The elasto-plastic properties and contact damage evolution of a commercial polycrystalline silicon nitride are evaluated as a function of temperature up to 1000 °C, using a recently developed method combining Hertzian indentation and FEM simulation. The results of the study are compared to existing data for other ceramic materials such as alumina and zirconia. Silicon nitride is found to exhibit an excellent combination of elasto-plastic properties in the pre-creep temperature range and good contact damage resistance. These qualities make this material ideal for high temperature applications in general, and in particular to be used in spherical indenters for the evaluation of mechanical properties of other materials at elevated temperature using the procedure applied in this work.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Metal and Thin Film Mechanics · Thermal properties of materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Application of Hertzian tests to measure stressstrain characteristics of ceramics at elevated temperatures10.1111/j.1551-2916.2006.01339.x ↗
2. Contact properties of yttria partially stabilized zirconia up to 1000 degrees C10.1111/j.1551-2916.2007.01963.x ↗
3. Temperature dependence of mechanical properties of alumina up to the onset of creep10.1016/j.jeurceramsoc.2007.02.191 ↗
4. Microstructure and room-temperature mechanical properties of SI3N4 with various alpha/beta phase ratios10.1023/A:1004497914264 ↗
5. Contact fatigue in silicon nitride10.1111/j.1151-2916.1999.tb01908.x ↗
6. Role of microstructure in Hertzian contact damage in silicon nitride. 1. Mechanical characterization10.1111/j.1151-2916.1997.tb03129.x ↗
7. Creep of silicon nitride10.1016/S0079-6425(03)00020-3 ↗
8. Creep mechanism of gas-pressure-sintered silicon nitride polycrystals—I. Macroscopic and microscopic experimental study10.1080/14786430410001725917 ↗
9. Creep mechanism of gas-pressure-sintered silicon nitride polycrystals—II. Deformation mechanism10.1080/14786430410001725926 ↗
10. Creep behaviour of two sintered silicon nitride ceramics10.1016/S0955-2219(02)00108-5 ↗
11. Assessment of the high temperature elastic and damping properties of silicon nitrides and carbides with the impulse excitation technique10.1016/S0955-2219(02)00111-5 ↗
12. Fatigue resistant silicon nitride ceramics due to anelastic deformation and energy dissipation10.1016/S0925-8388(00)00999-3 ↗
13. The innovative impulse excitation technique for high-temperature mechanical spectroscopy10.1016/S0925-8388(00)00966-X ↗
14. Roebben · 2000
15. High-temperature elastic-moduli of SI3N4 ceramics10.1143/JJAP.20.1751 ↗
16. Temperature dependence of Young's modulus in SI3N4-based ceramics: roles of sintering additives and of SiC-particle content10.1016/S1359-6454(02)00004-6 ↗
17. Tabor · 1951
18. Indentation of ceramics with spheres: a century after Hertz10.1111/j.1151-2916.1998.tb02580.x ↗
19. Johnson · 1985
20. On theory of Hertzian fracture10.1098/rspa.1967.0137 ↗
21. Contact fracture of brittle bilayer coatings on soft substrates10.1557/JMR.2001.0021 ↗
22. Effect of microstructural coarsening on Hertzian contact damage in silicon-nitride10.1007/BF01178419 ↗
23. Making ceramics ductile10.1126/science.263.5150.1114 ↗
24. Indentation fatigue—a simple cyclic Hertzian test for measuring damage accumulation in polycrystalline ceramics
25. Indentation stress–strain curves for “quasiductile” ceramics10.1016/1359-6454(95)00204-9 ↗
26. Stress analysis of contact deformation in quasi-plastic ceramics10.1111/j.1151-2916.1996.tb09023.x ↗
27. Cracking in ceramic/metal/polymer trilayer systems10.1557/JMR.2002.0163 ↗
28. Designing damage-resistant brittle-coating structures: I. Bilayers10.1016/S1359-6454(03)00290-8 ↗
29. Designing damage-resistant brittle-coating structures: II. Trilayers10.1016/S1359-6454(03)00263-5 ↗
30. The temperature dependence of the Young's modulus of MgSiN2, AlN and Si3N410.1016/S0955-2219(00)00210-7 ↗
31. Deformation and fracture of mica-containing glass–ceramics in Hertzian contacts10.1557/JMR.1994.0762 ↗