Wet chemical porosification of LTCC in phosphoric acid: Celsian forming tapes
Source abstract
Abstract
Abstract The wet chemical porosification of low temperature co-fired ceramics (LTCC) applying ortho-phosphoric acid enables the implementation of areas with low permittivity directly into the as-fired substrate surface. Currently, the corresponding chemical reaction is only investigated for the widely used anorthite forming tape DuPont 951. In this paper the research is extended to cover celsian forming tapes with different ceramic particles. As the investigations show, the residual glass after porosification together with the grains should provide stable phases or components and ensure a bearing surface for further metallization. In the LTCC investigated here, the necessary selective etching to the containing celsian phase is given. However, the locality of the pores suffers from the presence of willemite, which is a second predominantly dissolved phase. The high amount of modifier oxides and the agglomeration of the dispersed corundum grains further weaken the stability of the LTCC substantially with respect to this treatment.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microwave Dielectric Ceramics Synthesis · Ferroelectric and Piezoelectric Materials · Electrical and Thermal Properties of Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (65)
Show source-provided references
1. Imanaka · 2005
2. Barlow · 2007
3. Design and technology of microwave and millimeterwave LTCC circuits and systems10.1109/ISSSE.2007.4294524 ↗
4. Innovation steps towards a novel and cost efficient LTCC packaging technology for high end applications
5. Millimeter-wave radar for civil applications
6. Development of future short range radar technology
7. Automotive radar—status and perspectives
8. A 79-GHz radar sensor in LTCC technology using grid array antennas10.1109/TMTT.2013.2260766 ↗
9. Low-k dielectric materials10.1016/S1369-7021(04)00053-7 ↗
10. Materials chemistry for low-k materials10.1016/S1369-7021(06)71387-6 ↗
11. Effect of porosity and grain size on the microwave dielectric properties of sintered corundum10.1111/j.1151-2916.1997.tb03066.x ↗
12. The porosification of fired LTCC substrates by applying a wet chemical etching procedure10.1016/j.jeurceramsoc.2008.05.030 ↗
13. Imaging millimeter wave radar with phased array antenna
14. Recommendations for the characterization of porous solids (Technical Report)10.1351/pac199466081739 ↗
15. Talai · 2013
16. Development of advanced low temperature co-fired ceramics (LTCC)10.4028/www.scientific.net/KEM.264-268.1181 ↗
17. DuPont · 2001
18. Ferro · 2013
19. Etching method for the microstructure of LTCC10.5539/mas.v4n4p70 ↗
20. Feldspar dissolution at 25°C and pH 3: reaction stoichiometry and the effect of cations10.1016/0016-7037(95)00057-7 ↗
21. On the temperature dependence of mineral dissolution rates10.1016/0016-7037(92)90173-G ↗
22. Über die Einwirkung der Phosphorsäure auf Kieselsäure und Silikatgläser10.1002/zaac.19080590125 ↗
23. Gemeinert · 2009
24. Heraeus · 2010
25. Heraeus · 2010
26. Heraeus · 2011
27. Heraeus · 2010
28. Chemical structural and mechanical properties of LTCC tapes
29. Characterization and improvement of LTCC composite materials for application at elevated temperatures10.1016/j.jeurceramsoc.2009.05.023 ↗
30. A structural and dielectric characterization ofNaxCa1−xAl2−xSi2+xO8 (x=0 and 1) ceramics10.1016/j.jeurceramsoc.2005.03.151 ↗
31. Effect of anorthite and diopside on dielectric properties of Al2O3/glass composite based on high strength of LTCC substrate10.1007/s10853-007-2231-4 ↗
32. Solid-state synthesis of ceramics in the BaO–SrO–Al2O3–SiO2 system10.1016/S0272-8842(03)00059-2 ↗
33. Heraeus · 2015
34. Millipore Corporation, Stericup and Steritop, Filtration and Storage Systems, PR02863, Rev. A, June 2008.10.1016/S1365-6937(08)70382-4 ↗
35. The HighScore suite10.1017/S0885715614000840 ↗
36. Ahn · 1983
37. Holleman · 2007
38. Celsian formation in fiber-reinforced barium aluminosilicate glass-ceramic matrix composites10.1016/S0921-5093(02)00313-1 ↗
39. Preparation and properties of barium aluminosilicate glass-ceramics10.1023/A:1018699418458 ↗
40. Towards rational design of low-temperature co-fired ceramic (LTCC) materials10.1007/s40145-012-0011-3 ↗
41. Charakterisierung und Schwindungsverhalten von LTCC—Grünfolien
42. Pfaender · 1980
43. Transformation kinetics from hexacelsian to celsian for powders having uniform particle size10.1016/S0272-8842(00)00059-6 ↗
44. Phase transitions and associated domains in hexacelsian (BaAl2Si2O8)10.1007/BF00307980 ↗
45. High-temperature modification of barium feldspar10.1111/j.1151-2916.1951.tb09131.x ↗
46. Crystallization kinetics of BaO–Al2O3–SiO2 glasses10.1557/JMR.1989.1257 ↗
47. Microwave dielectric loss of titanium oxide10.1111/j.1151-2916.2000.tb01154.x ↗
48. Formation of willemite from powder mixture with TiO2 addition10.1007/BF01139057 ↗
49. Dissolution of willemite polycrystals: effects of pH, temperature and TiO2 solid solution10.1007/BF00595745 ↗
50. Chemical durability of oxide glasses in aqueous solutions: a review10.1111/j.1551-2916.2007.02101.x ↗
51. Unifying natural and laboratory chemical weathering with interfacial dissolution-reprecipitation: a study based on the nanometer-scale chemistry of fluid-silicate interfaces10.1016/j.chemgeo.2011.12.002 ↗
52. Insight into silicate-glass corrosion mechanisms10.1038/nmat2301 ↗
53. Physical properties of nano-composite silica-phosphate thin film prepared by sol–gel technique
54. Sintering, microstructure and dielectric properties of Ca-Al-B-Si-O glass/Al2O3 composites with various SiO2 content
55. Determination of quartz in presence of silicates using phosphoric acid10.1021/ac60052a021 ↗
56. Okrusch · 2010
57. General kinetic description of multioxide silicate mineral and glass dissolution10.1016/S0016-7037(01)00710-4 ↗
58. Some factors affecting the dissolution kinetics of anorthite at 25°C10.1016/0016-7037(92)90312-7 ↗
59. Experimental study of anorthite dissolution and the relative mechanism of feldspar hydrolysis10.1016/0016-7037(95)00326-6 ↗
60. Crystallization kinetics of BaO–Al2O3–SiO2 glasses10.1557/JMR.1989.1257 ↗
61. The acid decomposition of silicate minerals part I. Reactivities and modes of dissolution of silicates10.1016/0304-386X(83)90002-6 ↗
62. Low-temperature sintering and microwave dielectric properties of anorthite-based glass-ceramics10.1111/j.1151-2916.2002.tb00440.x ↗
63. Hydrothermal corrosion of corundum ceramics10.1111/j.1151-2916.1997.tb03258.x ↗
64. Chemical resistance of ceramic materials in acids and alkalis10.1023/B:GLAC.0000048706.05368.71 ↗
65. Corrosion of corundum ceramics in acidic aqueous solutions at high temperatures and pressures10.1023/A:1026714218522 ↗