journal article·2013-03Open access

Microstructure and mechanical properties of Ni/10mol% Sc2O3–1mol% CeO2–ZrO2 cermet anode for solid oxide fuel cells

Yan Chen, Nina Orlovskaya, Thomas Graule, Jakob Kuebler

Abstract

Abstract The mechanical properties of anode materials play an important role in the reliability and durability of solid oxide fuel cells operating at high temperatures in a reducing environment. In this paper, we produced the results of the mechanical properties investigation of Ni/10 mol% Sc 2 O 3 –1 mol% CeO 2 –ZrO 2 cermet anodes. Young's modulus as well as strength and fracture toughness of non-reduced and reduced anodes has been measured, both at room and at high temperatures. High temperature experiments were performed in the reducing environment of forming gas. It is shown that while at 700 °C and 800 °C, the anode specimens exhibited purely elastic deformation and brittle fracture, a brittle-to-ductile transition occurred for heating above 800 °C and the anode deformed plastically at 900 °C. Fractography of the anode specimens were performed to identify the fracture modes of anodes tested at different temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. A review on the status of anode materials for solid oxide fuel cells10.1016/S0921-5093(03)00620-8 ↗
2. Mechanical properties of tape cast nickel-based anode materials for solid oxide fuel cells before and after reduction in hydrogen10.1016/j.actamat.2004.08.023 ↗
3. Fracture properties of nickel-based anodes for solid oxide fuel cells10.1016/j.jeurceramsoc.2010.07.028 ↗
4. Evaluation of elastic properties of reduced NiO–8YSZ anode-supported bi-layer SOFC structures at elevated temperatures in ambient air and reducing environments10.1007/s10853-008-3141-9 ↗
5. Electrochemical and mechanical properties of solid oxide fuel cell Ni/YSZ anode fabricated from NiO/YSZ composite powder10.2109/jcersj2.119.876 ↗
6. Elastic properties of nickel-based anodes for solid oxide fuel cells as a function of the fraction of reduced NiO10.1111/j.1151-2916.2004.tb07499.x ↗
7. Study on zirconia solid electrolytes doped by complex additives10.1016/j.msea.2006.12.072 ↗
8. Characterization of ZrO2 co-doped with Sc2O3 and CeO2 electrolyte for the application of intermediate temperature SOFCs10.1016/j.ssi.2004.07.013 ↗
9. Presentation at E1-solid state topics general session (#1824)
10. Electrical properties of solid oxide electrolytes10.1021/cr60265a003 ↗
11. Materials and concepts for solid oxide fuel cells (SOFCs) in stationary and mobile applications10.1016/j.jpowsour.2003.09.024 ↗
12. Reforming activity and carbon deposition on cermet catalysts for fuel electrodes of solid oxide fuel cells10.1016/j.cattod.2009.01.033 ↗
13. Effect of oxide on carbon deposition behavior of CH4 fuel on Ni/ScSZ cermet anode in high temperature SOFCs10.1016/j.ssi.2005.12.009 ↗
14. Comparison between internal steam and CO2 reforming of methane for Ni–YSZ and Ni–ScSZ SOFC anodes10.1149/1.3435320 ↗
15. Metastable-stable phase diagrams in the zirconia-containing systems utilized in solid-oxide fuel cell application10.1016/0167-2738(96)00386-4 ↗
16. β-Cubic phase transition of scandia-doped zirconia solid solution: calorimetry, X-ray diffraction, and Raman scattering10.1063/1.1471576 ↗
17. Phase stability and sintering behavior of 10mol% Sc2O3–1mol% CeO2–ZrO2 ceramics10.1115/1.2971126 ↗
18. Temperature and stress induced changes of the vibrational response of cubic and rhombohedral 10mol% Sc2O3–1mol% CeO2–ZrO2 ceramics10.1016/j.jpowsour.2009.10.060 ↗
19. Rapid phase transformation of zirconia in the Ni–ScSZ cermet anode under reducing condition10.1016/j.ssi.2008.06.024 ↗
20. Carbon deposition over Ni–ScSZ anodes subjected to various heat-treatments for internal reforming of solid oxide fuel cells10.1149/1.2975337 ↗
21. Influence of preparation methods on the carbon deposition and reduction behavior of Ni–ScSZ cermet10.1149/1.3484094 ↗
22. EN 843-2 advanced technical ceramics – mechanical properties of monolithic ceramics at room temperature. Part 2. Determination of Young's modulus, shear modulus and Poisson's ratio; December 2006.
23. EN 843-1 advanced technical ceramics – mechanical properties of monolithic ceramics at room temperature. Part 1. Determination of flexural strength; December 2006.
24. A statistical distribution function of wide applicability10.1115/1.4010337 ↗
25. The validity of Weibull estimators – experimental verification
26. Prediction of strength of recrystallized silicon carbide from pore sized measurement. Part I. The bimodality of the distribution10.1023/A:1004705300886 ↗
27. Prediction of strength of recrystallized silicon carbide from pore sized measurement. Part II. The reliability of the prediction10.1023/A:1004757317724 ↗
28. CEN/TS 14425-5 advanced technical ceramics test methods for determination of fracture toughness of monolithic ceramics. Part 5. Single-edge V-notch beam (SEVNB) method; 2004.
29. Fracture toughness of ceramics using the SEVNB method: from a preliminary study to a standard test method
30. Sintering behavior and mechanisms of NiO-doped 8mol% yttria stabilized zirconia10.1016/j.jeurceramsoc.2011.03.025 ↗
31. Effect of NiO on the phase stability and microstructure of yttria-stabilized zirconia10.1111/j.1551-2916.2006.01464.x ↗
32. Solid-solution effects of a small amount of nickel oxide addition on phase stability and mechanical properties of yttria-stabilized tetragonal zirconia polycrystals10.1111/j.1151-2916.2003.tb03334.x ↗
33. Stability of cubic ZrO2 (10mol% Y2O3) when alloyed with NiO, Al2O3 or TiO2: implications to solid electrolytes and cermets10.1016/0921-5107(94)90252-6 ↗
34. The enhanced stabilization of the cubic phase in yttria-stabilized zirconia with the addition of nickel oxide10.1111/j.1551-2916.2010.04349.x ↗
35. Structure and impedance of ZrO2 doped with SC2O3 and CeO210.1016/j.matlet.2004.07.065 ↗
36. Piezo-spectroscopic coefficients of tetragonal-prime yttria-stabilized zirconia10.1111/j.1551-2916.2007.01622.x ↗
37. Structural changes of scandia-doped zirconia solid solutions: Rietveld analysis and Raman scattering10.1111/j.1151-2916.1998.tb02710.x ↗
38. Determination of cubic-tetragonal phase boundary in Zr1−XYXO2−X/2 solid solutions by Raman spectroscopy10.1063/1.354989 ↗
39. The temperature dependence of Young's modulus for nickel10.1103/PhysRev.44.116 ↗
40. Origin and development of residual-stresses in the Ni–NiO system – in situ studies at high-temperature by X-ray-diffraction10.1016/0921-5093(93)90504-8 ↗
41. Microstructure degradation of cermet anodes for solid oxide fuel cells: quantification of nickel grain growth in dry and in humid atmospheres10.1016/j.jpowsour.2010.08.017 ↗
42. Quantitative relationships between composition, particle size, triple phase boundary length and surface area in nickel-cermet anodes for solid oxide fuel cells10.1016/j.jpowsour.2010.08.006 ↗