journal article·2003-02

Metallorganic chemical vapor deposition of Ta2O5 films

A Porporati, S Roitti, O Sbaizero

Publisher page

Abstract

Abstract Ta2O5 films were grown by Pulsed-Metal Organic Chemical Vapor Deposition (Pulsed-MOCVD). This technique utilizes direct liquid injection of a precursor solution using an ultrasonic nozzle to introduce the precursor vapour into the low-pressure vertical cold-wall reactor. Tantalum (V) ethoxide (C10H25O5Ta) was chosen as alkoxide because it is already an oxygen-containing precursor and its decomposition temperature is low. Films were grown in the temperature range 400–800 °C. Three solution concentrations were tested (1, 2 and 4 vol.%). Experimental results were analysed to determine the growth rate controlling mechanisms and film quality. The highest growth rate was achieved with the most dilute solution and film thickness of 3 μm was achieved with this technology with a growing rate of 8.52 μm/h. The refractive index and dielectric constant of the films increase with the growth in temperature, and as for the growing rate, the 1 vol.% solution leads to the best results. Analysis shows that the morphology and porosity of the films can be controlled by deposition temperature and solution concentration. Pulsed-MOCVD has demonstrated good performance with uniform film thickness and high growth rate.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Optical Coatings and Gratings · Semiconductor materials and devices · ZnO doping and properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. Tantalum pentoxide for advanced DRAM applications10.1016/S0040-6090(96)08975-4 ↗
2. UV-O3 and dry O2–2 step annealed chemical vapor deposition Ta2O5 films for storage dielectrics of 64-MB drams10.1109/16.75185 ↗
3. Anmorphous silicon thin film transistors employing photoprocessed tantalum oxide films as gate insulator10.1143/JJAP.29.62 ↗
4. Electroluminescence of Tb3+ -doped anodic Ta2O5 films10.1021/j100147a032 ↗
5. A fiber optic wavelength modulation sensor based on tantalum pentoxide coatings for absolute temperature measurements10.1007/s10043-000-0205-8 ↗
6. Thin tantalum and tantalum oxide films grown by pulsed laser deposition10.1016/S0169-4332(00)00605-X ↗
7. Sputtered Ta2O5 antireflection coatings for silicon solar cells10.1016/0040-6090(82)90545-4 ↗
8. The migration of fluoride ions in growing anodic oxide films on tantalum10.1149/1.1837425 ↗
9. Dielectric constants of Ta2O5 thin films deposited by Rf sputtering10.1016/0040-6090(95)08234-4 ↗
10. Ohlsen–Tantalum oxide films on silicon grown by tantalum evaporation in atomic oxygen10.1016/0040-6090(96)08667-1 ↗
11. Properties of Ta2O3-based dielectric nanolaminates deposited by atomic layer epitaxy10.1149/1.1837399 ↗
12. Tang · Rev. Laser Eng. · 1996 · 24 · 11010.2184/lsj.24.110 ↗
13. Structural and optical properties of sol-gel deposited proton conducting Ta2O5 films10.1007/BF02436926 ↗
14. Autran · Le Vide: Science, Technique and Application · 1995 · 275 · 44
15. Experimental characterization and modeling of Pulsed-MOCVD utilizing ultrasonic atomization of liquid precursor10.1002/1521-3862(200103)7:2<85::AID-CVDE85>3.0.CO;2-9 ↗
16. Unique precursor delivery and control afforded by low-pressure Pulsed-CVD process with ultrasonic atomisation10.1051/jp4:20013146 ↗
17. Atomic layer epitaxy growth of tantalum oxide thin films from Ta(OC2H5)5 and H2O10.1149/1.2048637 ↗
18. Conversion efficiency of alkoxide precursor to oxide films grown by an ultrasonic-assisted, pulsed liquid injection, metalorganic chemical vapor deposition (Pulsed-CVD) process10.1111/j.1151-2916.1999.tb01968.x ↗