journal article·2004-09

Probability of cone crack initiation due to spherical contact loading

V. Licht, P. Hülsmeier, T. Fett

Journal of the European Ceramic Society· Volume 24· Issue 10-11
Publisher page

Abstract

The probability of the extension of surface cracks due to spherical indentation is analyzed. Contact loading problems typically result in multi-axle and strongly inhomogeneous stress fields near the contact surface. This property which strongly affects the stress intensity factors is taken into account in the failure analysis. Edge cracks were selected to model the actually occurring surface flaws. The stress intensity factors were integrated with the weight function method, and propagation of pre-existing cracks was assessed by using an energy release rate failure criterion. For the statistical analysis the Weibull theory was extended in some points. By applying the method to the cone crack formation during a spherical indentation, it was found that the probability for cone crack formation increases abruptly, when a certain yield load is exceeded. Therefore, the loading range can be divided into a critical and a less critical section, which were found to correlate to separated spatial regions of an occurring local risk of fracture. Because of the effects discovered, it seems to be inevitable to consider the strongly inhomogeneous stress fields in a failure analysis of a contact loading problem.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Mechanical stress and fatigue analysis · Fatigue and fracture mechanics · Numerical methods in engineering

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Weibull · 1939
2. A statistical theory or the fracture of brittle structures subjected to nonuniform stress10.1115/1.3423310 ↗
3. Weakest link theory reformulated or arbitrary fracture criterion10.1111/j.1151-2916.1978.tb09327.x ↗
4. A general approach or the statistical analysis of multiaxial fracture10.1111/j.1151-2916.1978.tb09314.x ↗
5. A probabilistic analysis of fracture loci under bi-axial stress state10.1299/jsme1958.24.290 ↗
6. Surface flaw reliability analysis of ceramic components with the SCARE finite element postprocessor program
7. Heger · 1991
8. Statistical approaches to failure of ceramics reliability assessment10.1111/j.1151-2916.1988.tb05825.x ↗
9. A general strength distribution function for brittle materials10.1016/0955-2219(92)90021-5 ↗
10. New fracture statistics or brittle materials
11. Influence of the fracture criterion on the failure prediction of ceramics loaded in biaxial flexure10.1111/j.1151-2916.1991.tb07295.x ↗
12. On the contribution of notches to the failure probability of ceramic components10.1016/0955-2219(96)00011-8 ↗
13. Strength predictions or notched alumina specimens10.1016/S0955-2219(97)00137-4 ↗
14. Brückner-Foit, A., Hülsmeier, P., Sckuhr, M. and Riesch-Oppermann, H. Limitations of the Weibull theory in stress fields with pronounced stress gradients. In Internat. Gas Turbine and Aeroengine Congress and Exhibition, Munchen, 8–11 May, 2000. ASME, New York (2000-GT-663).10.1115/2000-GT-0663 ↗
15. Brückner-Foit, A., Diegele, E., Hülsmeier P., Rettig, U. and Hohmann, C. Prediction of the failure probability of high strength ceramics subject to thermal shock loading. In: Proceedings of the 26th Annual International Conference on Advanced Ceramics and Composites, Cocoa Beach, 13–18 January 2002.10.1002/9780470294741.ch17 ↗
16. Influence of stress gradients on failure in contact strength tests with cylinder loading10.1016/S0013-7944(01)00147-3 ↗
17. Effect of multiaxiality and stress gradients on failure in cylinder contact strength tests10.1016/S0955-2219(03)00024-4 ↗
18. On a statistical approach to brittle rupture or multiaxial states of stress10.1016/0013-7944(84)90168-1 ↗
19. Lawn · 1993
20. Indentation o ceramics with spheres: a century after Hertz10.1111/j.1151-2916.1998.tb02580.x ↗
21. Johnson · 1985
22. Some useful results in the classical Hertz contact problem10.1243/03093247V182101 ↗
23. Some useful results in the tangentially loaded Hertzian contact problem10.1243/03093247V182107 ↗
24. Über die Berührung fester elastischer Körper10.1515/crll.1882.92.156 ↗
25. Fett · 1997
26. Kinked cracks and Richard Fracture criterion10.1023/A:1022609012480 ↗
27. Predicting Hertzian fracture10.1023/A:1018500522014 ↗
28. Measurement of very slow crack growth in glass10.1111/j.1151-2916.2001.tb01058.x ↗
29. Fett, T., Effective Mode-II Stress Intensity Factor for Partially Opened Natural Cracks under Mixed-mode Loading. Presented at the ICF10,Honolulu, Dec. 2001.
30. Mixed-mode stress intensity factors or partially opened cracks10.1023/A:1012473700907 ↗