Brazing of zirconia to titanium using pure gold: Physicochemical aspects
Source abstract
Abstract
The main objective of this study is to investigate the influence of several experimental parameters on the evolution of the joint microstructure and interfaces during brazing of zirconia with titanium using pure gold foils 25–150 μm thick. The brazing experiments were carried out under high vacuum at 1080–1100°C with 3–60 minutes of holding time. Cross sections of the joints were characterized by SEM with EDX analysis, TEM and X-ray diffraction. Four intermetallics and a Ti-Au solid solution were formed at Au / Ti interface and a submicron Ti2O3 layer at Au / ZrO2 interface. The interdiffusion in Au-Ti intermetallics is so fast that brazing with thin gold foils (25–50 μm) can lead to a total consumption of the liquid Au. To avoid isothermal solidification of the joint and obtain a thin and continuous Ti2O3 layer, low temperature, thick gold foil and short holding time are recommended for the brazing process.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Intermetallics and Advanced Alloy Properties · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. Review: special brazing and soldering10.1016/j.jmapro.2020.10.049 ↗
2. A review on fusion welding of dissimilar ferritic/austenitic steels: processing and weld zone metallurgy
3. Friction-based welding processes: friction welding and friction stir welding10.1080/01694243.2020.1780716 ↗
4. Dissimilar friction stir welding process-a review
5. Friction stir based welding, processing, extrusion and additive manufacturing
6. Adhesive wafer bonding10.1063/1.2168512 ↗
7. Recent development of ultrasonic brazing10.1007/s00170-021-06885-y ↗
8. Kinetics of voids evolution during diffusion bonding of dissimilar metals on consideration of the realistic surface morphology: Modeling and experiments10.1016/j.actamat.2024.120121 ↗
9. Overview of transient liquid phase and partial transient liquid phase bonding10.1007/s10853-011-5561-1 ↗
10. A review on the friction stir brazing for joining dissimilar materials
11. New attempt to improve friction stir brazing10.1016/j.matlet.2021.130688 ↗
12. Investigation into novel multipass friction stir vibration brazing of carbon steels10.1080/10426914.2021.2006220 ↗
13. M.G. Nicholas, The Brazing of Ceramics: Material Science Aspect of Reactive Braze Alloys, in Proceedings of the NATO Advanced Research Workshop on Interfacial Science in Ceramic Joining 1997. NATO ASI Series. 58 (1997) 97-109. https:\\doi: 10.1007/978-94-017-1917-9.10.1007/978-94-017-1917-9_9 ↗
14. N. Eustathopoulos, M.G. Nicholas, B. Drevet, Wettability at high temperatures, Pergamon Materials Series. Series Editor: R.W. Cahn.1999.
15. B. Hausner, B. Wielage, Chapter 12: Brazing of metals and ceramics joints, Advances in Brazing. Science, Technology and Applications. Editor: D.P. Sekulić. 2013.10.1533/9780857096500.2.361 ↗
16. Interfacial reactions between sapphire and Ag-Cu-Ti-based active braze alloys10.1016/j.actamat.2015.11.019 ↗
17. Brazing filler metals10.1080/09506608.2019.1613311 ↗
18. Recent advances in brazing fillers for joining of dissimilar materials10.3390/met11071037 ↗
19. N. Eustathopoulos, F. Hodaj, O. Kozlova, Chapter 1: The wetting process in brazing, Advances in Brazing. Science, Technology and Applications. Editor: D.P. Sekulić. 2013.10.1533/9780857096500.1.3 ↗
20. N. Eustathopoulos, F. Hodaj, Wetting and Capillarity in Brazing, Brazing Handbook.Volume 1. Series AWS Handbooks. Publisher: American Welding Society. 2021.
21. Wetting and interfacial reactions in liquid Au-Ti alloys / ZrO2 system10.1016/j.jeurceramsoc.2023.05.035 ↗
22. Zirconia-titanium joint interfaces10.4028/www.scientific.net/MSF.207-209.145 ↗
23. Active metal brazing of zirconia10.1016/S1359-6454(00)00256-1 ↗
24. Interactions at zirconia-Au-Ti interfaces at high temperatures10.4028/www.scientific.net/KEM.206-213.487 ↗
25. Interactions, joining and microstructure of Sn-Ti/ZrO2 system10.1016/j.jeurceramsoc.2018.12.010 ↗
26. Brazing of zirconia with AgCuTi and SnAgTi active filler metals10.1007/s11661-000-0169-0 ↗
27. Microstructure evolution and mechanical properties of ZrO2/ZrO2 joints brazed with Ni-Ti filler metal10.1088/2053-1591/ab574b ↗
28. Joining of zirconia to zirconia using AgCuTi filler metal10.1016/0924-0136(94)01611-4 ↗
29. Joining of zirconia to metals using Zr-Cu alloy10.1016/0013-7944(91)90254-X ↗
30. Effect of filler metal composition on the strength of Yttria stabilized zirconia joints brazed with Pd-Ag-CuOx10.1007/s11661-008-9565-7 ↗
31. Brazing YSZ ceramics by a novel SiO2 nanoparticles modified Ag filler10.1016/j.ceramint.2020.03.214 ↗
