Degradation of mechanical and electrical properties after long-term oxidation and corrosion of non-oxide structural ceramic composites
Source abstract
Abstract
This work summarizes the results related to the influence of the starting composition and of microstructure on properties degradation, due to oxidation and corrosion, relatively to the following structural ceramics: Si3 N4 TiN, Si3 N4 MoSi2, AlN SiC MoSi2, AlN SiC.The effects of: (i) long-term oxidation in air (100 h), in the temperature range 6001500 °C and (ii) of long-term corrosion (400 h) in acid or basic aqueous solution at RT, 40 and 70 °C, on the electrical resistivity and mechanical strength of the composites are analysed and compared. The degradation of the properties are related to the characteristics of the surface and sub-surface damage after oxidation and corrosion treatments.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Review-particulate silicon nitride composite10.1007/BF00356803 ↗
2. Microstructure, chemical aspects and mechanical properties of TiB2/Si3N4 and TiN/Si3N4 composites10.1557/JMR.1994.2349 ↗
3. Microstructure, fracture behaviour and mechanical properties of TiN/Si3N4 composites10.1016/0254-0584(95)01725-9 ↗
4. Development and characterization of electroconductive Si3N4–TiN composites10.1016/0955-2219(92)90049-J ↗
5. Microstructure and properties of Si3N4–MoSi2 composite
6. High-temperature resistant composite in the AlNSiCMoSi2 system10.1111/j.1151-2916.2003.tb03546.x ↗
7. Fabrication and microstructure of MoSi2-reinforced Si3N410.1111/j.1151-2916.1997.tb02953.x ↗
8. Investigation of SiCAlN: Part II. Mechanical properties10.1111/j.1151-2916.1996.tb08582.x ↗
9. Properties of silicon nitride–molybdenum disilicide particulate ceramic composites10.1111/j.1151-2916.1993.tb04030.x ↗
10. Microstructure–property relations of hot pressed silicon carbide–aluminum nitride compositions at room and elevated temperatures10.1111/j.1151-2916.1999.tb02107.x ↗
11. Hot pressed MoSi2-particulate reinforced α-SiAlON composites10.1111/j.1151-2916.1995.tb08249.x ↗
12. Effects of TiN particle size on mechanical properties of Si3N4TiN particulate composites10.2109/jcersj.100.617 ↗
13. Sintering behaviour and microstructure development in electroconductive Si3N4TiN composites
14. Optimization of mechanical and electrical properties of TiN/Si3N4 material by agglomerates-microstructure control10.2109/jcersj.106.75 ↗
15. Densification, microstructure and properties of electroconductive Si3N4TaN Composites. Part I: Densification and microstructure10.1016/S0955-2219(00)00198-9 ↗
16. Densification, microstructure and properties of electroconductive Si3N4TaN Composites. Part II: Electrical and mechanical properties10.1016/S0955-2219(00)00199-0 ↗
17. Densification, microstructure and properties of Si3N4TiCN composites10.1016/0955-2219(93)90104-Y ↗
18. Influence of additive content on the high temperature oxidation of silicon nitride-based composites10.1016/S0955-2219(02)00376-X ↗
19. Effects of metallic boride dispersion on fracture toughness and oxidation resistance in SiC ceramics10.2109/jcersj.100.991 ↗
20. Factors inducing degradation of properties after long term oxidation of Si3N4TiN composites10.1016/S0169-4332(02)00498-1 ↗
21. Effect of thermal treatments on properties of a Si3N4TiN composite10.1016/S0921-5093(03)00501-X ↗
22. Influence of long term oxidation on microstructure and properties of AlNSiCMoSi2 composite10.1016/S0955-2219(03)00095-5 ↗
23. Surface modifications and oxidation kinetics of hot-pressed AlNSiCMoSi2 electroconductive ceramic composite10.1016/S0169-4332(03)00155-7 ↗
24. Sciti, D., Winterhalter, F. and Bellosi, A., Oxidation behaviour of a pressureless sintered AlNSiC composite, J. Mater. Sci., 2004, 39 6965–6973.10.1023/B:JMSC.0000047539.40056.1a ↗
25. Factors inducing degradation of properties after long term oxidation of Si3N4MoSi2 electroconductive composites10.1557/JMR.2004.0210 ↗
26. High temperature oxidation and pesting of Mo(Si,Al)210.1016/S0921-5093(97)00673-4 ↗
27. Long-term stability of nonoxide ceramics in an oxidative environment at 1500°C10.1016/S0955-2219(02)00267-4 ↗
28. Silicon nitride/molybdenum disilicide composite with superior long-term oxidation resistance at 1500°C10.1111/j.1151-2916.2001.tb01027.x ↗
29. Influence of molybdenum silicide additions on high-temperature oxidation resistance of silicon nitride materials10.1111/j.1151-2916.1996.tb08993.x ↗
30. Corrosion of Si3N4MoSi2 ceramic composite in acid and basic aqueous environments: surface modifications and properties degradation10.1016/j.apsusc.2003.09.048 ↗
31. Corrosion of electroconductuiveAlNSiCMoSi2 ceramic composite in sodium hydroxide aqueous solution10.5006/1.3277605 ↗
32. Corrosion of hot pressed Si3N4TiN composite in sulphuric acid aqueous solutions10.1016/S0010-938X(03)00077-5 ↗
33. Investigation of SiCAlN system: Part I. Microstructure and solid solution10.1557/JMR.1995.0651 ↗
34. Investigation of phase stability in the system SiCAlN10.1111/j.1151-2916.1983.tb15713.x ↗
35. Hot isostatically pressed SiCAlN powder mixtures: effect of milling on solid solution formation and related properties10.1111/j.1151-2916.1998.tb02502.x ↗
36. Preparation and mechanical properties of SiCAlN ceramic alloy10.1007/BF00612422 ↗