journal article·2022-02

Pulsed current-driven wetting of 3YSZ by liquid Cu and its mechanisms

Yuan-Zhe Liang, Lin Li, Ping Shen

Publisher page

Abstract

Abstract The wettability of 3 mol% Y2O3-stabilized ZrO2 (3YSZ) by molten Cu can be greatly improved by applying pulsed currents at 1373 K. The improvement was closely related to current polarity and influenced by duty cycle and frequency. When the Cu/3YSZ interface was under cathodic condition, the wettability was mainly improved by the formation of substoichiometric ZrO2-δ and metallic Zr at the interface. Increasing duty cycle caused the interface to change from forming protrusions to creating depression. Decreasing frequency further deepened the depression. In the opposite polarity, the adsorption and enrichment of oxygen reduced the solid-liquid and liquid-vacuum interfacial energies, thus improving the wettability. Only bubbles formed at the interface. The larger the duty cycle, the more rapidly bubbles formed and escaped. The effect of frequency at this polarity was weak. Overall, this work provides a novel and effective strategy for tailoring the wettability and interfacial chemistry between zirconia and metals.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic and Structural Properties of Oxides · Semiconductor materials and devices · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Active metal brazing of zirconia10.1016/S1359-6454(00)00256-1 ↗
2. Tetragonal to monoclinic transformation in Y-TZP joined with metallic materials10.1023/A:1004787024464 ↗
3. Joining of zirconia ceramic to stainless steel and to itself using Ag57Cu38Ti5 filler metal10.1111/j.1151-2916.1995.tb08629.x ↗
4. Kinetic and microstructural aspects of the reaction layer at ceramic/metal braze joints10.1007/BF01139163 ↗
5. A braze system for sealing metal-supported solid oxide fuel cells10.1016/j.jpowsour.2006.02.067 ↗
6. Investigation of interaction of metal melts and zirconia10.1007/s10853-005-1928-5 ↗
7. Wettability of some metals against zirconia ceramics10.1007/BF01729384 ↗
8. The nonwettability behaviour of solid substrates in contact with chemical active reach Ti-, Zr- and Hf-liquid alloys10.1023/A:1006688713685 ↗
9. Brazing of zirconia with AgCuTi and SnAgTi active filler metals10.1007/s11661-000-0169-0 ↗
10. Wettability of zirconium diboride ceramics by Ag, Cu and their alloys with Zr10.1016/S1359-6462(02)00361-5 ↗
11. Significant improvement in the wettability of ZrO2 by molten Al under the application of a direct current10.1016/j.matdes.2016.08.081 ↗
12. Polarity effects on the wettability and interfacial chemistry at Cu-YSZ interface by applying a direct current10.1016/j.jeurceramsoc.2017.10.049 ↗
13. DC-assisted rapid wetting of 3Y-PSZ by molten 72Ag-28Cu and its application in joining10.1016/j.jeurceramsoc.2019.01.046 ↗
14. Flash-induced spreading of metals on zirconia10.1016/j.scriptamat.2019.09.013 ↗
15. Comparison of Cr(VI) removal by direct and pulse current electrocoagulation: implications for energy consumption optimization, sludge reduction and floc magnetism10.1016/j.jwpe.2020.101387 ↗
16. Cd removal by direct and positive single pulse current electrocoagulation: operating conditions and energy consumption
17. Pulse current electrodeposition and corrosion properties of Ni-W alloy coatings10.1007/s10800-011-0331-y ↗
18. Ni-Co alloys plated by pulse currents10.1016/j.surfcoat.2005.10.008 ↗
19. Effect of pulse current density on microstructure and wear property of Ni-TiN nanocoatings deposited via pulse electrodeposition10.1016/j.apsusc.2020.148139 ↗
20. Electric current activation of sintering: a review of the pulsed electric current sintering process10.1111/j.1551-2916.2010.04210.x ↗
21. Electrochemical blackening of yttria-stabilized zirconia-morphological instability of the moving reaction front10.1016/S0167-2738(98)00415-9 ↗
22. Electrical and hydrogen reduction enhances kinetics in doped zirconia and ceria: I. Grain growth study10.1111/jace.14615 ↗
23. Electrical and hydrogen reduction enhances kinetics in doped zirconia and ceria: II. Mapping electrode polarization and vacancy condensation in YSZ10.1111/jace.15274 ↗
24. Potential jumps at transport bottlenecks cause instability of nominally ionic solid electrolytes in electrochemical cells10.1016/j.actamat.2020.08.017 ↗
25. Griffiths · 1999
26. Reactive spreading: adsorption, ridging and compound formation10.1016/S1359-6454(00)00231-7 ↗
27. The wettability of solids by liquid metals10.1016/B978-0-12-571814-1.50011-7 ↗
28. Pauling · 1960