journal article·2011-08

Fracture behavior of silicon nitride ceramics under combined compression–torsion stresses analyzed by multiaxial fracture statistics

N. Kawai, T. Kotani, Y. Kakimoto, E. Sato

Publisher page

Abstract

Abstract Combined compression–torsion tests were performed on the thermal-treated and as-machined silicon nitride ceramics to investigate their fracture behavior under multiaxial stress states. The thermal-treated samples showed considerable high strength and low anisotropy to the grinding direction in flexure tests compared to the as-machined samples. Under combined compression and torsion stress states, the thermal-treated samples showed considerably higher tensile strength than that of as-machined samples at low compressive stress states and weakening with increasing compression stress. The as-machined samples showed little decrease in tensile strength with increasing compression stress and comparable tensile strength with the thermal-treated samples under a highly compressive stress state. The behavior of thermal-treated samples were well described by the statistical theory of multiaxial fracture for volume-distributed flaws combined with a mixed-mode fracture criterion with the shear sensitivity constant of 1.75 and 1.65 for Shetty’s criterion and the ellipsoidal criterion, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Rock Mechanics and Modeling · High-Velocity Impact and Material Behavior · Numerical methods in engineering

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Characterization of first-stage silicon nitride components after exposure to an industrial gas turbine10.1111/j.1551-2916.2005.00678.x ↗
2. Micrometeoroid impact on ceramic thin components for interplanetary probe10.1016/j.ijimpeng.2008.07.051 ↗
3. Weakest link theory reformulated for arbitrary fracture criterion10.1111/j.1151-2916.1978.tb09327.x ↗
4. A general approach for the statistical analysis of multiaxial fracture10.1111/j.1151-2916.1978.tb09314.x ↗
5. Probabilistic analysis of brittle fracture loci under bi-axial stress state10.1299/kikaia.46.605 ↗
6. Effects of combined stresses on fracture of alumina and graphite10.1111/j.1151-2916.1970.tb12034.x ↗
7. Strength of titania and aluminum silicate under combined stresses10.1111/j.1151-2916.1972.tb11307.x ↗
8. Failure of brittle solids under biaxial stresses10.1007/BF00049227 ↗
9. Fracture of Al2O3 in combined tension/torsion: I. Experiments10.1111/j.1151-2916.1981.tb15865.x ↗
10. Fracture of Al2O3 in combined tension/torsion: II. Weibull theory10.1111/j.1151-2916.1981.tb15866.x ↗
11. Multiaxial loading fracture of Al2O3 tubes: I. Experiments10.1111/j.1151-2916.1984.tb19138.x ↗
12. Multiaxial loading fracture of Al2O3 tubes: II. Weibull theory and analysis10.1111/j.1151-2916.1984.tb19138.x ↗
13. Fracture criterion for alumina ceramics subjected to triaxial stresses10.1111/j.1151-2916.1984.tb19166.x ↗
14. Fracture behavior of sintered silicon nitride under multiaxial stress states10.2109/jcersj.96.539 ↗
15. Fracture of alumina tubes under combined tension/torsion10.1111/j.1151-2916.1992.tb04157.x ↗
16. Fracture strength of silicon nitride under biaxial stresses10.2109/jcersj.100.1304 ↗
17. Fracture of SiC tubes under combined tension/torsion10.1007/BF00037089 ↗
18. Failure criterion with given survivability for ceramic notched elements under combined tension/torsion10.1016/S0921-5093(03)00161-8 ↗
19. Determination of the multiaxial failure criteria for alumina ceramics under tension–torsion test10.1016/j.jeurceramsoc.2010.08.008 ↗
20. Strength of hot-pressed silicon nitride after high-temperature exposure10.1111/j.1151-2916.1984.tb19637.x ↗
21. Crack healing behavior of hot pressed silicon nitride due to oxidation10.1016/0956-716X(92)90574-X ↗
22. (Crack-healing + proof test): a new methodology to guarantee the structural integrity of a ceramics component10.1016/S0955-2219(01)00236-9 ↗
23. Crack-healing and oxidation behavior of silicon nitride ceramics10.1016/S0955-2219(03)00645-9 ↗
24. Shock response of silicon nitride
25. ISO 20501:2003. Fine ceramics (advanced ceramics, advanced technical ceramics)—Weibull statistics for strength data.
26. The effect of grinding direction on flow character and strength of single crystal and polycrystalline ceramics10.1007/BF00542727 ↗
27. The effect of grinding on strength of hot-pressed silicon nitride10.2355/isijinternational.29.726 ↗
28. Influence of grinding direction on fracture strength of silicon nitride10.1115/1.2806815 ↗
29. Fracture of ceramics10.1002/adem.200700347 ↗
30. Mixed-mode fracture criteria for reliability analysis and design with structural ceramics10.1115/1.3240037 ↗
31. Combined mode fracture toughness measurement by the disk method10.1115/1.3443468 ↗
32. Statistical analysis of bending strengths for brittle solids: a multiaxial fracture problem10.1111/j.1151-2916.1983.tb10012.x ↗
33. Mixed-mode fracture of hot-pressed Si3N410.1111/j.1151-2916.1985.tb15238.x ↗
34. Fracture under mixed-mode loading in ceramics having a semi-circular crack10.1299/kikaia.55.1191 ↗
35. Fracture behavior of sintered silicon nitride under multiaxial stress states (part 2)10.2109/jcersj.99.574 ↗
36. Combined mode I and mode II fracture of monolithic ceramics10.1111/j.1151-2916.1993.tb07763.x ↗
37. Fracture behavior of a silicon nitride ceramic under mixed-mode fracture condition10.2109/jcersj.101.240 ↗
38. Mixed-mode high temperature toughness of silicon nitride10.1007/BF00354402 ↗