journal article·2004-05

Mechanical behaviour of ferroelectric films on perovskite substrate

O. Bernard, M. Andrieux, S. Poissonnet, A.-M. Huntz

Publisher page

Abstract

Abstract This paper is focused on the mechanical behaviour of single and multilayered ceramic systems on ceramic substrate. The ferroelectric ceramic PLT (Pb 0.9 La 0.1 TiO 3 ) was deposited using magnetron sputtering on (001) STO (SrTiO 3 ) and on a YBCO (YBa 2 Cu 3 O 7 ), as a 200 nm interlayer on STO. DRX and SEM observations were carried out to determine the microstructure of the various films, and TEM cross sections were realised to control the film thickness and grain epitaxial relationships. AFM was used as a roughness controller before and after deposition. Mechanical properties of the films and substrate were determined using micro and nanoindentation tests. Young’s modulus and hardness of each system (STO, PLT/STO, YBCO/STO, PLT/YBCO/STO) were calculated and a peculiar phenomenon, associated to the YBCO interlayer addition, was observed. This work shows that YBCO improve mechanical properties of multilayered ceramics.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Metal and Thin Film Mechanics · Ferroelectric and Piezoelectric Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Domain configurations due to multiple misfit relaxation mechanisms in epitaxial ferroelectric thin films. I. Theory10.1063/1.357097 ↗
2. Relative coherency strain and phase transformation history in epitaxial ferroelectric thin films10.1063/1.360978 ↗
3. Ferroelectric (Pb,La)(Zr,Ti)O3 epitaxial thin films on sapphire grown by rf-planar magnetron sputtering10.1063/1.337423 ↗
4. Crystallographic characterization of tetragonal (Pb,La)TiO3 epitaxial thin films grown by pulsed laser deposition10.1063/1.360120 ↗
5. Fatigue and dielectric properties of the (Pb,La)TiO3 thin films with various La concentrations10.1016/S0040-6090(00)01104-4 ↗
6. Indentation testing of engineering ceramics and cermets
7. New formula for indentation toughness in ceramics10.1007/BF01729352 ↗
8. A critical evaluation of indentation techniques for measuring fracture toughness. I. Direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
9. A critical evaluation of indentation techniques for measuring fracture toughness. II. Strength method10.1111/j.1151-2916.1981.tb10320.x ↗
10. Oliver · 1993
11. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
12. Epitaxial growth of (Pb,La)TiO3 thin films on (0001) Al2O3 and (001) SrTiO3 substrates by RF magnetron sputtering10.1080/00150199908009139 ↗
13. Mechanical behaviour of a multilayer system for microelectronic applications
14. High current YBa2Cu3O7-δ thick films on flexible nickel substrates with textured buffer layers10.1063/1.112830 ↗
15. Improvement of the conducting parameters of YBa2Cu3Ox films grown on sapphire through the use of strontium titanate buffer layer10.1134/1.1262242 ↗
16. Study of the mechanical properties of ceramic materials by the nanoindentation technique10.1016/S0955-2219(98)00083-1 ↗
17. Schutze · 1991
18. Plasticity and an inverse brittle-to-ductile transition in strontium titanate10.1103/PhysRevLett.87.085505 ↗
19. High-temperature indentation studies on the {110} plane of single-crystal magnesium oxide10.1111/j.1151-2916.1992.tb07218.x ↗
20. Nanoindentation and FEM study of the effect of internal stress on micro/nano mechanical property of thin CNx films10.1016/S0040-6090(00)01314-6 ↗
21. Assessment of coating hardness10.1179/sur.1987.3.1.69 ↗