New porous silicon carbide composite reinforced by intact high-strength carbon fibres
Source abstract
Abstract
A novel processing method to produce a carbon-fibre-reinforced silicon carbide (C/SiC) is presented and the mechanical properties are evaluated. The low-cost process yields a reaction bonded silicon carbide matrix but avoids efficiently reactive damage of the carbon fibres. Thus, the C/SiC-material shows a fibre-dominated behaviour due to high fibre strength and matrix porosity. The characteristics and mechanical properties of this C/SiC are highlighted. The discussion deals with the particular mechanical characteristics of porous-matrix materials relating to similar materials investigated hitherto.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Thermal properties of materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Ceramic fibres for reinforcement
2. Savage · 1993
3. Processing fiber reinforced ceramics with porous matrices
4. Review: The physics and mechanics of fibre-reinforced brittle matrix composites10.1007/BF00355946 ↗
5. Overview No. 85. The mechanical behavior of ceramic matrix composites10.1016/0001-6160(89)90291-5 ↗
6. The real structure of the interlayer between fibre and matrix and its influence on the properties of ceramic composites10.1002/pssa.2211460133 ↗
7. Chawla · 1993
8. Fiber-reinforced silicon carbide
9. Status of continuous fiber-reinforced ceramic matrix composite processing technology10.1002/9780470313008.ch26 ↗
10. Ceramic composites for applications at extremely high temperatures
11. Chemical vapor infiltration processing of ceramic matrix composites
12. CVD-processing of ceramic-ceramic composite materials
13. CVI composites
14. Design of gradient-CVI derived CMC components
15. Fiber-reinforced ceramic-matrix composites with a polysiloxane/boron-derived matrix10.1111/j.1151-2916.1997.tb03058.x ↗
16. The properties of carbon fibre/SiC composites fabricated through impregnation and pyrolysis of polycarbosilane10.1023/A:1004589316992 ↗
17. Fiber-reinforced composites with polymer-derived matrix: processing, matrix formation and properties10.1016/S1359-835X(98)00128-6 ↗
18. Carbon fibre-reinforced CMCs by PCS infiltration10.1023/A:1017990709819 ↗
19. Crack deflection at an interface between dissimilar elastic materials
20. Toughened silcomp composites – process and preliminary properties
21. Krenkel, W., Cost effective processing of CMC composites by melt infiltration (LSI-process). In 25th Annual International Conference on Advanced Ceramics & Composites 2001, Cocoa Beach (Florida, USA), American Ceramic Society, January 2001.
22. Carbon fibre reinforced CMCs: manufacture, properties, oxidation protection
23. The morphology of silicon carbide in C/C-SiC composites10.1016/S0921-5093(01)01719-1 ↗
24. Longitudinal and transthickness tensile behavior of several oxide/oxide composites10.1002/9780470294482.ch36 ↗
25. Notched fracture behavior of an oxide/oxide ceramic-matrix composite10.1111/j.1151-2916.1999.tb02207.x ↗
26. Processing and performance of an all-oxide ceramic composite10.1111/j.1151-2916.1998.tb02590.x ↗
27. Processing of damage-tolerant, oxidation-resistant ceramic matrix composites by a precursor infiltration and pyrolysis method10.1016/0921-5093(94)06513-6 ↗
28. Concept for a damage-tolerant ceramic composite with “strong” interfaces10.1111/j.1151-2916.1996.tb08138.x ↗
29. Oxide/oxide composites: control of microstructure and properties
30. Aluminosilicate fiber/mullite matrix composites with favorable high-temperature properties10.1016/S0955-2219(99)00260-5 ↗
31. Processing and microstructure of WHIPOX™
32. In-plane mechanical properties of an all-oxide ceramic composite10.1111/j.1151-2916.1999.tb02148.x ↗
33. Effects of matrix porosity on the mechanical properties of a porous-matrix, all-oxide ceramic composite10.1111/j.1151-2916.2001.tb01059.x ↗
34. Effect of cyclic infiltrations on microstructure and mechanical behavior of porous mullite/mullite composites10.1016/S0921-5093(01)01478-2 ↗
35. EN 658-5: Advanced Technical Ceramics; Mechanical properties of ceramic composites at room temperature. Part 5: Determination of shear strength by short span bend test (Three-point). German version. European Committee for Standardisation, 2002.
36. Determination of the in situ fiber strength of ceramic-matrix composites from crack-resistance evaluation using single-edge notched-beam tests10.1111/j.1151-2916.2000.tb01628.x ↗
37. Kuntz, M., Risswiderstand keramischer Faserverbundwerkstoffe. Ph.D. thesis, University of Karlsruhe, Karlsruhe, Germany, 1995.
38. C/C-SiC composites for advanced friction systems10.1002/1527-2648(20020717)4:7<427::AID-ADEM427>3.0.CO;2-C ↗
39. Schunk Kohlenstofftechnik GmbH, Werkstoff CF 222. Datenblatt. Data Sheet. Heuchelheim, August 2003.
40. Applications of non-oxide CMCs
41. Thermomechanical properties of carbon fibres at high temperatures (up to 2000 °C)10.1016/S0266-3538(01)00140-3 ↗