journal article·2025-09

Effect of molten NaCl on the wet oxidation behavior of Al2O3-modified SiC-B4C ceramics at 1300 ℃

Qingliang Shan, Ziluo Lin, Hongbin Zhang, Xiao You, Xiangkun Tian, Rui Li, Junjie Qian, Hao Qin

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Nuclear materials and radiation effects

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
2. Accelerated oxidation of SiC CMC’s by water vapor and protection via environmental barrier coating approach10.1016/S0955-2219(02)00141-3 ↗
3. Degradation of a SiC-SiC composite in water vapor environments10.1111/jace.16838 ↗
4. Effect of coating defects on oxidation behavior of three dimensional C/SiC composites from room temperature to 1500°C10.1023/A:1021089411141 ↗
5. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
6. Oxidation behavior of a multi-layered ceramic-matrix composite (SiC)f/C/(SiBC)m10.1016/S0266-3538(00)00243-8 ↗
7. Fatigue behavior of a Hi-NicalonTM/SiC-B4C composite at 1200°C in air and steam10.1016/j.msea.2011.11.049 ↗
8. Boron-bearing species in ceramic matrix composites for long-term aerospace applications10.1016/j.jssc.2003.03.005 ↗
9. Oxidation behavior of Cf/SiC composite with CVD Si-B-C coating in a wet oxygen environment10.1007/s10443-008-9077-z ↗
10. Hot-corrosion of silicon carbide in combustion gases at temperatures above the dew point of salts10.1016/S0955-2219(98)00239-8 ↗
11. Molten salt corrosion of SiC and Si3N4 ceramics10.1111/j.1151-2916.1976.tb10962.x ↗
12. High-temperature Na2SO4 deposit-assisted corrosion of silicon carbide - I: temperature and time dependence10.1111/jace.13409 ↗
13. High temperature oxidation and microstructural evolution of SiC layer of TRISO particles in the presence of NaCl10.1016/j.matchemphys.2023.127906 ↗
14. Investigation of alkali induced corrosion of SiC filter candles at high temperature, in gasification environment10.1016/j.jeurceramsoc.2013.10.035 ↗
15. Effects of molten Na2SO4 on wet oxidation behavior of SiCf/SiC composites above 1200 ℃10.1016/j.jeurceramsoc.2022.11.038 ↗
16. High temperature Na2SO4 deposit-assisted corrosion of silicon carbide–II: effects of B, C, and Si10.1111/jace.14596 ↗
17. Mechanical properties and oxidation behaviors of self-healing SiCf/SiC-SiBCN composites exposed to H2O/O2/Na2SO4 environments10.1007/s40195-023-01596-7 ↗
18. SiO2-B2O3-BaO-WO3 glasses with varying Al2O3 content as a sealing material for reversible solid oxide fuel cells10.1016/j.ceramint.2020.04.148 ↗
19. Preparation of Ni2P supported on Al2O3 and B2O3 mixed oxides by temperature-programmed reduction of phosphate precursors with low P/Ni ratios10.1007/s11244-020-01344-6 ↗
20. Oxidation behaviour of ZrB2-SiC (Al/Y) ceramics at 1700 ℃10.1016/j.jeurceramsoc.2016.02.037 ↗
21. ZrB2-SiC(Al) ceramics with high resistance to oxidation at 1500 ℃10.1016/j.corsci.2013.04.037 ↗
22. More effective crack self-healing capability of SiCf/SiC-B4C with Al2O3 modified under wet environment10.1111/jace.17371 ↗
23. Oxidation behavior in wet oxygen environment of Al2O3, added reaction-sintered Si-B-C ceramics10.1016/j.ceramint.2017.11.196 ↗
24. The anti-oxidation mechanism of SiCf/SiC-B4C modified with Al2O3 in wet atmosphere based on machine learning10.1111/jace.18525 ↗
25. Hot corrosion of Al2O3 and SiC ceramics by KCl-NaCl molten salt10.2109/jcersj2.123.685 ↗
26. Microstructural evolution during the infiltration of boron carbide with molten silicon10.1016/j.jeurceramsoc.2009.09.021 ↗
27. Structural studies of silicate glasses and melts-applications and limitations of Raman spectroscopy
