Abstract

Abstract We investigated annealing effects of La1−xSrxMnO3 (x = 0–0.6) on electrical resistivity and the temperature coefficient of resistivity (TCR). The annealed samples’ resistivity was lower than those of non-annealed samples. For example, annealing changed the resistivity of x = 0.3 at 25 °C from 4.50 × 10−5 to 3.71 × 10−5 Ω m. Remarkable difference in TCR was observed after annealing, for x = 0.3, 0.45, and 0.5. For x = 0.3, the TCR after annealing was 4000 ppm/°C, which was 1250 ppm/°C greater than that before annealing. We investigated (1) crystal phase, (2) Mn average valence, (3) Mott insulator–metal transition temperature, and (4) microstructure. The microstructure was remarkably varied for annealed x = 0.3 and 0.5. The average grain size of the x = 0.3 increased from 1.60 up to 2.38 μm. Results show that annealing affects resistivity and TCR because of grain growth during annealing.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic and transport properties of perovskites and related materials · Ferroelectric and Piezoelectric Materials · Multiferroics and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (13)

Show source-provided references
1. Electrical properties and conduction mechanisms of Ru-based thick-film (cermet) resistors10.1063/1.323595 ↗
2. Particle size effects in thick film resistors10.1063/1.331364 ↗
3. Firing, quenching and annealing studies on thick-film resistors10.1016/S0955-2219(03)00462-X ↗
4. Correlation between microstructure and gauge factors of thick film resistors10.1007/BF00258161 ↗
5. Environment friendly perovskite ruthenate based thick film resistors10.1016/j.matlet.2006.05.015 ↗
6. Insulator–metal transition and giant magnetoresistance in La1−xSrxMnO310.1103/PhysRevB.51.14103 ↗
7. Charge ordering and sound velocity anomaly in La1−xSrxMnO3 (x≥0.5)10.1143/JPSJ.67.2582 ↗
8. Colossal magnetoresistive manganites10.1016/S0304-8853(99)00352-2 ↗
9. Controlling temperature coefficient of resistivity in La1−xSrxMnO3 ceramics10.1016/j.matlet.2009.08.032 ↗
10. Influence of the grain-size and oxygen stoichiometry on magnetic and transport properties of polycrystalline La0.67Ca0.33MnO3±δ perovskites10.1016/S0304-8853(98)00257-1 ↗
11. Resistivity, giant magnetoresistance and thermopower in La0.7Sr0.3MnO3 showing a large difference in temperatures corresponding to the ferromagnetic transition and the insulator–metal transition10.1016/0038-1098(96)00233-5 ↗
12. Role of grain boundaries in double exchange manganite oxides La1−xAxMnO3 (A=Ba, Ca)10.1016/S0038-1098(97)00031-8 ↗
13. Characterization of La0.67Ca0.33MnO3±δ particles prepared by the sol–gel route10.1039/a707226k ↗