtcomm.2019.01.013 ↗
28. Statistical analysis of failure of SiC fibres in the presence of bimodal flaw populations10.1023/A:1018600119250 ↗
29. ISO ISO 19630, Fine ceramics (advanced ceramics, advanced technical ceramics) --Methods of test for reinforcements -- Determination of tensile properties of filaments at ambient temperature.
30. European Standard, determination of distribution of tensile strength and of tensile strain to failure of filaments within a multifilament tow at ambient temperature, CEN TC 184, ENV 1007–5 (1998).
31. The statistical theory of the strength of bundles of threads. I
32. On the strength of classical fibers bundle10.1016/0022-5096(58)90039-5 ↗
33. Experimental probability estimators for Weibull plots10.1007/BF01729379 ↗
34. On the estimation of the Weibull modulus10.1007/BF00719924 ↗
35. Stochastic modeling of multi-filament yarns. I. Random properties within the cross-section and size effect10.1016/j.ijsolstr.2005.06.063 ↗
36. Probabilistic strength analysis of fibre bundle structures10.1016/0015-0568(74)90003-7 ↗
37. Failure of fiber bundles10.1016/j.compscitech.2003.07.003 ↗
38. Dependency of fatigue predictions on the form of the crack velocity Eq10.1111/j.1151-2916.1981.tb10305.x ↗
39. Munz · 2001
40. Dependency of fatigue predictions on the form of the crack velocity equation10.1111/j.1151-2916.1981.tb10305.x ↗
41. R.J. Surfaces, strain-dependent reactions and strength
42. Stress corrosion and static fatigue of glass10.1111/j.1151-2916.1970.tb15962.x ↗
43. Environmentally enhanced fracture of glass: a Historical perspective10.1111/j.1551-2916.2009.03097.x ↗
44. An atomistic model of kinetic crack growth in brittle solids10.1007/BF00543692 ↗
45. Part-circular surface cracks in round bars under tension, bending and twisting10.1007/BF00032340 ↗
46. Subcritical crack growth in silica optical fibers in a wide range of crack velocities10.1111/j.1151-2916.1996.tb07879.x ↗
47. An incompatible singular elastic element for two-and three-dimensional crack problems10.1007/BF00018917 ↗
48. Zero stress aging in notched multi-component glass fibers10.1111/jace.16507 ↗
49. Damage and failure of SiC fiber tows during environment activated slow crack growth: residual behavior and strength-probability-time diagrams10.1016/j.actamat.2017.03.073 ↗
50. Static fatigue of SiC multifilament tows at temperatures up to 1200 °C in air10.3390/ceramics2030033 ↗
51. A. Laforet, Rupture différée en fatigue statique aux très hautes températures (800°C-1300°C) des fils Hi-Nicalon, des composites Hi-Nicalon/type PyC/SiC et des composites Hi-Nicalon/type PyC/B4C, PhD Thesis, University of Bordeaux, France (2009).
52. Fine diameter ceramic Fbres10.1016/S0955-2219(00)00090-X ↗