28. Vibrational study of the role of trivalent ions in sodium trisilicate glass10.1016/0022-3093(94)90030-2 ↗
29. Effect of Fe2O3 concentration on the structure of the SiO2-Na2O-Al2O3-B2O3 glass system10.1016/j.saa.2011.05.074 ↗
30. Investigation of the viscosity and structural properties of CaO-SiO2-TiO2 slags10.1007/s11663-014-0053-8 ↗
31. Raman spectroscopy of borosilicate and germanate-silicate glasses and melts10.1134/S0036029511080040 ↗
32. Structure and mechanical properties of compressed sodium aluminosilicate glasses: role of non-bridging oxygens10.1016/j.jnoncrysol.2016.03.011 ↗
33. Crystallization of R2O-MgO-Al2O3-B2O3-SiO2-F (R=K+, Na+) glasses with different fluorine source10.1016/S0167-577X(00)00201-9 ↗
34. Raman spectroscopy of heat-treated B2O3-SiO2 glasses10.1111/j.1151-2916.1981.tb09893.x ↗
35. Structural investigation in the TiB2-(Na2O-B2O3-Al2O3) system10.1016/j.jssc.2010.07.023 ↗
36. Raman study of lead borate glass10.1016/0022-3093(90)90823-5 ↗
37. Raman spectral studies of borate glasses10.1016/0022-3093(93)91277-A ↗
38. Effect of chlorine on the viscosities and structures of blast furnace slags10.1080/03019233.2016.1234541 ↗
39. FTIR, Raman and NMR investigation of CaO-SiO2-P2O5 and CaO-SiO2-TiO2-P2O5 glasses10.1016/j.jnoncrysol.2015.04.017 ↗
40. Short-range and medium-range structural order in CaO-SiO2-TiO2-B2O3 glasses10.2355/isijinternational.ISIJINT-2015-586 ↗
41. Effect of B2O3 on structure of CaO-Al2O3-SiO2-TiO2-B2O3 glassy systems10.2355/isijinternational.ISIJINT-2019-679 ↗
42. Factors Affecting Microscopic Basicity of Silicate Glasses from the Perspective of O1s Binding Energy
43. H. Urie-Lopez-Herrera, J. Escorcia-Garc, C.A. Guti-errez-Chavarr, V. Agarwal, V.E. Ceniceros-Orozco Influence of CaO and Dy2O3 on the structural, chemical and optical properties of thermally stable luminescent silicate nano-glass-ceramics, J. Mater. Res. Technol. 20 (2022) 1544-1557.10.1016/j.jmrt.2022.07.148 ↗
44. Influence of β-Si3N4 whiskers on sintering and crystallization of fused silica ceramics10.1111/jace.18800 ↗
45. Preparation of Al2O3‑SiO2 aerogel by ambient pressure drying for thermal insulation application10.1007/s10934-023-01457-9 ↗
46. Bridging, non-bridging and free (O2–) oxygen in Na2O-SiO2 glasses: an X-ray Photoelectron Spectroscopic (XPS) and Nuclear Magnetic Resonance (NMR) study10.1016/j.jnoncrysol.2010.09.031 ↗
47. Ab initio molecular orbital calculations on the electronic structure of sodium silicate glasses10.1021/j100167a021 ↗
48. X-ray photoelectron spectroscopy of sodium borosilicate glasses10.1016/S0022-3093(01)00720-7 ↗
49. Performance and transition mechanism from acidity to basicity of amphoteric oxides (Al2O3 and B2O3) in SiO2-CaO-Al2O3-B2O3 system: a molecular dynamics study10.1016/j.ceramint.2021.01.074 ↗
50. Raman and infrared spectroscopy study on structure and microstructure of glass-ceramic materials from SiO2-Al2O3-Na2O-K2O-CaO system modified by variable molar ratio of SiO2/Al2O310.1016/j.saa.2015.07.045 ↗
51. Structure-viscosity relationship of low-silica calcium aluminosilicate melts10.2355/isijinternational.54.2031 ↗
52. Tuning the interfacial reaction between CaO-SrO-Al2O3-B2O3-SiO2 sealing glass-ceramics and Cr-containing interconnect: crystalline structure vs. glass structure10.1016/j.jeurceramsoc.2014.01.023 ↗
53. Lowenstein’s rule in zeolite A: a computational study10.1016/0144-2449(92)90065-W ↗
54. Degradation mechanisms of a self-healing SiC(f)/BN(i)/[SiC-B4C](m) composite at high temperature under different oxidizing atmospheres10.1016/j.jeurceramsoc.2018.05.001 ↗