Enhancing oxidation resistance of silicon nitride using a Ca2+ stabilizer
Source abstract
Abstract
Silicon nitrides are widely used in ceramic heaters for combustion engines due to their high strength and wear resistance. However, their poor oxidation resistance at elevated temperatures limits their reliability. Oxidation products, such as silica and intermediate compounds from sintering additives, often suffer from microcracks due to phase transformation and volume expansion mismatch during thermo-mechanical cycles. Use of cation dopants to chemically stabilize the transformation of the oxidation front is proposed. This study investigated the effect of Ca 2+ treatment on Si 3 N 4 with MgO and Y 2 O 3 sintering aids. The Si 3 N 4 samples were coated with CaO and the phase composition, microstructure, and chemical distribution of the oxidation products were analyzed using XRD, SEM, TEM, STEM, and EDS. The oxidation coupon tests revealed that the CaO coating effectively protected Si 3 N 4 from oxidation at 1300 ºC for 40 h. Moreover, the microstructure analysis showed that CaO coating created more favorable microstructures which reduced oxidation reactions.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Advanced ceramic materials synthesis · Electronic and Structural Properties of Oxides
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Degradation oF Silicon Nitride Glow Plugs in Various Environments Part 3: NGDI engine10.1111/j.1744-7402.2011.0202724.x ↗
2. Motily A. Evaluation of hot surface ignition device performance with high-pressure kerosene fuel sprays. PhD Thesis; 2020.10.2514/6.2021-0414 ↗
3. Development of a high-strength Si3N4 sintered body10.1016/0263-4368(91)90021-F ↗
4. Corrosion of silicon-based ceramics in combustion environments10.1111/j.1151-2916.1993.tb03684.x ↗
5. VS. High-Temperature Oxidation Behavior of High-Purity α-, β-, and Mixed Silicon Nitride Ceramics10.1111/j.1151-2916.2002.tb00101.x ↗
6. 2008
7. Problems with glow plug – a review10.19206/CE-140114 ↗
8. Mechanism of Liquid-Phase Sintering of Silicon Carbide and Nitride with Oxide Activating Additives10.1007/s10717-013-9557-y ↗
9. Oxidation Behavior of Rare-Earth Disilicate–Silicon Nitride Ceramics10.1111/j.1151-2916.1992.tb04463.x ↗
10. Oxidation Behavior of Chemically-Vapor-Deposited Silicon Carbide and Silicon Nitride from 1200° to 1600°C10.1111/j.1151-2916.1998.tb02431.x ↗
11. Influence of rare-earth oxide additives on the oxidation resistance of Si3N4–SiC nanocomposites10.1016/j.jeurceramsoc.2013.01.008 ↗
12. High oxidation resistance of hot pressed silicon nitride containing yttria and lanthania10.1016/S0955-2219(98)00237-4 ↗
13. Toughening of Mullite/Cordierite Laminated Composites by Transformation Weakening of β-Cristobalite Interphases10.1111/j.1551-2916.2005.00303.x ↗
14. Thermal shock resistance of Si3N4 and Si3N4–SiC ceramics with rare-earth oxide sintering additives10.1016/j.jeurceramsoc.2014.04.034 ↗
15. Effect of Re2O3–MgO additives on the microstructure evolution and properties of β-Si3N4 ceramics10.1016/j.ceramint.2021.04.228 ↗
16. Effects of rare-earth (RE) intergranular adsorption on the phase transformation, microstructure evolution, and mechanical properties in silicon nitride with RE2O3 +MgO additives: RE=La, Gd, and Lu10.1111/j.1551-2916.2008.02448.x ↗
17. Abnormal behavior of silica doped with small amounts of aluminum
18. Pressureless sintering of silicon nitride with magnesia and yttria10.1016/j.matchemphys.2004.08.041 ↗
19. General relationship for the thermal oxidation of silicon10.1063/1.1713945 ↗
20. Synthesis and hydration study of portland cement components prepared by the organic steric entrapment method10.1007/BF02480579 ↗
21. Structure and chemistry of interfaces in Si3N4 ceramics studied by transmission electron microscopy10.2109/jcersj.105.453 ↗
22. Microstructure and thermal conductivity of gas-pressure-sintered Si3N4 ceramic: the effects of Y2O3 additive content10.1016/j.jeurceramsoc.2020.08.035 ↗
23. Preparation and properties of Si3N4 ceramics via digital light processing using Si3N4 powder coated with Al2O3-Y2O3 sintering additives
24. Study on the thermal conductivity of silicon nitride ceramics with magnesia and yttria as sintering additives10.1016/S0167-577X(02)00690-0 ↗
25. Paralinear oxidation of silicon nitride in a water-vapor/oxygen environment10.1111/j.1151-2916.2003.tb03461.x ↗
26. Oxidation of silicon nitride hot pressed with Y2O3+MgO10.1007/BF00543830 ↗
27. Oxidation behaviour of pressureless liquid-phase-sintered α-SiC with additions of 5Al2O3+3RE2O3 (RE=La, Nd, Y, Er, Tm, or Yb)10.1016/j.jeurceramsoc.2010.07.013 ↗
28. Identification of oxidation mechanisms in silicon nitride ceramics by transmission electron microscopy studies of oxide scales10.1557/JMR.1995.2306 ↗
29. Critical thermodynamic evaluation and optimization of the CaO–MgO–SiO2 system10.1016/j.jeurceramsoc.2004.02.012 ↗
30. Coesite Formation at ambient pressure and low temperatures10.1155/2008/406067 ↗
31. Theoretical investigation of the solid state reaction of silicon nitride and silicon dioxide forming silicon oxynitride (Si2N2O) under pressure10.1002/zaac.200300122 ↗
32. Effect of rare earth oxides addition on the mechanical properties and coloration of silicon nitride ceramics10.1016/j.jeurceramsoc.2019.11.058 ↗
33. On the effect of local grain-boundary chemistry on the macroscopic mechanical properties of a high-purity Y2O3 -Al2O3-containing silicon nitride ceramic: role of oxygen10.1111/j.1551-2916.2005.00412.x ↗
34. Factors influencing structural evolution in the oxide of hot-pressed Si3N4-Y2O3-SiO2 materials10.1007/BF02396923 ↗
35. Relationship between topological order and glass forming ability in densely packed enstatite and forsterite composition glasses10.1073/pnas.1104692108 ↗
36. Oxidation behaviour and strength degradation of a Yb2O3−SiO2−doped hot-pressed silicon nitride between 1200 and 1500°C