journal article·2002-10

Stability of intergranular phases in hot-pressed Si3N4 studied with mechanical spectroscopy and in-situ high-temperature XRD

R.G. Duan, G. Roebben, J. Vleugels, O. Van der Biest

Publisher page

Abstract

Abstract The impulse excitation technique (IET) and high temperature X-ray diffraction (HTXRD) were used to investigate the intergranular glass phase and its crystallisation behaviour in four hot-pressed silicon nitrides. The internal friction or damping peak height measured with IET near the glass transition temperature, T g , is used as a qualitative indicator for the amount of residual intergranular amorphous phase after sintering. Silicon nitride powder was hot-pressed with different sintering additives. The silicon nitride containing 4 wt.% Al 2 O 3 does not reveal an internal friction peak at T g , i.e. it does not contain a significant amount of intergranular glass phase. Three other silicon nitrides, containing either 8 wt.% Y 2 O 3 , 6 wt.% Y 2 O 3 +2 wt.% Al 2 O 3 , or 2 wt.% Y 2 O 3 +4 wt.% Al 2 O 3 +2 wt.% TiN, do show an internal friction peak near T g . This “ T g -peak” is nearly unaffected by heating up to 1400 °C in the silicon nitride with Y 2 O 3 +Al 2 O 3 +TiN sintering aids, whereas the amount of intergranular glass in the ceramics containing either Y 2 O 3 +Al 2 O 3 or Y 2 O 3 as a sintering aid is strongly reduced by subsequent heating. As observed from HTXRD, the onset temperature of crystallisation of the intergranular glass in the ceramic containing Y 2 O 3 +Al 2 O 3 sintering aids is about 1100 °C, with the formation of Y–N-apatite (Y 20 N 4 Si 12 O 48 ) and O-sialon (Al 0 . 04 Si 1 . 96 N 1 . 96 O 1 . 04 ). The O-sialon phase in the yttria and alumina containing ceramics, formed either during sintering or during heat treatment, is not stable at elevated temperatures and dissolves in the intergranular glass phase between 1300 and 1400 °C. The O-sialon phase in the ceramic without Y 2 O 3 sintering additive, however, is thermally stable. The presence of Ti 4+ ions in the intergranular glass phase is suggested to inhibit its crystallisation, resulting in a stable high temperature damping behaviour.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Glass properties and applications · Nuclear materials and radiation effects

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
2. Fabrication and properties of dense polyphase silicon nitride
4. Structure and chemistry of interfaces in Si3N4 ceramics studied by transmission electron microscopy10.2109/jcersj.105.453 ↗
5. Effect of grain growth of β-silicon nitride on strength, Weibull modulus, and fracture toughness10.1111/j.1151-2916.1993.tb06670.x ↗
6. Nitrogen self-diffusion in silicon nitride10.1063/1.433464 ↗
7. Development, characterisation and oxidation behaviour of Si3N4–Al2O3 ceramics10.1016/0955-2219(94)90135-X ↗
8. Viscous energy dissipation at high temperature in silicon nitride10.1016/S1359-6454(98)00131-1 ↗
9. Evolution of grain boundary films in liquid phase sintered silicon nitride during high temperature testing10.1016/S1359-6454(98)00183-9 ↗
10. Mode 1 fracture toughness of a small-grained silicon nitride10.1111/j.1151-2916.1999.tb02134.x ↗
11. Oxidation behaviour of hot-pressed Si3N4 with Re2O3 (Re=Y, Yb, Er, La)10.1016/S0955-2219(99)00077-1 ↗
12. High-temperature properties of Si3N4 ceramics10.1557/S0883769400049186 ↗
13. Strength and microstructure of sintered Si3N4 with rare-earth-oxide additions
14. Effect of grain-boundary crystallisation on the high temperature strength of silicon nitride10.1007/BF00553273 ↗
15. Grain-boundary phase crystallisation and strength of silicon nitride sintered with a YSiAlON glass10.1111/j.1151-2916.1990.tb09803.x ↗
16. Effect of crystallising the grain-boundary glass phase on the high-temperature strength of hot-pressed Si3N4 containing Y2O310.1111/j.1151-2916.1975.tb11488.x ↗
17. The effect of Ti4+ on the site of Al3+ in the structure of CaO–Al2O3–SiO2–TiO2 system glass10.1016/S0921-5093(98)00570-X ↗
18. Effect of changing TiO2 content on structure and crystallisation of CaO–Al2O3–SiO2 system glasses10.1016/S0955-2219(98)00105-8 ↗
19. A critical evaluation of indentation techniques for measuring fracture toughness10.1111/j.1151-2916.1981.tb10320.x ↗
20. Impulse excitation apparatus to measure resonant frequencies, elastic moduli, and internal friction at room and high temperature10.1063/1.1148422 ↗
21. ASTM E 1876-99, Am. Soc. Testing and Materials, 2000.
22. Dense single-phase β-sialon ceramics by glass-encapsulated hot isostatic pressing10.1007/BF01105715 ↗
23. Composition and stability of Y–Si–Al–O–N solid solutions based on α-Si3N4 structure10.1007/BF00569297 ↗
24. Glass transition and α relaxation in Y–Si–Al–O–N glasses and in Si3N4 ceramics studied by mechanical spectroscopy10.1080/01418619708200008 ↗
25. Structure and viscosity of grain boundary in high-purity sialon ceramics10.1111/j.1151-2916.2000.tb01589.x ↗
26. The kinetics of precipitation from supersaturated solid solutions10.1016/0022-3697(61)90054-3 ↗
27. Epitaxial deposition of silicon nitride during post-sintering heat treatment10.1007/BF00729782 ↗
28. High temperature viscosity of nitrogen modified silica glass10.1016/S0022-3093(00)00005-3 ↗
29. Synthesis and characterisation of a SiAlON glass10.1111/j.1151-2916.1990.tb07617.x ↗
30. Evidence for the formation of SiON glasses10.1016/S0022-3093(97)00467-5 ↗
31. Properties of soda aluminosilicate glasses, 110.1111/j.1151-2916.1962.tb11040.x ↗
32. Structure of sodium aluminosilicate melts containing at least 50 mol.% SiO2 at 1500 °C10.1063/1.1727145 ↗
33. The stable energy of glass structure unit10.2320/matertrans1989.39.1162 ↗
34. Effects of temperature on viscosities and elastic modulus of oxynitride glass10.4028/www.scientific.net/KEM.89-91.351 ↗
35. Solubility of aluminium in silicon oxynitride10.1007/BF01756778 ↗
36. The influence of different oxides on the formation of Si2N2O from SiO2 and Si3N410.1016/0955-2219(90)90028-E ↗