journal article·2009-05

Fabrication of green and sintered bodies prepared by centrifugal compaction process using wet-jet milled slurries

Katsuya Sato, Yuji Hotta, Huseyin Yilmaz, Koji Watari

Publisher page

Abstract

Properties of green and sintered bodies prepared by high-speed centrifugal compaction process (HCP) using wet-jet milled slurries were investigated. At 30 vol.% solids loading, the relative packing density of compacted body prepared from wet-jet milled slurry was 67%. On the other hand, the density of compacted body prepared from ball-milled slurry was 56% at the same loadings. The difference in relative densities of the top and bottom of green bodies prepared from wet-jet milled slurry was decreased to one-third of the ones prepared from ball-milled slurry. Moreover, the linear shrinkage of the sintered bodies prepared from wet-jet milled slurries was almost constant at sintering temperatures above 1400 °C; it was found to be increasing for bodies prepared from ball-milled slurries with increasing sintering temperature. Furthermore, activation energy for grain-growth was estimated. The grain-growth of green bodies prepared from wet-jet milled slurries was promoted at lower-sintering temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Powder Metallurgy Techniques and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Agglomerates and particle size effects on sintering yttria-stabilized zirconia10.1111/j.1151-2916.1981.tb09552.x ↗
2. Powder processing science and technology for increased reliability10.1111/j.1151-2916.1989.tb05945.x ↗
3. Microstructure control though colloidal consolidation
4. Processing monosized powders
5. Pressure slip casting of submicron alumina powder10.2497/jjspm.40.3 ↗
6. Mechanical properties and microstructure of centrifugally compacted alumina and hot-isostatically pressed alumina10.1016/S0921-5093(96)10439-1 ↗
7. Cutting performance of high purity alumina ceramic tools formed by a high-speed centrifugal compaction process10.1016/S0924-0136(96)02448-X ↗
8. Dependence of mechanical properties on sintered microstructure of high purity alumina made by high-speed centrifugal compaction process10.2497/jjspm.46.331 ↗
9. Effect of slip condition kinetics of high-speed centrifugal compaction process
10. Adding a second element to high-speed centrifugal compaction process (HCP) alumina green compacts by immersion in nitrate solutions
11. Effect of powder characteristics on sintering behavior and mechanical properties of alumina compacted by high-speed centrifugal compaction process10.2497/jjspm.47.866 ↗
12. Observation of alumina green compacts made by high-speed centrifugal compaction process casting using liquid immersion technique10.2497/jjspm.47.874 ↗
13. Centrifugal consolidation of Al2O3 and Al2O3/ZrO2 composite slurries vs. interparticle potentials: particle packing and mass segregation10.1111/j.1151-2916.1991.tb08284.x ↗
14. Compacting mechanism in high-speed centrifugal compaction process (Part I)10.2109/jcersj.109.1266_137 ↗
15. Compacting mechanism in high-speed centrifugal compaction process (Part II)10.2109/jcersj.109.1267_248 ↗
16. Preparation of Al2O3 and Al2O3–ZrO2 ceramic foams with adjustable cell structure by centrifugal slip casting10.1016/j.msea.2007.04.100 ↗
17. Sintering of wet-milled centrifugal cast alumina10.1016/0955-2219(94)90029-9 ↗
18. Alumina of high reliability by centrifugal casting10.1016/0955-2219(95)00053-W ↗
19. Effect of grinding synthesis of MgAl2O4 spinel from a powder mixture of Mg(OH)2 and Al(OH)310.1016/S0032-5910(00)00208-4 ↗
20. Influence of milling conditions on magnetic properties of Nd(Fe, Mo)12Nx compounds10.1016/S0304-8853(98)00334-5 ↗
21. Onodera, T., Kannari, C., Koyano, A., Furukawa, Y., Mitake, K., Yasuda, F., Miyake, F. and Fujishima, F., Fine particle producing devices for reducing materials to tiny particles—the device can exhibit stable particle size reducing performance for an extended period of time by reducing the abrasion of flow guiding blocks, Kokai-Tokkyo-Koho, 1998, JP10180068-A.
22. Wet jet milling of Al2O3 slurries10.1016/j.jeurceramsoc.2006.04.001 ↗
23. Slip casting using wet-jet milled slurry10.1016/j.jeurceramsoc.2006.04.004 ↗
24. State of the dispersant and particle surface during wet-jet milling for preparation of a stable slurry10.1111/j.1551-2916.2008.02310.x ↗
25. The settling of particles through Newtonian and non-Newtonian media10.1016/0021-9797(82)90237-5 ↗
26. Densification and grain growth in BaTiO3 ceramics fabricated from nanopowders synthesized by ball-milling assisted hydrothermal reaction10.1016/j.jeurceramsoc.2007.07.007 ↗