Crystal growth of a new aluminum sodium boride NaAlB14 and some properties
Source abstract
Abstract
Abstract Single crystals of a new ternary boride NaAlB14 were obtained from the Na-Al-B system using a high-temperature Al self-flux under an Ar atmosphere. The reagents used to prepare the samples were Na2B4O7 powder, crystalline boron powder and Al metal chips. The optimum conditions to obtained relatively large crystals were found to include soaking temperature 1573 K, soaking time 1 h, cooling rate 50 K/h and the atomic ratios (n = B/Na = 1.0–4.0) of starting materials. The NaAlB14 crystal prepared had maximum sizes of approximately 7.3 mm × 3.3 mm × 2.8 mm. The crystals were generally obtained in the form of plate-like crystals with well-developed {0 1 0} faces or trapezoidal-shape crystals enclosed by {1 0 0}, {0 1 0}, {0 1 1} and {0 0 1} faces, and were reddish black with a metallic luster. The values of Vickers microhardness are in the ranges of 23.3 ± 1.0 and 28.4 ± 0.6 GPa for {1 0 0} and {0 1 0} faces, respectively. The susceptibility does not show any particular features, but an increase at low temperatures is indicative of a paramagnetic contribution.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Rare-earth and actinide compounds · Superconductivity in MgB2 and Alloys · Inorganic Chemistry and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. 1977 · 439
2. 1995 · 4
3. Floating zone crystal growth and structure analysis of a novel ScB19 family compound, ScB19+XSiY10.1006/jssc.2002.9524 ↗
4. Growth and some properties of Sc2AlB6 crystal obtained from the solution in aluminum melt10.1016/j.jssc.2003.01.002 ↗
5. Hardness and oxidation resistance of perovskite-type borocarbide system YRh3BxC1−X (0 ≦X≦1)10.1016/S0925-8388(03)00011-2 ↗
6. Synthesis and magnetic properties of binary boride REB25 compounds10.1088/0953-8984/13/20/105 ↗
7. Crystal growth and some properties of REMn2Si2 (RE=Er, Tm, Yb, Lu)10.1016/S0022-0248(02)01689-5 ↗
8. Crystal structure of α-AlB1210.1016/0022-4596(77)90052-4 ↗
9. Crystal chemistry of some boron-rich phases10.1016/0022-5088(76)90066-7 ↗
10. Crystal growth and properties of AlLiB1410.1143/JJAP.41.L928 ↗
11. Boron-rich crystals in Al-M-B (M=Li, Be, Mg) systems grown from high-temperature aluminum solutions10.1016/S0022-0248(07)80108-4 ↗
12. Refinement of the structure of MgAlB1410.1016/0022-5088(83)90490-3 ↗
13. Crystal growth of aluminium magnesium borides from Al-Mg-B ternary system solutions and properties of the crystals
14. Spin glass behavior in rhombohedral B12C luster compounds