32. Interfacial characterization and mechanical properties of reactive air brazed ZrO2 ceramic joints with Ag–CuO–Al2TiO5 composite filler metal10.1016/j.ceramint.2021.07.076 ↗
33. Microstructural evolution and bonding mechanisms of the brazed Ti/ZrO2 joint using an Ag10.1557/jmr.2014.30 ↗
34. Evolution of the interlayer microstructure and the fracture modes of the zirconia/Cu-Ag-Ti filler/Ti active brazing joints10.1016/j.matlet.2006.05.024 ↗
35. Joining of yttria stabilised zirconia to Ti6Al4V alloy using novel CuO nanostructure reinforced Cu foam interlayer10.1016/j.matlet.2019.06.029 ↗
36. Interface microstructure and mechanical behaviour of brazed TA6V/zirconia joints10.1007/BF00721864 ↗
37. Zirconia to Ti-6Al-4V braze joint for implantable biomedical device10.1002/jbm.b.30161 ↗
38. Effects of fabrication parameters on interface of zirconia and Ti-6Al-4V joints using Zr55Cu30Al10Ni5 amorphous filler10.1007/s11665-013-0534-y ↗
39. Microstructural and mechanical properties of jointed ZrO2/Ti-6Al-4V alloy using Ti33Zr17Cu50 amorphous brazing filler10.1016/j.matdes.2012.12.023 ↗
40. Effect of interface microstructure on joint strength of zirconia/titanium alloy brazed with amorphous Zr-Ti-Ni-Cu active filler metal10.3390/met10060718 ↗
41. Joining of Zirconia and Ti-6A1–4 V Using a Ti-based Amorphous Filler10.1016/S1005-0302(11)60121-7 ↗
42. Vacuum brazing of YSZ ceramic and TC4 alloy with a Ti20Zr20Hf20Cu20Ni20 high entropy amorphous alloy10.1016/j.msea.2022.143815 ↗
43. S. Agathopoulos, S. Pina, R.N. Correia, A Review of Recent Investigations on Zirconia Joining for Biomedical Applications, in: C.A. Lewinsohn, M. Singh, R. Loehman (Eds), Advances in Joining of Ceramics, Ceramic Transactions Series. (2006) 135-147. https://doi: 10.1002/9781118405802.ch7.10.1002/9781118405802.ch7 ↗
44. Evaluation of Biomedical Ti / ZrO2 Joint Brazed with Pure Au Filler: Microstructure and mechanical properties10.3390/met10040526 ↗
45. Influence of pH on the corrosion behavior of biomedical Ti/Au/ZrO2 brazing joints
46. Brazing of zirconia to titanium using Ag-Cu and Au-Ni filler alloys10.1590/S0104-92242013000400007 ↗
47. M. Fischer, Physico-chemistry of zirconia to titanium brazing using pure gold: wetting and interfacial reactivity, PhD thesis Univ. Grenoble Alpes France, 2022, [Online]. Available: 〈https://theses.hal.science/tel-03772548%0Ahttps://theses.hal.science/tel-03772548/document〉.
48. Low temperature brazing between pre-metallized ZrO2 ceramics and medical pure titanium using AuSn20 filler metal10.1016/j.vacuum.2022.111537 ↗
49. Interfacial reaction behavior and mechanical characterization of ZrO2/TC4 joint brazed by Ag-Cu filler metal10.1016/j.msea.2015.08.067 ↗
50. Blackening mechanism and mechanical properties variation of zirconia ceramic induced by active metal brazing10.1002/adem.202200105 ↗
51. Brazing ZrO2 ceramic to Ti-6Al-4V alloy using NiCrSiB amorphous filler foil: Interfacial microstructure and joint properties10.1016/j.matchar.2013.04.009 ↗
52. Interfacial microstructure and mechanical properties of ultrasonic-assisted brazing joints between Ti–6Al–4V and ZrO210.1016/j.ceramint.2019.11.276 ↗
53. M. Fischer, V. Chaumat, G. Tourrel, F. Hodaj, Wetting and reactivity of zirconia by Au-Ti active alloys in view of zirconia / titanium brazing with pure gold, in Proceedings of 8th International Brazing and Soldering Conference IBSC 2021. Ed. R. Gourlay, American Welding Society, pp 1-5.
54. Automated crystal orientation and phase mapping in TEM10.1016/j.matchar.2014.08.010 ↗
55. Diffusion of Gold in β-Titanium10.4028/www.scientific.net/DDF.95-98.623 ↗
56. Autodifusion de titanio beta y hafnio beta10.1016/0001-6160(68)90010-2 ↗
57. Bulk and grain boundary diffusion of titanium in yttria-stabilized zirconia10.1016/S0955-2219(99)00212-5 ↗
58. Nist-Janaf Thermochemical Tables, J. Phys. Chem. Ref. Data, Monograph n°9, 4th edition, (1998).
59. Thermochemistry of binary liquid gold alloys: the, systems (Au + Cr), (Au+ V), (Au + Ti), and (Au + Sc) at 1379 K10.1007/BF02656716 ↗
60. Thermochemistry of binary alloys of transition metals: the Me-Ti, Me-Zr, and Me-Hf (Me = Ag, Au) systems10.1007/BF02675574 ↗
61. R.A. Robie, P.M. Bethke, K.M. Beardsley, Selected X-ray crystallographic data molar volumes, and densities of minerals and related substances, Geological Survey, Bulletin 1248, U.S. Government Printing Office, Washington, 1967, p. 55.10.3133/ofr66113 ↗
62. Density of liquid gold measured by a non-contact technique10.1007/BF03214876 ↗
63. New experimental setup for wettability characterization under monitored oxygen activity: I, role of oxidation state and defect concentration on oxide wettability by gold10.1111/j.1151-2916.1993.tb03941.x ↗
64. Investigation of interaction of metal melts and zirconia10.1007/s10853-005-1928-5 ↗