Synergistic roles of carbon fibres and ZrO2 particles in strengthening and toughening Li–α–sialon composites
Source abstract
Abstract
Abstract Carbon fibre reinforced Li-α-sialon ceramic matrix composites have been fabricated by a process of slurry infiltration followed by hot-pressing. The roles of both carbon fibres and ZrO 2 particles in the strengthening and toughening of Li-α-sialon ceramic matrix composites are discussed. SEM observations show that microcracks in the matrix resulting from the thermal mismatch between the carbon fibres and the matrix can be eliminated by the addition of the ZrO 2 and a considerable amount of fibre pullout was achieved during fracture failure of the composites. Measurement of mechanical properties indicates that a synergistic strengthening and toughening has been achieved with bending strength and fracture toughness of ∼410 MPa and ∼12 MPa m 1/2 respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. High-strength graphite fibre/lithium aluminosilicate composites10.1007/BF02397909 ↗
2. Carbon fibre reinforced ceramic composites10.2978/jsas.2.4_247 ↗
3. Guo J. K., Mao, Z., Bao, C., Wang, T. and Yan, D. S., Carbon fibre reinforced silicon nitride composite. J. Mater. Sci., 1982, 3611-3316.10.1007/BF00752204 ↗
4. Carbon fibre reinforcement of nitrogen glass10.1016/S1359-835X(97)00005-5 ↗
5. Yu, Z. B. and Thompson, D.P., Fabrication and mechanical behaviour of carbon fibre reinforced alpha sialon composites, FRC'98, 15–17 April. In: Proceeding of the Seventh International Conference on Fibre Reinforced Composites, Consolidating New Applications, ed A. G. Gibson. Woodhead Publishing Limited, 1998, pp. 264–270.
6. Richerson · 1992
7. Design principles of multiphase ceramic materials
8. Glass forming regions and thermal expansion of some Ln–Si–Al–O–N glasses (Ln=La, Nd)
9. Preparation of single phase Li–α–sialon ceramics
10. High-strength graphite-fibre/lithium aluminosilicate composites10.1007/BF02397909 ↗
11. Carbon fibre composites with ceramic and glass matrices10.1007/BF00549379 ↗
12. Phase Diagrams for Ceramists, ed. E. M. Levin, E. R. Robbins and H. F. McMurdie. J. Am. Ceram. Soc., 1964.
13. The role of interfaces in fibre-reinforced brittle matrix composites10.1016/0266-3538(91)90010-M ↗
14. Kingery · 1976
15. Chawla, K. K., Ceramic Matrix Composites. Chapman & Hall, 1993.10.1007/978-1-4757-2216-1 ↗
16. Theoretical analysis of the fibre pullout and push out test10.1111/j.1151-2916.1991.tb07144.x ↗
17. Nitride-stabilized cubic zirconia10.1111/j.1151-2916.1978.tb09333.x ↗
18. Compressive surface stresses developed in ceramics by an oxidation induced phase change10.1111/j.1151-2916.1980.tb10645.x ↗
19. Nitrogen containing tetragonal zirconia10.1111/j.1151-2916.1991.tb04355.x ↗
20. Nitridation of zirconia10.1111/j.1151-2916.1996.tb09028.x ↗