Microstructural evolution in nanocrystalline Y–TZP containing a silicate glass
Source abstract
Abstract
Abstract Nanocrystalline yttria stabilized tetragonal zirconia polycrystal (NC–Y–TZP) powders were coated with a sodium strontium silicate glass using the sol-gel technique. The compact powders were sintered at 1400°C for 1 h resulting in dense nanocrystalline pellets with 5, 10 and 15 vol.% glass. Short pre-sintering heat treatment at 800°C caused the full stabilization of the tetragonal phase while long treatments led to the devitrification of the glassy phase. The mean grain size decreased from 196 nm in the glass-free specimen to 140, 110 and 100 nm in the specimens containing 5, 10 and 15 vol.% glass, respectively. The grain size distribution width also decreased with increase in the glass content. TEM revealed the morphological changes of the highly facetted polyhedral grains in the glass-free specimens into the round-shape grains with increase in the glass content. The effect of the glass on the phase formation, densification and microstructure have been discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Glass properties and applications · Advanced ceramic materials synthesis · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Superplasticity of yttria-stabilized tetragonal ZrO2 polycrystals10.1111/j.1551-2916.1986.tb00026.x ↗
2. Superplastic behavior of a yttria-stabilized tetragonal xirconia polycrystal10.1016/S0036-9748(88)80150-9 ↗
3. Nieh · 1997
4. Joining of yttria-tetragonal stabilized zirconia polycrystals using nanocrystals10.1016/S1359-6462(99)00190-6 ↗
5. Joining of alumina ceramics using nanocrystalline tape cast interlayers10.1557/JMR.2000.0248 ↗
6. On creep enhanced by a liquid phase10.1016/0001-6160(83)90072-X ↗
7. Creep deformation due to a viscous grain boundary phase10.1016/0001-6160(89)90085-0 ↗
8. Effect of a liquid phase on superplasticity of 2-mol%–Y2O3-stabilized tetragonal zirconia polycrystals10.1111/j.1151-2916.1990.tb09806.x ↗
9. Role of grain-boundary glass phase on the superplastic deformation of tetragonal zirconia polycrystal10.1111/j.1151-2916.1990.tb06718.x ↗
10. Influence of amorphous grain boundary phases on the superplastic behavior of 3-mol.%-yttria-stabilized tetragonal zirconia polycrystals (3Y-TZP)10.1111/j.1151-2916.1993.tb06635.x ↗
11. The brittle to ductile transition in a Si3N4/SiC composite with a glassy grain boundary phase10.1016/0956-7151(93)90050-3 ↗
12. Seidensticker · Scripta Metall. Mater. · 1994 · 31 · 174910.1016/0956-716X(94)90476-6 ↗
13. The enhancement of superplastic flow in tetragonal zirconia polycrystals with SiO2-doping10.1016/0956-7151(94)00320-H ↗
14. Compressive deformation behaviour of superplastic Y-TZP based ceramics10.1016/S0955-2219(96)00122-7 ↗
15. Influence of a transition metal oxide (CuO) on the superplastic behaviour of 8 mol.% yttria-stabilised cubic zirconia polycrystal (8Y-CSZ)10.1023/A:1013268810031 ↗
16. Microstructural characterization of superplastic SiO2-doped TZP with a small amount of oxide addition10.1111/j.1151-2916.1998.tb02715.x ↗
17. Chen · Mater. Sci. Forum · 1997 · 243-245 · 24510.4028/www.scientific.net/MSF.243-245.245 ↗
18. Superplastic flow of fine-grained yttria-stabilized zirconia polycrystals: constitutive equation and deformation mechanisms10.1111/j.1151-2916.1998.tb02695.x ↗
19. Creep of nanocrystalline Y-SZP ceramics10.1016/S0965-9773(99)00339-6 ↗
20. Plastic deformation in impure nanocrystalline ceramics10.1557/JMR.1999.0336 ↗
21. Liquid-phase sintering of alumina coated with magnesium aluminosilicate glass10.1111/j.1151-2916.1998.tb02464.x ↗
22. Reinforcement of hyroxyapatite biocermic by addition of ZrO2 coated with Al2O310.1111/j.1151-2916.1999.tb02189.x ↗
23. Percolative composite model for prediction of the properties of nanocrystalline materials10.1557/JMR.1997.0251 ↗
24. Stabilization of tetragonal ZrO2 in ZrO2–SiO2 binary oxides10.1111/j.1151-2916.2000.tb01243.x ↗
25. Chemical interactions promoting the ZrO2 tetragonal stabilization in ZrO2-SiO2 binary oxides10.1111/j.1151-2916.2000.tb01418.x ↗
26. Preparation and sintering of silica- doped zirconia by colloidal processing10.1557/PROC-457-33 ↗
27. On the equilibrium thickness of intergranular glass phases in ceramic materials10.1111/j.1151-2916.1987.tb04846.x ↗
28. Liquid phase sintering of RE2O3: YSZ ceramics, Part I: Grain growth and expelling of the grain boundary glass phase10.1023/A:1004659832382 ↗
29. Synthesis and characterization of yttria-stabilized tetragonal zirconia polycrystalline powder coated with silica layers10.1016/0167-577X(96)00024-9 ↗
30. Grain growth of silica-added zirconia annealed in the cubic/tetragonal two-phase region10.1111/j.1151-2916.1998.tb02591.x ↗
31. Imaging secondary-ion mass spectroscopy observation of the scavenging of siliceous film from 8-mol%-yttria-stabilized zirconia by the addition of alumina10.1111/j.1151-2916.2000.tb01366.x ↗
32. Phase Diagrams for Zirconium+Zirconia Systems, ed. H. M. Ondik and H. F. McMurdie. The ACS and NIST, Westerville, Ohio, 1998, p. 134.
33. High-temperature behavior of SiO2 at grain boundaries in TZP10.1023/A:1008777500697 ↗