Optimization of ball milling process for fabrication of α-Al2O3 based coatings via laser-assisted combustion synthesis
Source abstract
Abstract
Abstract In this study, the Al 2 O 3 coatings were prepared by using laser-assisted combustion synthesis method with Al-TiO 2 -C powder mixture. α-Al 2 O 3 , a more desired thermally stable phase of Al 2 O 3 , has been achieved in a single step without any post-coating treatments. The obtained coating showed a uniform and dense morphology with a thickness of 150 μm and well adhered to the substrate. The absence of porosity and crack in the coating was attributed to the high energy in the fabrication process from both the high power laser and the combustion reaction. The effect of ball milling condition, specifically ball milling time ( T b ), on morphology, microstructure evolution and physical properties of the α-Al 2 O 3 based coatings were studied. It was concluded that 2 h ball milling process followed by laser-assisted combustion synthesis is sufficient to prepare an α-Al 2 O 3 based coating with fine structures, which can be expected to be widely used as protective coatings.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced ceramic materials synthesis · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Thermal barrier coatings for gas-turbine engine applications10.1126/science.1068609 ↗
2. Microstructure and sliding wear resistance of an Al-12wt.% Si/TiC laser clad coating10.1016/j.wear.2012.01.022 ↗
3. Composite Ni/Al2O3 coatings and their corrosion resistance10.1016/j.electacta.2005.01.040 ↗
4. The relationship between structure and dielectric properties in plasma-sprayed alumina coatings10.1016/0257-8972(88)90042-4 ↗
5. Relationship between particle erosion and lamellar microstructure for plasma-sprayed alumina coatings10.1016/j.wear.2005.07.006 ↗
6. Preliminary study of HDA coating on CLAM steel followed by high temperature oxidation10.1016/j.jnucmat.2013.03.011 ↗
7. Investigation on the suitability of plasma sprayed Fe-Cr-Al coatings as tritium permeation barrier10.1016/S0022-3115(99)00059-8 ↗
8. Development of tritium permeation barriers on Al base in Europe10.1016/S0022-3115(98)00792-2 ↗
9. Dependence of the stabilization of α-alumina on the spray process10.1007/s11666-007-9107-7 ↗
10. On the formation of thermally sprayed alumina coatings10.1007/BF00550387 ↗
11. Synthesis and cladding of Ni3Al intermetallic on steel substrate by laser controlled reactive synthesis10.1016/j.jmatprotec.2005.07.009 ↗
12. Synthesis and cladding of Al2O3 ceramic coatings on steel substrates by a laser controlled thermite reaction10.1016/S0257-8972(03)00255-X ↗
13. Effect of h-BN addition on the properties of nanostructured Al2O3-TiB2-TiN based coatings developed by combined SHS and laser surface alloying10.1016/j.surfcoat.2009.10.047 ↗
14. Study on the effect of laser post-treatment on the properties of nanostructured Al2O3-TiB2-TiN based coatings developed by combined SHS and laser surface alloying10.1016/j.surfcoat.2010.06.015 ↗
15. Facile fabrication and microstructure of a-Al2O3/TiC composite coating as tritium permeation barrier10.1111/ijac.12398 ↗
16. Mechanochemically synthesized Al2O3-TiC nanocomposite10.1016/j.jallcom.2009.10.206 ↗
17. Thermal cycling behavior of plasma-sprayed thermal barrier coatings with various MCrAIX bond coats10.1361/105996300770350041 ↗
18. Post-deposition treatment of zirconia thermal barrier coatings using sol–gel alumina10.1361/105996399770350458 ↗
19. Thermal cycling behavior of plasma sprayed segmented thermal barrier coatings10.2320/matertrans.47.306 ↗
20. Atmospheric plasma sprayed thick thermal barrier coatings with high segmentation crack density10.1016/j.surfcoat.2004.01.002 ↗
21. Atmospheric plasma sprayed thermal barrier coatings with high segmentation crack densities: spraying process, microstructure and thermal cycling behavior10.1016/j.surfcoat.2011.06.032 ↗