Wetting and interfacial reactions in liquid Au-Ti alloys / ZrO2 system
Source abstract
Abstract
This study investigates wetting of zirconia by Au-Ti alloys containing 0.6–4 wt% Ti in view of brazing zirconia to titanium with pure gold for biomedical applications. Experiments were carried out using sessile and dispensed drop methods under high vacuum at 1040–1250 ◦C. Bulk drops and Au-Ti / ZrO2 interfaces were characterized by SEM and FEG-SEM with EDXS analysis. While Au does not wet zirconia, the contact angle θ being ~ 120◦, the addition of Ti in Au leads to a significant improvement of wetting due to the formation of a wettable oxide layer at Au-Ti / ZrO2 interface. The nature of this oxide was determined by X-ray diffraction of the reaction layer after the detachment of the droplet from the substrate or after the dissolution of the droplet. The mechanism offormation and growth of the oxide layer and its growth kinetics were determined based on fine analysis of theAu-Ti / oxide layer / ZrO2 interfacial system.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Catalytic Processes in Materials Science · ZnO doping and properties · Catalysis and Hydrodesulfurization Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Interactions, joining and microstructure of Sn-Ti/ZrO210.1016/j.jeurceramsoc.2018.12.010 ↗
2. Brazing of zirconia with AgCuTi and SnAgTi active filler metals10.1007/s11661-000-0169-0 ↗
3. Joining of zirconia to zirconia using Ag-Cu-Ti filler metal10.1016/0924-0136(94)01611-4 ↗
4. Zirconia-titanium joint interfaces10.4028/www.scientific.net/MSF.207-209.145 ↗
5. Active metal brazing of zirconia10.1016/S1359-6454(00)00256-1 ↗
6. Joining of zirconia to metals using Zr-Cu alloy10.1016/0013-7944(91)90254-X ↗
7. Microstructure evolution and mechanical properties of ZrO2/ZrO2 joints brazed with Ni-Ti filler metal10.1088/2053-1591/ab574b ↗
8. Brazing YSZ ceramics by a novel SiO2 nanoparticles modified Ag filler10.1016/j.ceramint.2020.03.214 ↗
9. Effect of filler metal composition on the strength of Yttria stabilized zirconia joints brazed with Pd-Ag-CuOx10.1007/s11661-008-9565-7 ↗
10. S. Agathopoulos, R.N. Correia, E. Joanni, J.R.A. Fernandes, Interactions at zirconia-Au-Ti interfaces at high temperatures, Key Engineering Materials. 206–213 (2002) 487–490, Trans Tech Publications Ltd, doi:10.4028/www.scientific.net/kem.206–213.487.10.4028/www.scientific.net/KEM.206-213.487 ↗
11. Brazeability, microstructure, and joint characteristics of ZrO2/Ti-6Al-4V brazed by Ag-Cu-Ti filler reinforced with cerium oxide nanoparticles
12. S.H. Wei, C.C. Lin, Microstructural evolution and bonding mechanisms of the brazed Ti/ZrO2 joint using an Ag68.8Cu26.7Ti4.5 interlayer at 900 °C, J Mater Res. 72 (2014) 684–694, doi:10.1557/jmr.2014.30.10.1557/jmr.2014.30 ↗
13. Evolution of the interlayer microstructure and the fracture modes of the zirconia/Cu-Ag-Ti filler/Ti active brazing joints10.1016/j.matlet.2006.05.024 ↗
14. Interface microstructure and mechanical behaviour of brazed TA6V/zirconia joints10.1007/BF00721864 ↗
15. Effect of interface microstructure on joint strength of zirconia/titanium alloy brazed with amorphous Zr-Ti-Ni-Cu active filler metal10.3390/met10060718 ↗
16. Effects of fabrication parameters on interface of zirconia and Ti-6Al-4V joints using Zr55Cu30Al10Ni5 amorphous filler10.1007/s11665-013-0534-y ↗
17. Evaluation of biomedical Ti / ZrO2 joint brazed with pure Au filler: microstructure and mechanical properties
18. M. Fischer, V. Chaumat, G. Tourrel, F. Hodaj, Wetting and reactivity of zirconia by Au-Ti active alloys in view of zirconia / titanium brazing with pure gold. Proceedings of the 8th International Brazing and Soldering Conference, October 3–6, 2021.
19. A review of recent investigations on zirconia joining for biomedical applications
20. Brazing of zirconia to titanium using Ag-Cu and Au-Ni filler alloys10.1590/S0104-92242013000400007 ↗
21. Brazing ZrO2 ceramic to Ti-6Al-4V alloy using NiCrSiB amorphous filler foil: Interfacial microstructure and joint properties10.1016/j.matchar.2013.04.009 ↗
22. Zirconia-high entropy alloys joints for biomedical applications: The role of Ag-based fillers on interfacial reactivity10.1016/j.jallcom.2022.164764 ↗
23. Effect of zirconium on wettability of alumina and zirconia by silver-indium base alloy10.1007/BF00729276 ↗
24. Investigation of interaction of metal melts and zirconia10.1007/s10853-005-1928-5 ↗
25. Wetting and interfacial behavior of Sn–Ti alloys on zirconia10.1007/s10853-018-2829-8 ↗
26. H. Bian, W. Fu, Y.Z. Lei, X.G. Song, D. Liu, J. Cao, J.C. Feng, Wetting and low temperature bonding of zirconia metallized with Sn0.3Ag0.7Cu-Ti alloys. Ceram Int. 44 (2018) 11456–11465, https://doi.org/10.1016/j.ceramint.2018.03.207.10.1016/j.ceramint.2018.03.207 ↗
27. Reactive wetting and interfacial characterization of ZrO2 by SnAgCu-Ti alloy10.1016/j.ceramint.2018.12.163 ↗
28. Wetting, spreading and joining in the alumina-zirconia-Inconel 738 system10.1016/j.scriptamat.2003.10.015 ↗
29. Wettability and interfacial reaction of alumina and Zirconia By Reactive Silver-Indium Base alloy at mid-temperatures10.1007/BF01191971 ↗
30. N. Eustathopoulos, M.G. Nicholas, B. Drevet, Wettability at high temperatures. Pergamon Materials Series. Series Editor: R.W. Cahn. 1999.
31. New experimental setup for wettability characterization under monitored oxygen activity: I, role of oxidation state and defect concentration on oxide wettability by gold10.1111/j.1151-2916.1993.tb03941.x ↗
32. J.L. Murray, The Au-Ti (Gold-Titanium) system. Bull. Alloy Phase diagr. 4 (1983) 4:278–283.10.1007/BF02868667 ↗
33. Reaction diffusion in the Au-Ti system between 1110K and 1150K10.4028/www.scientific.net/DDF.194-199.1569 ↗
34. Contact angle hysteresis10.1016/j.cocis.2022.101574 ↗
35. The relation between wetting and interfacial chemistry in the CuAgTi/alumina system10.1016/j.actamat.2005.11.048 ↗
36. The effect of substrate surface roughness on the wettability of Sn-Bi solders
37. Wetting transitions in reactive metal/oxide systems10.1016/0956-716X(94)90326-3 ↗
38. B.F. Naylor, High-Temperature Heat Contents of TiO, Ti2O3, Ti3O5, and TiO2, J. Am. Chem. Soc. 68 (1946) 1077–1080, https://doi.org/10.1021/ja01210a047.10.1021/ja01210a047 ↗