Densification and properties of superhard B6O materials with cobalt additions
Source abstract
Abstract
Abstract The search for suitable additives for boron suboxide (B6O) materials which could improve densification, reduce sintering temperature and tailor the microstructure has been productive. B6O materials doped with 0–5 vol% cobalt addition were sintered at temperatures up to 1850 °C and pressure of 50 MPa for 20 min. Relationships between the formed phases, microstructures and mechanical properties of the sintered materials were investigated as a function of sintering conditions and added cobalt content. The hardness of the sintered B6O materials increases with sintering temperature, while the fracture toughness increases with increasing cobalt content and reduces with increasing sintering temperature.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Boron and Carbon Nanomaterials Research · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. High-pressure high-temperature synthesis and characterization of boron suboxide (B6O)10.1021/cm970433+ ↗
2. Microstructure and mechanical properties of B6O–B4C sintered composites prepared under high pressure10.1023/A:1004753116816 ↗
3. B6O–cBN composites prepared by high pressure sintering10.1111/j.1151-2916.2000.tb01224.x ↗
4. High pressure consolidation of B6O–diamond mixtures10.1023/A:1012499214307 ↗
5. Hard and tough boron suboxide based composite10.1016/j.ceramint.2007.05.010 ↗
6. Ellison-Hayashi C, Zandi M, Csillag FJ, Kuo S-Y. Boron suboxide material and method for its preparation. United State Patent – US 5135892; 1992.
7. An investigation of the physicomechanical properties of B6O and SiB410.1016/0022-5088(79)90028-6 ↗
8. Hot pressing of various boron phases10.1016/0022-5088(86)90003-2 ↗
9. Mechanical properties of hot-pressed boron suboxide and boron
10. Goosey BF. Method of fabricating boron suboxide articles. United State Patent – US 3816586; 1974.
11. Liquid phase assisted hot pressing of boron suboxide materials10.1016/j.jeurceramsoc.2007.10.011 ↗
12. B6O: a correlation between mechanical properties and microstructure evolution upon Al2O3 addition during hot-pressing10.1111/j.1551-2916.2007.02167.x ↗
13. Andrews A. Development of boron suboxide composites with improved toughness. PhD thesis, University of the Witwatersrand; 2008.
14. Liquid phase assisted densification of superhard B6O materials10.1016/j.jeurceramsoc.2009.03.002 ↗
15. Field-assisted densification of superhard B6O materials with Y2O3/Al2O3 addition10.1111/j.1551-2916.2009.03197.x ↗
16. Boron suboxide materials with Co sintering additives10.1016/j.ceramint.2010.02.035 ↗
17. Microstructure and interfacial reactions between B6O and (Ni, Co) couples10.1016/j.ceramint.2010.07.018 ↗
18. A critical evaluation indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
19. Shabalala TC. The preparation and characterization of boron suboxide (B6O) based composites. PhD thesis, University of the Witwaterstand; 2007.
20. Synthesis of aluminium infiltrated boron suboxide drag cutters and drill bits10.1023/A:1004649325328 ↗
21. High pressure sintering of B6O powder and properties of the sintered compact10.2472/jsms.47.1000 ↗
22. Prediction of new superhard boron-rich compounds10.1021/jp052547b ↗
23. Binary alloy phase diagrams. Ac–Au to Fe–Rh
24. Holcombe CE, Ottis JH. Method for preparing boron suboxide. United State Patent – US 3 660 031; 1972.
25. Bush PR. On the toughening mechanisms present in boron suboxide materials with sintering aids. MSc dissertation. University of Witwatersrand; 2011.
26. Kosolapova T, Svoistva J. Poluschenie i primenenie tugoplavkich soedinenii. Metallurgija, Moscow; 1986.