Abstract Low-temperature sintering of 12Pb(Ni 1/3 Sb 2/3 )O 3 –40PbZrO 3 –48PbTiO 3 (12PNS–40PZ–48PT) calcined powders with V 2 O 5 and excess PbO additives has been investigated. Adding 0.20 to 0.40 wt.% V 2 O 5 and 1.0 wt.% excess PbO to 12PNS–40PZ–48PT calcined powders and sintering at 950 °C for 4 h, the sintered samples only contain the perovskite structure. The calcined powders are doped with 3.0 wt.% excess PbO and 0.20 to 1.0 wt.% V 2 O 5 and sintered at 950 °C for 4 h, the coexistence of both tetragonal and rhombohedral phases with the minor phase of pyrochlore is observed. During the calcined powders contain 1.0 wt.% excess PbO and are sintered at 950 to 975 °C for 2 h, the bulk density decreases with V 2 O 5 addition greater than 0.6 wt.%. When the calcined powders with 3.0 wt.% excess PbO are sintered at 900 to 975 °C for 2 h, the bulk density decreases with added V 2 O 5 content increased. The values of the planar coupling coefficient ( K p ) approach the maxima, namely, 0.51 obtained for the compacts containing 0.40 wt.% V 2 O 5 and 1.0 wt.% excess PbO and sintered at 950 °C. As the calcined powders are added with 3.0 wt.% excess PbO and 0.80 wt.% V 2 O 5 and sintered at 975 °C for 2 h, the maximum Q m value 1100 is obtained.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Advanced ceramic materials synthesis · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Atkin, R. B. and Fulrath, R. M., Point defects and sintering lead zirconate titanate. J. Am. Ceram. Soc., 1971, 54, 265–270.10.1111/j.1151-2916.1971.tb12286.x ↗
2. Some aspects of the physics of piezoelectric ceramics10.1080/00150198308225269 ↗
3. Phase transition in solid solution of lead zirconate and lead titanate10.1143/JPSJ.7.5 ↗
4. Phase transition in solid solution of lead zirconate and lead titanate10.1143/JPSJ.7.12 ↗
5. Developments in fabrication of ceramics10.1080/00150198208210611 ↗
6. Piezoelectric properties of lead zirconate-lead titanate solid solution ceramics10.1063/1.1721741 ↗
7. Structural dependence on sintering temperature of lead zirconate-titanate solid solution10.1111/j.1151-2916.1985.tb11519.x ↗
8. Electromechanical properties of lead titanate zirconate ceramics with lead partially replaced by calcium or strontium10.1111/j.1151-2916.1959.tb09141.x ↗
9. Oxygen firing can replace hot-pressing for PZT
10. Electrical, optical and acoustic properties of PLZT ceramics by two-stage processing10.1080/00150197608241977 ↗
11. Fabrication of transparent electrooptic PLZT ceramics by atmosphere sintering10.1111/j.1151-2916.1973.tb12365.x ↗
12. The preparation of transparent PLZT ceramics from oxide powders by liquid-phase sintering
13. Hot-pressed (Pb, La) (Zr, Ti)O3 ferroelectric ceramics for electrooptic applications10.1111/j.1151-2916.1970.tb12105.x-i1 ↗
14. Chemical preparation of PLZT powder from aqueoces solution10.1016/0025-5408(76)90198-7 ↗
15. Intrinsic nonstoichiometry in single-phase Pb(Zr0.5Ti0.5)O3 ceramics10.1111/j.1151-2916.1972.tb11256.x ↗
16. Chemical preparation of PLZT powders from aqueous nitrate solutions
17. The effects of some variations in fabrication procedure on the properties of lead zirconate-lead titanate ceramics made from spary-dried co-precipitated powders
18. Studies in the preparation properties of lead zirconate-lead titanate ceramics
19. Low-temperature sintering of lead-based piezoelectric ceramics10.1111/j.1151-2916.1989.tb06160.x ↗
20. Wang, M. C., Huang, M. S. and Wu, N. C., Effects of 30B2O3–25Bi2O3–45CdO glass addition on the sintering of 12Pb (Ni1/3 Sb2/3)O3–40PbZrO3–48PbTiO3 piezoelectric ceramics. J. Eur. Ceram. Soc., 2001, 21, 695–701.10.1016/S0955-2219(00)00272-7 ↗
21. Low-temperature densification of lead zirconate-titanate with vanadium pentoxide additive10.1111/j.1151-2916.1981.tb09902.x ↗
22. Wu, N. C., Huang, M. S., Wung, J. S. and Wang, M. C., Sintering and piezoelectric properties of Pb(Ni1/3Sb2/3)O3–PBTiO3–PbZrO3 ceramic. J. Mater. Sci. 2002, (in press).
23. Effect of sintering heating rate of the electrical properties of Sr–PZT10.1080/00150198108223506 ↗
24. Methods for measuring piezoelectric, elastic, and dielectric coefficients of crystals and ceramics10.1109/JRPROC.1954.274752 ↗
25. Piezoelectric properties of polycrystalline lead titanate zirconate compositions10.1109/JRPROC.1960.287467 ↗
26. Direct determination of the coexistence region in the solid solution Pb (ZrxTi1−x)O310.1088/0022-3727/8/15/018 ↗
27. On the phenomenon of morphotropic tetragonal–rhombohedral phase boundary in the ferroelectric ceramics10.1143/JJAP.17.637 ↗
28. Behaviour of piezoceramics type Pb(ZrxTi1−x)O3 near the region of morphotropic phase transition
29. German, R. M., Liquid Phase Sintering. Plenum, New York,1985.10.1007/978-1-4899-3599-1 ↗
30. Mechanism of the formation of zirconium-silicon-vanadium and some other ceramic pigments10.1007/BF00677187 ↗
31. Effect of impurity doping in lead zirconate–titanate ceramics10.1080/00150198208210617 ↗
32. Wu, N. C., Hunag M. S. and Wang, M. C., Effect of PbO excess addition on the sintering and piezoelectric properties of 12Pb(Ni1/3Sb2/3)O3–40PbZrO3–48PbTiO3 ceramics. J. Mater. Sci. 2002, (in press).