journal article·2015-07

Effect of the addition of alkaline earth sulfates to mullite ceramics on the corrosion and wetting by Al–Mg alloy

M.N. Ibarra, J.M. Almanza, D.A. Cortés, J.C. Escobedo, M. Pech, R. Martinez

Publisher page

Abstract

Abstract Novel ceramics showing a high corrosion resistance were obtained by adding alkaline earth sulfates to mullite (Al 6 Si 2 O 13 ). Powder samples of mullite, mullite–SrSO 4 and mullite–BaSO 4 were prepared. Disk pellets of 4 cm in diameter were conformed by uniaxial pressing at 78 MPa and sintered at 1450 °C for 6 h. Wetting experiments were carried out by the sessile drop test at 900 °C using an Al–7Mg alloy. After sintering, substrates of mullite, mullite–SrAl 2 Si 2 O 8 or mullite–BaAl 2 Si 2 O 8 were obtained. The contact angles between samples surface of alkaline earth sulfates containing mullite and molten alloy were higher than that corresponding to pure mullite, showing a non-wetting behavior. Cross-section analysis by SEM and EDS of samples after the wetting test showed that the corrosion products were spinel (MgAl 2 O 4 ) and periclase (MgO). The BaAl 2 Si 2 O 8 -containing samples showed a higher corrosion resistance.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Influence of non-wetting agents on the modification of dynamic wetting of high alumina monolitics refractories by aluminum alloy
2. Kinetics of metal–ceramic composite by reactive penetration of silicates with molten aluminum10.1111/j.1151-2916.1998.tb02634.x ↗
3. Subrata Banerjee · 1998
4. Effect of Cr2O3 on composites and properties of mullite–spinel composites10.1179/096797803225004936 ↗
5. Additives and the corrosion resistance of aluminosilicate refractories in molten Al–5Mg10.1007/s11837-998-0245-2 ↗
6. Totten · 2003 · vol. 1
7. The reactive liquid processing of ceramic–metal composites10.1007/BF02914716 ↗
8. Wetting in nonreactive liquid metal-oxides systems10.1007/BF02914715 ↗
9. Ceramic–metal interfaces and the spreading of reactive liquids10.1007/s11837-999-0209-1 ↗
10. Reactive wetting of liquid metals on ceramic substrates10.1016/1359-6454(95)00235-9 ↗
11. The corrosion of refractory aggregates by molten aluminum10.1007/s11837-000-0034-z ↗
12. Role of ceria in enhancing the resistance of aluminosilicate refractories to attack by molten aluminum alloy10.1111/j.1151-2916.1989.tb06241.x ↗
13. Furnaces improving low cement castables by non-wetting additives10.1007/s11837-001-0130-8 ↗
14. Refractories for molten aluminum contact Part I: Thermodynamics and kinetics
15. Additive effects on the physical properties of castable systems for aluminum contact applications, refractories for the next millennium
16. New refractories for aluminum melting furnaces
17. Effect of CaF2 on interfacial phenomena of high alumina refractories with Al alloy10.1007/s11663-008-9169-z ↗
18. Effects of different calcium compounds on the corrosion resistance of andalusite-based low-cement castables in contact with molten Al-alloy10.1007/s11663-010-9468-z ↗
19. Effects of AlPO4 addition on the corrosion resistance of andalusite-based low-cement castables with molten Al-alloy10.1016/j.jeurceramsoc.2012.11.005 ↗
20. Effects of V2O5 addition on the corrosion resistance of andalusite-based low-cement castables in contact with molten Al-alloy10.1016/j.jeurceramsoc.2012.01.023 ↗
21. Effects of different boron compounds on the corrosion resistance of andalusite-based low-cement castables in contact with molten Al alloy10.1007/s11663-011-9619-x ↗
22. Effects of different barium compounds on the corrosion resistance of andalusite-based low-cement castables in contact with molten Al-alloy10.1007/s11663-011-9522-5 ↗
23. Aluminum–alumina interface morphology and thermodynamics from dewetting experiments10.1016/S1359-6454(03)00084-3 ↗
24. Effect of magnesium addition on the wetting of alumina by aluminum10.1016/j.apsusc.2009.05.044 ↗
25. Synthesis of Al6Si2O13–BaAl2Si2O8–ZrO2-based composites and their wettability by molten Al and an Al–Si alloy
26. Preparation of reactive Sr-celsian powders by solid-state reaction and their sintering10.1016/S0955-2219(03)00215-2 ↗
27. The influence of BaO additives on the reaction of Al2O3–SiO2 ceramics with molten Al and Al–Si alloys10.1016/S1359-6454(01)00449-9 ↗
28. Interfacial phenomena in wettability of TiC by Al–Mg alloys10.1016/j.actamat.2003.10.034 ↗
29. Transmission electron microscopy study of interfacial microstructure formed by reacting Al–Mg alloy with mullite at high temperature10.1016/S1359-6454(99)00176-7 ↗
30. Estudio Cinético de la Eliminación de Magnesio en las Aleaciones de Aluminio Mediante la Inyección de Polvos de Sílice