Rigid-resilient transition in calcium borosilicate sealing glass–ceramics: Effect of preferred orientation
Source abstract
Abstract
Abstract At present, the insufficient thermo-mechanical stability of sealing glass presents a challenge for solid oxide fuel cells (SOFCs). In this work, we report for the first time that a rigid-resilient transition occurs in a calcium borosilicate sealing glass upon heating at 700 °C for different durations. The elastic modulus increases from 28.1–40.0 GPa for 24 h to 92.3–105.1 GPa for 100 h, while the corresponding hardness increases from 2.5–3.1 GPa to 8.1–9.2 GPa. In addition, a possible mechanism for the rigid-resilient transition has been proposed. The reported results provide a new approach to solve the sealing problem of SOFCs.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Progress in material selection for solid oxide fuel cell technology: a review10.1016/j.pmatsci.2015.01.001 ↗
2. Development of bilayer glass-ceramic SOFC sealants via optimizing the chemical composition of glasses - a review10.1007/s10008-015-2925-5 ↗
3. Aluminosilicate-based sealants for SOFCs and other electrochemical applications - a brief review10.1016/j.jpowsour.2013.05.099 ↗
4. Sealants for solid oxide fuel cells10.1016/j.jpowsour.2005.05.002 ↗
5. A review of sealing technologies applicable to solid oxide electrolysis cells10.1007/s10853-006-0409-9 ↗
6. Glass-based seals for solid oxide fuel and electrolyzer cells - a review10.1016/j.mser.2009.12.002 ↗
7. Thermal cycle stability of BaO-B2O3-SiO2 sealing glass10.1016/j.jpowsour.2009.06.018 ↗
8. Optimization of Al2O3-glass composite seals for planar intermediate-temperature solid oxide fuel cells10.1016/j.jpowsour.2012.10.084 ↗
9. Development of solid oxide fuel cell materials for intermediate-to-low temperature operation10.1016/j.ijhydene.2011.04.030 ↗
10. Stress and fracture behavior of monolithic fuel cell tapes10.1111/j.1151-2916.1986.tb04821.x ↗
11. A modeling study on the thermomechanical behavior of glass-ceramic and self-healing glass seals at elevated temperatures10.1016/j.jpowsour.2009.01.006 ↗
12. Self-healing performance of composite coatings prepared by phosphating and cerium nitrate post-sealing10.1007/s11595-015-1233-3 ↗
13. Study of geometric stability and structural integrity of self-healing glass seal system used in solid oxide fuel cells10.1016/j.jpowsour.2010.10.002 ↗
14. Can crystalline phases be self-healing sealants for solid oxide fuel cells?10.1016/j.jpowsour.2010.09.014 ↗
15. High temperature melt viscosity and fragile to strong transition in Zr–Cu–Ni–Al–Nb (Ti) and Cu47Ti34Zr11Ni8 bulk metallic glasses10.1016/j.actamat.2012.05.019 ↗
16. Thermodynamic determination of fragility in liquids and a fragile-to-strong liquid transition in water10.1038/19042 ↗
17. Fragile-to-strong transition in metallic glass-forming liquids
18. Quantitative analysis of ettringite in cement hydration products by "Value K" method of XRD
19. Effect of Fe2O3 concentration on the structure of the SiO2-Na2O-Al2O3-B2O3 glass system10.1016/j.saa.2011.05.074 ↗
20. Effect of HfO2 on the compatibility of borosilicate sealing glasses for solid oxide fuel cells application10.1039/C5RA10216B ↗
21. Quantitative measurement of Q3 species in silicate and borosilicate glasses using Raman spectroscopy10.1016/j.jnoncrysol.2007.06.105 ↗
22. Controlling the reaction between boron-containing sealing glass and a lanthanum-containing cathode by adding Nb2O510.1016/j.jpowsour.2016.06.075 ↗
23. Indentation size effect and shear transformation zone size in a bulk metallic glass in two different structural states10.1016/j.actamat.2012.08.061 ↗
24. Mixed alkali effect on Vickers hardness and cracking10.1016/j.jnoncrysol.2012.03.029 ↗
25. Mechanical properties of high-temperature-degraded yttria-stabilized zirconia10.1016/j.actamat.2014.01.017 ↗
26. Further damage induced by water in micro-indentations in phosphate laser glass10.1016/j.apsusc.2013.11.129 ↗
27. Effective elastic constants of plagioclase feldspar aggregates in dependence of the anorthite content - a concise review
28. Characterization of natural feldspars by Raman spectroscopy for future planetary exploration10.3749/canmin.46.6.1477 ↗
29. Raman and infrared spectroscopy study on structure and microstructure of glass-ceramic materials from SiO2-Al2O3-Na2O-K2O-CaO system modified by variable molar ratio of SiO2/Al2O310.1016/j.saa.2015.07.045 ↗
30. Raman study of anorthite, calcium Tschermank’s pyroxene, and gehlenite in crystalline and glassy state
31. Structural analysis of CaSiO3 glass by X-ray diffraction and Raman spectroscopy10.1016/0022-3093(86)90391-1 ↗
32. The medium range structure of sodium silicate glasses: a molecular dynamics simulation10.1016/j.jnoncrysol.2004.08.264 ↗
33. Investigation of ion-exchange ‘stuffed’ glass structures by molecular dynamics simulation10.1016/j.jnoncrysol.2012.05.025 ↗
34. Anorthite and CaAl2Si2O8 glass: low frequency Raman spectroscopy and neutron scattering10.1016/S0022-3093(03)00302-8 ↗
35. Thermal and physical properties of 30SrO–40SiO2–20B2O3–10A2O3 (A = La, Y, Al) glasses and their chemical reaction with bismuth vanadate for SOFC10.1016/j.ssi.2009.12.005 ↗
36. Compositional and microstructural design of highly bioactive P2O5-Na2O-CaO-SiO2 glass-ceramics10.1016/j.actbio.2011.10.014 ↗
37. Crystallization toughening of a model glass-ceramic10.1016/j.actamat.2014.12.007 ↗
38. First-principles investigation on crystal structure and physical properties of HfB410.1016/j.jallcom.2017.06.303 ↗
39. Mechanical anisotropy in austenitic NiMnGa alloy: nanoindentation studies