Abstract

Abstract A SiC particulate-reinforced Si–C–N ceramic composite was fabricated using the precursor impregnation and pyrolysis method, and its thermal and mechanical properties were analyzed. The weight loss of the composite was 5% after a heating at 2100 °C in Ar. The pores of the composite enlarged at and above 1700 °C in Ar due to the decomposition of the Si–C–N matrix. However, the composite retained mechanical properties such as strength and hardness after heating at 1700 °C. 88% of the original strength was remained after heating at 2000 °C for 10 h although the fabrication temperature was 1350 °C. The weight gain of the composite was 3.2% after an oxidation at 1450 °C for 30 min in air. The inner oxidation of the particulate-reinforced composites (PRC) was suppressed above 1400 °C due to the closure of the open pores by SiO2. Consequently, the composite possessed excellent creep resistance at 1400 °C in air. The SiC/Si–C–N composite is a challenging candidate for the application at high temperature.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Novel high-performance ceramics—amorphous inorganic networks from molecular precursors10.1002/anie.199703281 ↗
2. Boron-modified polysilylcarbodi-imides as precursors for Si–B–C–N ceramics: synthesis, plastic-forming and high-temperature behavior10.1002/(SICI)1099-0739(199810/11)12:10/11<725::AID-AOC777>3.0.CO;2-2 ↗
3. Polymer-derived ceramic coatings on C/C–SiC composites10.1016/0955-2219(96)00025-8 ↗
4. Boron-modified polysilazane as a novel single-source precursor for SiBCN ceramic fibers: synthesis, melt-spinning, curing and ceramic conversion10.1039/b408295h ↗
5. Fabrication of fiber-reinforced ceramic composites by the modified slurry infiltration technique10.1111/j.1551-2916.2007.01795.x ↗
6. Processing of damage-tolerant, oxidation-resistant ceramic-matrix composites by a precursor infiltration and pyrolysis method10.1016/0921-5093(94)06513-6 ↗
7. Processing and properties of C/Si–B–C–N fiber-reinforced ceramic matrix composites prepared by precursor impregnation and pyrolysis10.1016/j.actamat.2007.12.001 ↗
8. Active-filler-controlled pyrolysis of preceramic polymers10.1111/j.1151-2916.1995.tb08404.x ↗
9. Phase equilibria of precursor-derived Si-(B-)C-N ceramics10.1002/aoc.238 ↗
10. Particulate-reinforced precursor-derived Si–C–N ceramics: optimization of pyrolysis atmosphere and schedules10.1111/j.1551-2916.2005.00587.x ↗
11. Calculation of heterogeneous phase-equilibria in oxide-nitride systems. 1. The quaternary system C–Si–N–O10.1016/0364-5916(81)90039-0 ↗
12. Lee, S. H. and Aldinger, F., Processing and thermal stability of a Cfiber/SiCfiller/Si–C–Nmatrix composite—effect of oligomer vaporization and the surface oxide layer of SiC filler. J. Mater. Sci., in press.
13. Effects of powder bed conditions on the liquid-phase sintering of Si3N410.1557/JMR.2002.0065 ↗
14. The ball on three balls test for strength testing of brittle discs: stress distribution in the disc10.1016/S0955-2219(01)00458-7 ↗
15. Gas permeability behavior of mullite-bonded porous silicon carbide ceramics10.1007/s10853-007-1577-y ↗
16. Ordered mesoporous SiOC and SiCN ceramics from atmosphere-assisted in situ transformation10.1021/cm070283v ↗
17. Synthesis of a polycyclic silazane network and its evolution to silicon carbonitride glass10.1016/S0022-3093(02)01007-4 ↗
18. Formation kinetics of crystalline Si3N4/SiC composites from amorphous Si–C–N ceramics10.1016/j.jnoncrysol.2004.04.021 ↗
19. Silicon carbonitride derived from an organometallic precursor: influence of the microstructure on the oxidation behaviour10.1016/0272-8842(92)90055-I ↗
20. A silicoboron carbonitride ceramic stable to 2000°C10.1038/382796a0 ↗
21. Oxidation kinetics of an amorphous silicon carbonitride ceramic10.1111/j.1151-2916.2001.tb00918.x ↗
22. Microstructural dependence of mechanical behavior of ceramics
23. Strength variability of indented soda-lime glass10.1111/j.1151-2916.1987.tb05665.x ↗
24. Influence of crystallinity of matrix on mechanical properties of fiber-reinforced composites prepared by polysilazanes as matrix precursor10.2109/jcersj.110.775 ↗
25. Synthesis, microstructure and properties of Si–C–N ceramics prepared from tailored polymers10.1016/S0254-0584(99)00114-5 ↗
26. Compression creep behaviour of precursor-derived Si–C–N ceramics10.1016/S0955-2219(99)00093-X ↗