Preparation of c-axis-oriented Bi4Ti3O12 thick films by templated grain growth

Ping-Hua Xiang, Yoshiaki Kinemuchi, Koji Watari

Publisher page

Abstract

Abstract Highly c -axis-oriented Bi 4 Ti 3 O 12 thick films were successfully fabricated by templated grain growth. The effects of template particles and sintering conditions on grain orientation in thick films were investigated. SEM micrographs and X-ray diffraction (XRD) patterns exhibited that thick films were c -axis-oriented. The degree of grain orientation (Lotgering factor, f ) increases with increasing sintering temperature and soaking time. Highly c -axis-oriented thick film (orientation degree of ∼ 0.98) is obtained with the use of only 5 wt.% template particles by sintering at 1000 °C for 2 h. This film exhibits a better temperature-independent dielectric constant and a lower dielectric loss.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Multiferroics and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Materials for high-temperature acoustic and vibration sensors: a review
2. Materials of Bi4Ti3O12 type for high temperature acoustic piezo-sensors10.1016/S0924-4247(99)00223-X ↗
3. Lanthanum-substituted bismuth titanate for use in non-volatile memories10.1038/44352 ↗
4. Layered perovskites with giant spontaneous polarizations for nonvolatile memories10.1103/PhysRevLett.89.087601 ↗
5. Electrical and optical properties of ferroelectric Bi4Ti3O12 single crystals10.1063/1.1656542 ↗
6. Ferroelectric field effect memory device using Bi4Ti3O12 film10.1063/1.322014 ↗
7. Integration of ferroelectric thin films in to nonvolatile memories10.1116/1.578044 ↗
8. Preparation of C-axis-orientated thin films by metalorganic chemical vapor deposition10.1143/JJAP.32.4086 ↗
9. Oriented bismuth titanate thin films by single-solid-source metal-organic chemical vapour deposition10.1016/S0022-0248(99)00261-4 ↗
10. Microstructure, electrical conductivity, and piezoelectric properties of bismuth titanate10.1111/j.1151-2916.1996.tb08086.x ↗
11. Thick-film capacitors with relaxor dielectrics10.1016/S0955-2219(03)00358-3 ↗
12. Fabrication of PZT thick films on silicon substrates for piezoelectric actuator10.1023/A:1009924113335 ↗
13. Templated grain growth of textured bismuth titanate10.1111/j.1151-2916.1999.tb01854.x ↗
14. Fabrication of textured bismuth titanate by templated grain growth using aqueous tape casting10.1016/S0955-2219(03)00035-9 ↗
15. Topotactical reactions with ferrimagnetic oxides having hexagonal crystal structures-I10.1016/0022-1902(59)80070-1 ↗