Creep of monolithic and fibre-reinforced silicon carbide
Source abstract
Abstract
Abstract The mechanisms governing tensile creep and creep fracture are identified for siliconized silicon carbide (Si–SiC) and sintered silicon carbide (SSC), as well as for various SiC-matrix composites reinforced with interwoven bundles of different fibres. With Si–SiC and SSC, creep is controlled by the rate at which intergranular damage development allows grain boundary sliding. Fracture then results from the formation and link up of grain boundary cavities and cracks, unless premature failure occurs by rapid crack propagation from a pre-existing flaw. In contrast, with the woven SiC-matrix composites, immediate failure was never encountered on loading at stresses less than the UTS, despite the presence of macroscopic pores. Instead, the longitudinal fibres control the rates of creep strain accumulation and crack growth. However, the fracture properties are determined by oxidation-assisted fibre failure, because matrix cracking permits oxygen ingress during tests in air. By clarifying the processes limiting the creep capabilities of current product ranges, possible development avenues are suggested for fibre-reinforced composites displaying improved long-term service performance in oxidizing atmospheres.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. Ruffles · 1995
2. Advanced materials means advanced engines10.1179/isr.1996.21.2.117 ↗
3. Perspectives on the development of high-toughness ceramics10.1111/j.1151-2916.1990.tb06493.x ↗
4. Oxidation embrittlement probe for ceramic-matrix composites10.1111/j.1151-2916.1995.tb08621.x ↗
5. High temperature corrosion and crack growth of SiC–SiC at variable oxygen partial pressures10.1016/0921-5093(95)80064-2 ↗
6. Tensile creep and creep fracture of a fibre-reinforced SiC–SiC composite10.1016/S1359-6462(98)00181-X ↗
7. Tensile and creep strengths of hot-pressed Si3N410.1007/BF00823215 ↗
8. Deformation and fracture processes during creep of reaction bonded and hot pressed silicon nitride
9. Damage enhanced creep in siliconized silicon carbide: phenomenology10.1111/j.1151-2916.1988.tb05926.x ↗
10. Deformation and failure processes during tensile creep of sintered silicon carbide
11. Non-oxide ceramics, creep and creep rupture of silicon nitrides and silicon carbides
12. Fracture of silicon nitride and silicon carbide at elevated temperatures10.1016/0921-5093(94)90958-X ↗
13. Norton · 1929
14. Structural ceramics10.1016/0079-6425(76)90001-3 ↗
15. A review of creep in silicon nitride and silicon carbide
16. Theories of creep in ceramics10.1080/10408439608241255 ↗
17. 1999 · 391
18. Creep of dispersion strengthened materials: a critical assessment
19. Evans · 1985
20. The θ approach to creep of structural ceramics
21. The influence of stress distribution on the deformation and fracture behaviour of ceramic materials under compressive creep conditions10.1007/BF00708259 ↗
22. Some aspects of the high temperature performance of ceramics and ceramic composites
23. Constitutive equations for creep rupture10.1016/0001-6160(77)90135-3 ↗
24. Creep damage resistance of ceramic-matrix composites10.1016/j.jeurceramsoc.2007.03.029 ↗
25. Creep property comparisons for ceramic–fibre-reinforced ceramic-matrix composites10.1016/S0955-2219(01)00452-6 ↗
26. Creep and fatigue behaviour of SiC fibre reinforced SiC composite at high temperatures10.1016/S0921-5093(96)10872-8 ↗
27. Creep and fatigue behaviour of an enhanced SiC–SiC composite at high temperatures10.1111/j.1151-2916.1998.tb02621.x ↗
28. Creep and fatigue behaviour in Hi-Nicalon Trade Mark-fibre-reinforced silicon carbide composites at high temperatures10.1111/j.1151-2916.1999.tb01731.x ↗
29. Deformation and damage processes during tensile creep of ceramic–fibre-reinforced ceramic-matrix composites10.1016/S0955-2219(99)00175-2 ↗
30. Tensile creep behaviour of a silicon-carbide-based fibre with a low oxygen content10.1007/BF00356326 ↗
31. Correlation between microstructure and mechanical behaviour at high temperatures of a SiC fibre with a low oxygen content (Hi-Nicalon)10.1023/A:1018515430675 ↗
32. Oxidation kinetics of enhanced SiC–SiC10.1002/9780470314784.ch30 ↗
33. Creep behaviour and structural characterization at high temperature of Nicalon Trade Mark SiC fibres10.1007/BF02396938 ↗
34. Creep damage in SiC/SiC composites10.1016/0921-5093(95)09867-4 ↗
35. Elevated temperature creep and cyclic creep behaviour of fibre-reinforced ceramics
36. Damage of a 2D Al2O3–SiC composite during uniaxial creep10.1016/0266-3538(96)00027-9 ↗
37. State of the art and perspectives for oxide–oxide composites
38. Origin and effect of fibre attack for the processing of C/SiC
39. Applications of CMCs made via the liquid silicon infiltration (LSI) technique
40. Influence of high temperature argon heat treatment on tensile properties of four types of BN/SiC-coated SiC fiber preforms
41. Understanding the creep behaviour of a 2.5D Cf–SiC composite. I. Morphology and microstructure of the as-received material10.1016/S0921-5093(99)00626-7 ↗
42. Understanding the creep behaviour of a 2.5D Cf–SiC composite. II. Experimental specification and macroscopic mechanical creep responses10.1016/S0921-5093(00)00922-9 ↗
43. Deformation processes during high-temperature creep of lime, magnesia and doloma10.1016/0390-5519(77)90005-9 ↗
44. The influence of variations in composition on the creep behaviour of doloma10.1016/0390-5519(78)90121-7 ↗