Mullite/Mo interfaces formed by intrusion bonding
Source abstract
Abstract
The microstructure and strength of Mo/mullite interfaces formed by diffusion bonding at 1650 C has been analyzed. Interfacial metal-ceramic interlocking contributes to flexural strength of approx. 140 MPa as measured by 3 point bending. Saturation of mullite with MoO2 does not affect the interfacial strength.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Structure and composition of metal/ceramic interfaces10.4028/www.scientific.net/KEM.116-117.1 ↗
2. Electron microscopy studies of defects at diffusion-bonded Nb/Al2O3 interfaces10.1016/0001-6160(89)90012-6 ↗
3. Some aspects of the mechanical strength of ceramic/metal bonded systems10.1016/0001-6160(86)90110-0 ↗
4. Mullite/molybdenum ceramic–metal composites10.1016/S1359-6454(99)00220-7 ↗
5. Wetting and work of adhesion in oxide/metal systems
6. Chemical reactions and adherence at glass/metal interfaces: and analysis10.1016/S0109-5641(86)80063-X ↗
7. Mullite for structural, electronic, and optical applications10.1111/j.1151-2916.1991.tb06768.x ↗
8. High-temperature compressive creep of polycrystalline mullite10.1111/j.1151-2916.1991.tb06787.x ↗
9. Suitability of mullite for high temperature applications10.1016/S0955-2219(99)00116-8 ↗
10. Outokumpu · 1993
11. Baker · 1979
12. Grain boundary segregation and intergranular fracture in molybdenum10.1098/rspa.1980.0043 ↗
13. Srivastava, S. C. and Seigle, L. L. Solid solubility of oxygen in molybdenum. In 5th Spring Meeting of the Metallurgical Society of AIME. Metallurgical Soc. AIME, 1973, pp. 124–125.10.1007/BF02642925 ↗
14. Evolution of the nickel/zirconia interface10.1002/9780470312568.ch6 ↗
15. Effects of composite processing on the strength of sapphire fiber-reinforced composites10.1016/0956-7151(95)90281-3 ↗