journal article·2024-02Open access

Obtaining SiC Fibers–PyC interfacial properties through push-out FEM Models

Alvaro Martinez-Pechero, Yevhen Zayachuk, Anna Widdowson, David E.J. Armstrong, Edmund Tarleton

Abstract

Silicon carbide (SiC) has attractive properties for use in nuclear reactors. However, it is hampered by inherent brittleness that is overcome through a fiber-reinforced composite. A finite element model based on cohesive zone contact coupled to Coulomb friction is proposed to simulate the push-out response of isolated fibers in SiC/PyC fiber-reinforced composites. The model reproduces the measurements obtained during push-out experiments of isolated fibers in different configurations and predicts interfacial failure between the PyC interphase and fiber. The brittle properties predicted coincide with literature indicating that fiber-PyC interface could prevent the crack propagation through the fiber, fulfilling the function of the structure.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Current status and recent research achievements in SiC/SiC composites10.1016/j.jnucmat.2014.06.003 ↗
2. Current status and prospects of SiCf/SiC for fusion structural applications10.1016/j.jeurceramsoc.2013.02.013 ↗
3. DiCarlo · 2014
4. The high-temperature oxidation, reduction, and volatilization reactions of silicon and silicon carbide10.1007/BF00613092 ↗
5. Kinetics and mechanisms of high-temperature creep in silicon carbide: I, reaction-bonded10.1111/j.1151-2916.1984.tb19726.x ↗
6. Brittle dynamic fracture of crystalline cubic silicon carbide (3C-SiC) via molecular dynamics simulation10.1063/1.2135896 ↗
7. Chemical vapor deposition of silicon carbide and silicon nitride—Chemistry’s contribution to modern silicon ceramics10.1002/anie.197902951 ↗
8. 3.11 - Radiation effects in graphite
9. Ceramic composites: A review of toughening mechanisms and demonstration of micropillar compression for interface property extraction10.1557/jmr.2017.473 ↗
10. Linking microstructure and local mechanical properties in SiC-SiC fiber composite using micromechanical testing10.1016/j.actamat.2019.02.001 ↗
11. Statistically sound application of fiber push-out method for the study of locally non-uniform interfacial properties of SiC-SiC fiber composites10.1016/j.jeurceramsoc.2019.11.041 ↗
12. Simulation of fiber debonding with friction in a model composite push-out test10.1016/S0020-7683(01)00085-3 ↗
13. Some theoretical considerations of fibre pull-out from an elastic matrix
14. Interfacial bond strength in SiC/C/SiC composite materials, as studied by single-fiber push-out tests10.1111/j.1151-2916.1998.tb02434.x ↗
15. Influence of surface fibre properties and textural organization of a pyrocarbon interphase on the interfacial shear stress of SiC/SiC minicomposites reinforced with Hi-Nicalon S and Tyranno SA3 fibres10.1016/j.jeurceramsoc.2013.08.027 ↗
16. Influence of texture and thickness of pyrocarbon coatings as interphase on the mechanical behavior of specific 2.5 D SiC/SiC composites reinforced with hi-nicalon S fibers10.3390/coatings12050573 ↗
17. Fabrication of SiC–SiC composites for fuel cladding in advanced reactor designs10.1016/j.pnucene.2011.10.002 ↗
18. Evaluation of nanoindentation load-depth curve of MEMS bridge structures by calculating the critical elastic-plastic bending deflections10.1016/j.apsusc.2017.10.106 ↗
19. Melt infiltration approach to ceramic matrix composites10.1111/j.1151-2916.1988.tb05840.x ↗
20. Liquid silicon infiltration: description of infiltration dynamics and silicon carbide formation10.1016/S1359-835X(96)00135-2 ↗
21. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗
22. Damage production and accumulation in SiC structures in inertial and magnetic fusion systems10.1016/j.jnucmat.2010.12.077 ↗
23. Oxidation of silicon carbide fibers during static fatigue in air at intermediate temperatures10.1111/j.1551-2916.2009.03180.x ↗
24. Fracture toughness of a crystalline silicon carbide fiber (Tyranno-SA3)10.1111/j.1551-2916.2006.01116.x ↗
25. Optimizing the fiber push-out method to evaluate interfacial failure in SiC/BN/SiC ceramic matrix composites10.1111/jace.17673 ↗
26. A molecular dynamics based cohesive zone model for interface failure under monotonic tension of 3D four direction SiCf/SiC composites10.1016/j.compstruct.2021.114397 ↗
27. Mode II fracture toughness of a brittle adhesive layer10.1016/0020-7683(94)90168-6 ↗
28. Theoretical analysis of the fiber pullout and pushout tests10.1111/j.1151-2916.1991.tb07144.x ↗
29. Interfacial mechanics of push-out tests: theory and experiments10.1016/S1359-835X(00)00051-8 ↗
30. Smith · 2022
31. Impact-induced delamination of composites: a 2D simulation10.1016/S1359-8368(98)00013-4 ↗
32. A simplex method for function minimization10.1093/comjnl/7.4.308 ↗
33. Joglekar · 2016
34. Modified deformation behavior of self-ion irradiated tungsten: A combined nano-indentation, HR-EBSD and crystal plasticity study10.1016/j.ijplas.2020.102817 ↗
35. Micro-mechanical evaluation of SiC-SiC composite interphase properties and debond mechanisms10.1016/j.compositesb.2017.07.035 ↗
36. Crack deflection at an interface between dissimilar elastic materials10.1016/0020-7683(89)90021-8 ↗
37. The influence of the interphase and associated interfaces on the deflection of matrix cracks in ceramic matrix composites10.1016/S1359-835X(00)00095-6 ↗
38. Fracture toughness anisotropy of a pyrolytic carbon10.1007/BF01114701 ↗
39. The strength of adhesive joints using the theory of cracks10.1007/BF00186749 ↗
40. Begley · 2022
41. A novel trench fibre push-out method to evaluate interfacial failure in long fibre composites10.1557/s43578-021-00153-1 ↗
42. Effect of interfacial roughness parameters on the fiber pushout behavior of a model composite10.1111/j.1151-2916.1994.tb04575.x ↗
43. Combining interface damage and friction in a cohesive-zone model10.1002/nme.1728 ↗